Abstract The surface of Qiong kiln opaque glaze celadon exhibits a phenomenon of hole corrosion. Using scanning electron microscopy, energy spectrometry, Raman spectroscopy, and other analytical means to conduct the analysis, the results show that this pore corrosion is induced in the tubular crystal, formed by various corrosion behaviors combined with effect formation. The tubular structure constitutes a channel connecting the external environment with the interior of the glaze layer. At the same time, the surface adsorption and ion exchange properties of the tubular structure itself may increase the rate of glaze corrosion.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Cultural Heritage Materials Analysis · Conservation Techniques and Studies · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Zhang F. K. The Science of Ancient Chinese Ceramics (Shanghai People’s Fine Arts Publishing House, 2000) (in Chinese).
2. Chen L. Q. New Exploration of Qiong Kiln. In: Shanghai Institute of Silicate editor. Research on Chinese Ancient Ceramics. 349–353 (Chinese Academy of Sciences Press, 1987) (in Chinese).
3. Chen L. Q. Overview of the development of Qiong Kiln ancient ceramics. In Geng B. C. editor. Studies on the Ancient Ceramics of Qiong Kiln 97 (University of Science and Technology of China Press, 2002) (in Chinese).
4. Li, Z. M., Ma, Y., Ma, Q. L., Chen, J. C. & Yan, S. New perspective on Jun glaze corrosion: study on the corrosion of light greenish blue and reddish purple glazes from Juntai Kiln, Yuzhou, Henan, China. Herit. Sci. 08, 2 (2020).10.1186/s40494-019-0346-y ↗
5. Zhou, B. Y., Ma, Q. L., Li, Z. M. & Chen, J. C. Corrosion research on Ru porcelain glazes excavated at Qingliangsi, Baofeng, China. Coatings 13, 1011 (2023).10.3390/coatings13061011 ↗
6. Frankel, G. S. et al. A comparative review of the aqueous corrosion of glasses, crystalline ceramics, and metals. npj Mater. Degrad. 2, 15 (2018).10.1038/s41529-018-0037-2 ↗
7. Zhang, Z. M. & Carter, M. L. An X-ray photoelectron spectroscopy investigation of highly soluble grain-boundary impurity films in hollandite. J. Am. Ceram. Soc. 93, 894–899 (2010).10.1111/j.1551-2916.2009.03518.x ↗
8. Wu, H. Z. et al. Was bone used in the glaze of the ancient Qiong kilns for the production of Tang dynasty opaque glaze celadon? J. Eur. Ceram. Soc. 45, 117017 (2025).10.1016/j.jeurceramsoc.2024.117017 ↗
9. Kara, A. & Stevens, R. Characterisation of biscuit fired bone china body microstructure. Part I: XRD and SEM of crystalline phases. J. Eur. Ceram. Soc. 22, 731–736 (2002).10.1016/S0955-2219(01)00371-5 ↗
10. Zhang, Y., Yang, Y., Li, W. & Ren, Y. Effect of Al2O3 addition on the flexural strength and light-transmission properties of bone china. Int. J. Appl. Ceram. Technol. 12, 875–884 (2015).10.1111/ijac.12296 ↗
11. Li, Y., Shen, Y. M., Zheng, J. M. & Wang, G. Y. Comparative microstructural study of celadon excavated from Housi’ ao kiln site in China (Late Tang and Five Dynasties): Mi-se porcelain and ordinary Yue celadon. J. Eur. Ceram. Soc. 41, 430–440 (2021).10.1016/j.jeurceramsoc.2021.08.050 ↗
12. Wang, T. et al. Philippe Sciau, micro-structural study of Yaozhou celadons (Tang to Yuan Dynasty): probing crystalline and glassy phases. J. Eur. Ceram. Soc. 40, 4676–4683 (2020).10.1016/j.jeurceramsoc.2020.03.066 ↗
13. Geng C. Scientific research on the raw materials and related processes of Yaozhou kiln porcelain production in Shaanxi (Shandong University, 2023) (in Chinese).
14. Simsek, G. et al. Toward a fast non-destructive identification of pottery: the sourcing of 14th–16th century Vietnamese and Chinese ceramic shards. J. Cult. Herit. 16, 159–172 (2015).10.1016/j.culher.2014.03.003 ↗
15. Michelin, A. et al. Silicate glass alteration enhanced by iron: origin and long-term implications. Environ. Sci. Technol. 47, 750–756 (2013).10.1021/es304057y ↗
16. Hellmann, R. et al. Nanometre-scale evidence for interfacial dissolution–reprecipitation control of silicate glass corrosion. Nat. Mater. 14, 307–311 (2015).10.1038/nmat4172 ↗
17. Lenting, C. et al. Towards a unifying mechanistic model for silicate glass corrosion. Npj Mat. Degrad. 2, 28 (2018).10.1038/s41529-018-0048-z ↗
18. Gin, S. et al. The controversial role of inter-diffusion in glass alteration. Chem. Geol. 440, 115–123 (2016).10.1016/j.chemgeo.2016.07.014 ↗
19. Chinese Soil Taxonomy. Cooperative Research Group on Chinese Soil Taxonomy (Science Press, 2001).
20. Kunicki-Goldfinger, J. J. Unstable historic glass: symptoms, causes, mechanisms and conservation. Stud. Conserv. 53, 47–60 (2008).10.1179/sic.2008.53.Supplement-2.47 ↗
21. Tournié, A., Ricciardi, P. & Colomban, P. H. Glass corrosion mechanisms: a multiscale analysis. Solid State Ion. 179, 2142–2154 (2008).10.1016/j.ssi.2008.07.019 ↗
22. Hussin, M. S. F., Abdullah, H. Z., Idris, M. I. & Wahap, M. A. A. Extraction of natural hydroxyapatite for biomedical applications—a review. Heliyon 08, e10356 (2022).10.1016/j.heliyon.2022.e10356 ↗
23. Wijesinghe, W. P. S. L. et al. Facile synthesis of both needle-like and spherical hydroxyapatite nanoparticles: effect of synthetic temperature and calcination on morphology, crystallite size and crystallinity. Mat. Sci. Eng. C 42, 83–90 (2014).10.1016/j.msec.2014.05.032 ↗
24. Amenaghawon, A. N., Anyalewechi, C. L., Darmokoesoemo, H. & Kusuma, H. S. Hydroxyapatite-based adsorbents: applications in sequestering heavy metals and dyes. J. Environ. Manag. 302, 113989 (2022).10.1016/j.jenvman.2021.113989 ↗
25. Asri, S. E. et al. Conversion of natural phosphate rock into mesoporous hydroxyapatite for heavy metals removal from aqueous solution. Colloid Surf. A 362, 33–38 (2010).10.1016/j.colsurfa.2010.03.036 ↗
26. Wang, F. et al. Facile preparation of hydroxyapatite with a three-dimensional architecture and potential application in water treatment. Crystengcomm 13, 5634–5637 (2011).10.1039/c1ce05485f ↗
27. Wang, J. et al. Progress of hydroxyapatite composites for adsorption and removal of uranium from groundwater. Nonferrous Met. (Extract. Metall.) 08, 37–45 (2021). (in Chinese).
28. Cawthray, J. F., Creagh, A. L., Haynes, C. A. & Orvig, C. Ion exchange in hydroxyapatite with lanthanides. Inorg. Chem. 54, 1440–1445 (2015).10.1021/ic502425e ↗
29. Fu, L. H. et al. Microwave-assisted hydrothermal synthesis of cellulose/hydroxyapatite nanocomposites. Polymers 08, 316 (2016).10.3390/polym8090316 ↗