journal article·2025-06

High-cycle fatigue properties of hot-rolled bonding titanium-clad bimetallic steel

Huiyong Ban, Chenyang Huang, Yongjiu Shi, Letian Hai

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Material Properties and Applications · Surface Treatment and Residual Stress

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Corrosion protection of steel elements in façade systems – A review
2. Manufacturing technology and application trends of titanium clad steel plates10.1016/S1006-706X(15)30099-6 ↗
3. Corrosion of titanium: Part 1: Aggressive environments and main forms of degradation
4. Administration of Quality Supervision · 2019
5. Huiyong Ban, Yongjiu Shi. An innovative high performance steel product for structural engineering: Bimetallic steel. Proceedings of the International Conference on Engineering Research and Practice for Steel Construction, Hong Kong, China 2018. pp. 424-430.
6. Huiyong Ban, Yongjiu Shi, Xiaoyan Tao. Use of clad steel in engineering structures. Proceedings of The Fifteenth East Asia-Pacific Conference on Structural Engineering & Construction (EASEC-15), October 11-13, China 2017, pp. 1167-1173.
7. Application countermeasures of the manufacturing processes of titanium-steel composite plates10.1088/2053-1591/aaebf0 ↗
8. Administration of Quality Supervision · 2008
9. Administration of Quality Supervision · 2009
10. Japanese Industrial Standards Committee Standards Board, JIS G 3603:2012 Titanium clad steels, Japanese Standards Association, Tokyo, 2012(in Japanese).
11. American Society for Testing and Materials International · 2019
12. Manufacturing process and interface properties of vacuum rolling large-area titanium-steel cladding plate10.3103/S1067821219020032 ↗
13. Explosive welding of titanium/stainless steel by controlling energetic conditions10.2320/matertrans.47.2049 ↗
14. Material properties and stress-strain curves for titanium-clad bimetallic steels10.1016/j.jcsr.2019.105756 ↗
15. Study on the material properties and constitutive model of titanium-clad steel
16. Bonding condition of rolled titanium clad steels10.2355/tetsutohagane1955.72.6_671 ↗
17. Bond strength of explosively welded specimens10.1016/j.matdes.2007.06.010 ↗
18. Dehan Yang, Zongan Luo, Guangming Xie, Tao Jiang, Suang Zhao, R.D.K. Misra. Interfacial microstructure and properties of a vacuum roll-cladding titanium-steel clad plate with a nickel interlayer. Materials Science and Engineering: A. 753 (2019), 49-58.10.1016/j.msea.2019.03.008 ↗
19. Cyclic behavior of hot-rolled titanium-clad bimetallic steel under large plastic strain reversals10.1016/j.jcsr.2023.108112 ↗
20. Experimental cyclic behaviour and constitutive modelling of hot-rolled titanium-clad bimetallic steel10.1016/j.conbuildmat.2022.129591 ↗
21. Fatigue properties of titanium-clad bimetallic steel butt-welded joints10.1016/j.tws.2024.112149 ↗
22. Fatigue tests and metallographic of explosively cladded steel-titanium bimetal10.2478/amm-2014-0265 ↗
23. Fatigue phenomena in explosively welded steel–titanium clad components subjected to push–pull loading10.1016/j.ijfatigue.2012.10.007 ↗
24. The influence of heat treatment parameters on the cracks growth under cyclic bending in St-Ti clad obtained by explosive welding10.3390/met9030338 ↗
25. Research on high-cycle fatigue properties of hot rolled titanium-clad bimetallic steel with low bonding strength
26. High-cycle fatigue properties of explosion bonded titanium-clad bimetallic steel10.1016/j.ijfatigue.2022.107499 ↗
27. High-cycle fatigue properties of titanium-clad bimetallic steel with different interfacial conditions10.3390/buildings13030758 ↗
28. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
29. Fatigue crack initiation and propagation behavior of forging die steels10.1016/j.ijfatigue.2009.07.020 ↗
30. Effect of surface roughness on the fatigue failure and evaluation of TC17 titanium alloy10.1080/02670836.2021.1885777 ↗
31. Lee · 2005
32. inistry of Housing and Urban-Rural Construction of the People's Republic of China, Administration of Quality Supervision, Inspection and Quarantine of People's Republic of China, GB 50017-2017 Standard for design of steel structures. China Architecture & Building Press, Beijing 2017 (in Chinese).
33. Administration of Quality Supervision · 2007
34. American Society for Testing and Materials International · 2015
35. European Committee for Standardization (CEN), EN 1993-1-1 Eurocode 3 Design of Steel Structures–Part 1-1: General rules and rules for buildings, European Committee for Standardization (CEN), Brussels, 2022.
36. Letian Hai, HuiyongBan, Chenyang Huang, Yongjiu Shi. Experimental cyclic behaviour and constitutive modelling of hot-rolled titanium-clad bimetallic steel. Construction and Building Materials, 360(2022), 129591.10.1016/j.conbuildmat.2022.129591 ↗
37. Administration of Quality Supervision, Inspection and Quarantine of People's Republic of China, Standardization Administration of China, GB/T 228.1–2010 Metallic Materials - Tensile Testing - Part 1: Method of Test at Room Temperature. China Standards Press, Beijing, 2010 (in Chinese).
38. The International Organization for Standardization (ISO), ISO 6892-1:2019 Metallic materials—Tensile testing—Part 1: Method of test at room temperature. The International Organization for Standardization (ISO), 2019.
39. Administration of Quality Supervision · 2008
40. The International Organization for Standardization (ISO), ISO 1099: 2017 Metallic materials—Fatigue testing—Axial force-controlled method. The International Organization for Standardization (ISO), 2017.
41. American Society for Testing and Materials International · 2015
42. Frequency effect and influence of testing technique on the fatigue behaviour of quenched and tempered steel and aluminium alloy10.1016/j.ijfatigue.2016.05.013 ↗
43. Effect of test frequency on fatigue strength of low carbon steel10.1111/j.1460-2695.2009.01350.x ↗
44. European Committee for Standardization (CEN), EN 1993-1-9 Eurocode 3, Design of Steel Structures—Part 1-9: Fatigue, Comité Européen de Normalisation, Brussels, 2005.
45. Fatigue analysis of the fiber reinforced additively manufactured objects10.1007/s00170-018-2398-7 ↗
46. Low-cycle fatigue behaviour and fracture feature of stainless-clad bimetallic steel10.1016/j.jcsr.2022.107437 ↗
47. Spiegel · 2001 · 114
48. Shisong Mao, Yiming Cheng, Xiaolong Pu. Probability and statistics. Higher Education Press, Beijing, 2011, 396 (in Chinese).
49. American Institute of Steel Construction · 2016
50. British Standards Institution · 2015