Effect of grain boundary phase formed by Mn addition on initiation and propagation of fatigue cracks in homogenized Cu-6Ni-1.3Si alloy
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Microstructure and mechanical properties · Microstructure and Mechanical Properties of Steels · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Increasing strength and conductivity of Cu alloy through abnormal plastic deformation of an intermetallic compound10.1038/srep30907 ↗
2. Alloy design strategies to increase strength and its trade-offs together10.1016/j.pmatsci.2020.100720 ↗
3. Recent development of advanced precipitation-strengthened Cu alloys with high strength and conductivity: a review10.1016/j.pmatsci.2023.101141 ↗
4. Microstructure and aging behavior of Cu-Be alloy processed by high-pressure torsion10.4028/www.scientific.net/MSF.783-786.2707 ↗
5. Deformation of Cu-Be-Co alloys by aging at 593 K10.2320/matertrans.M2011057 ↗
6. Microstructure and mechanical properties of Cu-Ni-Si alloys10.1016/j.msea.2006.12.163 ↗
7. Structure and strength of the age hardened Cu-Ni-Si alloy10.1016/S0254-0584(02)00451-0 ↗
8. Effect of inclusion on strength and conductivity of Cu-Ni-Si alloys with discontinuous precipitation10.1016/j.jallcom.2020.156006 ↗
9. Fatigue crack initiation and propagation behaviors of solution-treated and air-cooled Cu-6Ni-1.5Si alloy strengthened by precipitation hardening10.1016/j.ijfatigue.2019.02.004 ↗
10. Precipitate structure in a Cu–Ni–Si alloy10.1007/BF00356596 ↗
11. Effect of alloy composition on precipitation behavior in Cu–Ni–Si alloys10.2320/jinstmet1952.62.4_301 ↗
12. Orientation and diffraction patterns of δ-Ni2Si precipitates in Cu–Ni–Si alloy10.1016/j.jallcom.2012.12.154 ↗
13. The crystallographic and morphological evolution of the strengthening precipitates in Cu–Ni–Si alloys10.1016/j.actamat.2012.10.031 ↗
14. Microstructure-dependent fatigue behavior of aged Cu-6Ni-1.5Si alloy with discontinuous/cellular precipitates10.1016/j.msea.2019.01.057 ↗
15. Effect of pre–deformation before aging on discontinuous precipitation behavior in Cu–Ni–Si alloys10.1080/09500839.2020.1844916 ↗
16. Enhanced strength of Cu-Ni-Si alloy via heterogeneous nucleation at grain boundaries during homogenization10.1016/j.matchar.2024.114198 ↗
17. Fatigue of metals, in: G.E. Dieter (Ed.), Mechanical Metallurgy–2nd Edition, McGraw-Hill (1976) 403–450.
18. Role of microstructure on initiation and propagation of fatigue cracks in precipitate strengthened Cu–Ni–Si alloy10.1016/j.ijfatigue.2016.01.004 ↗
19. Influence of grain size and precipitation hardening on high cycle fatigue performance of CuNiSi alloys10.1016/j.msea.2016.12.082 ↗
20. Characterization of uniaxial fatigue behavior of precipitate strengthened Cu-Ni-Si alloy(SICLANIC®)
21. Fatigue crack growth behaviour of precipitate-strengthened CuNi2Si alloy under different loading modes10.3390/ma13102228 ↗
22. Simultaneous increase in electrical conductivity and fatigue strength of Cu–Ni–Si alloy by utilizing discontinuous precipitates10.1016/j.matlet.2021.129353 ↗
23. Influence of surface micro shot peening on short fatigue crack behavior of CuNi2Si alloy
24. Physical background of significant increase in mechanical properties and fatigue strength of groove-rolled Cu-Ni-Si alloy with discontinuous precipitates10.1016/j.jallcom.2023.169569 ↗
25. On the crystal structure of the Mn–Ni–Si G-phase10.1016/j.jallcom.2008.01.142 ↗
26. Magnetic and structural studies of G‑phase compound Mn6Ni16Si710.1021/acs.inorgchem.8b01964 ↗
27. Helium behaviors at Mn6Ni16Si7 precipitate in α-Fe: insights from ab initio modeling10.1016/j.commatsci.2020.109735 ↗
28. The intergranular precipitation behavior of G phase in a high-performance complex cast Cu-Ni-Al alloy10.1016/j.matchar.2022.112611 ↗
29. Statical investigation of the behaviour of small cracks and fatigue life in carbon steels with different ferrite grain size10.1111/j.1460-2695.1994.tb00262.x ↗
30. A small-crack growth law and its related phenomena10.1016/0013-7944(92)90297-R ↗
31. Microstructure and fatigue properties of Cu-Ni-Si alloy strengthened by Ni2Si intrametric compounds
32. Fatigue life prediction of heat-treated carbon steels and low alloy steels based on a small-crack growth law10.1111/j.1460-2695.1994.tb00799.x ↗
33. Growth behavior and crack distribution characteristics of small surface cracks of age-hardened Al-alloy 2017-T410.2472/jsms.45.675 ↗
34. The Behaviour of Short Fatigue Cracks. K.J. Miller, E.R. de los Rios, (Eds.), vol. 1. EGF-Pub; 1986. MEP: Small Fatigue Cracks-Mechanics, Mechanisms and Applications, K.S. Ravichandran, R.O. Ritchie, Y. Murakami (Eds.), Elsevier; 1999.