journal article·2026-03

Experimental investigation of surface integrity and fatigue performance of TC17 alloy simulated blades under milling, polishing, vibration finishing, and shot peening conditions

Liang Tan, Shuaifeng Xue, Jiazhi Tang, Manqi Wang, Chuangguo Hu, Changfeng Yao

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Surface Treatment and Residual Stress · High-Velocity Impact and Material Behavior · Bladed Disk Vibration Dynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Cyclic softening behavior of TC17 titanium alloy fabricated by laser directly energy deposition10.1016/j.msea.2023.145883 ↗
2. Effects of different mechanical surface treatments on surface integrity of TC17 alloys10.1016/j.surfcoat.2020.126073 ↗
3. Effect of solution aging heat treatment on microstructure evolution and properties of TC17 titanium alloy formed by laser solid forming10.1007/s11665-023-08075-1 ↗
4. Additive manufacturing of metallic components-Process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
5. The fatigue behavior of TC17 titanium alloy under different test environments: the effect of saltwater on fatigue failure characteristics and life estimation
6. Failure analysis of Ti6Al4V titanium alloy under fatigue loading: an experimental and numerical study10.1016/j.engfailanal.2024.108715 ↗
7. Fatigue failure mechanism of Ti60 titanium alloy in HCF and VHCF regime at different temperatures10.1016/j.engfailanal.2023.107393 ↗
8. Influence of milling stability on machined surface integrity and fatigue performance of Ti-6Al-4V titanium alloy10.1016/j.engfailanal.2024.109103 ↗
9. Enhancement of machinability and surface quality of Ti-6Al-4V by longitudinal ultrasonic vibration-assisted milling under dry conditions10.1016/j.measurement.2021.110324 ↗
10. Effects of rotary ultrasonic elliptical machining for side milling on the surface integrity of Ti-6Al-4V
11. Surface topography analysis and cutting parameters optimization for peripheral milling titanium alloy Ti-6Al-4V10.1016/j.ijrmhm.2015.04.001 ↗
12. Influence of milling-finishing-shot peening hybrid machining on the surface integrity and fatigue performance of TC11 titanium integral impeller10.1007/s00170-024-14416-8 ↗
13. Thermo–metallo–mechanical based phase transformation modeling for high–speed milling of Ti-6Al-4V through stress-strain and temperature effects10.1016/j.jmrt.2024.03.096 ↗
14. Investigation of the impact of high-speed machining in the milling process of titanium alloy on tool wear, surface layer properties, and fatigue life of the machined object10.3390/ma16155361 ↗
15. Shot peening coverage effect on laser powder bed fused steel10.1016/j.ijmecsci.2024.109520 ↗
16. A promising approach to enhance fatigue life of TC11 titanium alloy: Low dislocation density and surface grain refinement induced by electropulsing10.1016/j.jmst.2024.03.020 ↗
17. Effects of fine particle peening treatment applied with different shot types and coverages on the surface integrity of TC11/Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy10.1016/j.surfcoat.2025.131853 ↗
18. On the severe shot peening effect to generate nanocrystalline surface towards enhancing fatigue life of injection-moulded Ti-6Al-4V alloy10.1007/s10853-023-08978-3 ↗
19. Effect of surface high density twin microstructure induced by shot peening on the fatigue behavior of Ti-6Al-4V10.1016/j.jmrt.2024.03.234 ↗
20. The effect of shot peening time on mechanical properties and residual stress in Ti-6Al-4V alloy10.1051/metal/2022036 ↗
21. Experimental study and fatigue life prediction on high cycle fatigue performance of laser-peened TC4 titanium alloy10.1016/j.msea.2021.141658 ↗
22. Effect of machined surface integrity on fatigue resistance of aluminum-silicon alloy ZL109
23. Surface integrity and fatigue behavior for high-speed milling Ti-10V-2Fe-3Al titanium alloy10.1007/s11668-013-9772-4 ↗
24. Experimental investigation on surface integrity and fatigue performance of Ti60 alloy under ultrasonic impact treatment10.1016/j.engfailanal.2024.108639 ↗
25. Research on surface integrity and fatigue properties in the turning of TC17 titanium alloy based on the response surface method10.3390/ma16227180 ↗
26. A modified fatigue life prediction model considering residual stresses relaxation and microhardness distribution for surface strengthening materials10.1016/j.ijfatigue.2025.108862 ↗
27. Effect of cutting surface integrity on fatigue properties of TC17 titanium alloy10.3390/ma16165658 ↗
28. Improving the high cycle fatigue property of Ti6Al4V ELI alloy by optimizing the surface integrity through electric pulse combined with ultrasonic surface rolling process10.1016/j.jmst.2023.06.029 ↗
29. Strategy and mechanism to improve the fatigue properties of Ti6Al4V ELI alloy by microstructure modulation combined with surface strengthening process10.1016/j.msea.2023.146005 ↗
30. Influence mechanism of abrasive belt wear on fatigue resistance of TC17 grinding surface10.1016/j.engfailanal.2022.106644 ↗
31. Improving fatigue performance of thin-walled components via synchronous double-sided ultrasonic surface rolling process10.1016/j.jmatprotec.2025.118775 ↗
32. The effects of laser peening and shot peening on fretting fatigue in Ti-6Al-4V coupons10.1016/j.triboint.2009.04.005 ↗
33. Effect of laser shock peening on boring hole surface integrity and conformal contact fretting fatigue life of Ti-6Al-4 V alloy10.1016/j.ijfatigue.2022.107241 ↗
34. Effects of defects on fatigue behavior of TC17 titanium alloy for compressor blades: Crack initiation and modeling of fatigue strength10.1016/j.engfracmech.2021.108136 ↗
35. Effect of shot peening on high cycle and very high cycle fatigue properties of Ni-based superalloys10.1016/j.ijfatigue.2022.107429 ↗
36. Combined effect of random porosity and surface defect on fatigue lifetime of additively manufactured micro-sized Ti6Al4V components: an investigation based on numerical analysis and machine learning approach10.1016/j.tafmec.2024.104451 ↗
37. Fatigue crack propagation behavior in Ti-6Al-4V alloy with surface gradient structure fabricated by high-energy shot peening10.1016/S1003-6326(23)66313-7 ↗
38. Effects of beads and shot peening intensity on the surface integrity and fatigue performance of a stainless gear steel
39. Surface roughness prediction of SiCp/Al composites in ultrasonic vibration-assisted grinding10.1016/j.jmapro.2023.05.093 ↗
40. Comprehensive experimental study of shot peening on the surface integrity evolution of 12Cr2Ni4A high-strength steel
41. Surface integrity and fatigue lives of Ti17 compressor blades subjected to laser shock peening with square spots10.1016/j.surfcoat.2018.05.023 ↗
42. Fatigue crack growth behavior of an additively manufactured titanium alloy: Effects of spatial and crystallographic orientations of α lamellae10.1016/j.ijplas.2023.103819 ↗
43. Slip and fatigue crack formation processes in an α/β titanium alloy in relation to crystallographic texture on different scales10.1016/j.actamat.2008.04.036 ↗
44. Microstructural effects on fatigue crack initiation mechanisms in a near-alpha titanium alloy10.1016/j.actamat.2023.118957 ↗
45. Crack initiation mechanisms in Ti-6Al-4V subjected to cold dwell-fatigue, low-cycle fatigue and high-cycle fatigue loadings10.1016/j.actamat.2022.118560 ↗
46. Study on low fatigue damage behavior of TC17 titanium alloy with basket-weave microstructure10.1016/j.ijfatigue.2024.108462 ↗
47. Effect of α-phase morphology on low-cycle fatigue behavior of TC21 alloy10.1016/j.ijfatigue.2015.01.010 ↗
48. Predicting the fatigue life of machined specimen based on its surface integrity parameters10.1007/s00170-021-08429-w ↗
49. Surface integrity investigations for prediction of fatigue properties after machining of alloy 71810.1016/j.ijfatigue.2020.106059 ↗
50. Effect of machined surface integrity on fatigue performance of metal workpiece: a review10.1186/s10033-021-00631-x ↗
51. Crystal plasticity modeling of fretting fatigue crack initiation behavior in Ti6Al4V10.1016/j.engfailanal.2024.109074 ↗
52. Titanium alloy components fabrication by laser depositing TA15 powders on TC17 forged plate: Microstructure and mechanical properties10.1016/j.msea.2021.141382 ↗
53. Ti-6Al-4V hybrid structure mechanical properties-Wrought and additive manufactured powder-bed material
54. Rebuilding of metal components with laser cladding forming10.1016/j.apsusc.2005.10.025 ↗