Influence of dynamic strain aging on low-cycle fatigue behavior in nano-sized κ-carbide strengthened FeMnAlC lightweight steel
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · High Temperature Alloys and Creep · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (66)
Show source-provided references
1. A general perspective of Fe-Mn-Al-C steels10.1007/s10853-018-2551-6 ↗
2. High-strength Fe–20Mn–Al–C-based alloys with low density10.2355/isijinternational.50.893 ↗
3. Alloy design, combinatorial synthesis, and microstructure-property relations for low-density Fe-Mn-Al-C austenitic steels10.1007/s11837-014-1032-x ↗
4. Phase transformations in FeMnAlC austenitic steels with Si addition10.1007/s11661-002-0345-5 ↗
5. High Manganese and aluminum steels for the military and transportation industry10.1007/s11837-014-1068-y ↗
6. Microstructural developments and tensile properties of lean Fe-Mn-Al-C lightweight steels10.1007/s11837-014-1128-3 ↗
7. Current state of Fe-Mn-Al-C low density steels10.1016/j.pmatsci.2017.05.002 ↗
8. Effect of Nb on high-temperature properties for ferritic stainless steel10.1016/1359-6462(96)00214-X ↗
9. Effect of alloying additions on phase equilibria and creep resistance of alumina-forming austenitic stainless steels10.1007/s11661-009-9886-1 ↗
10. Effect of Niobium Addition on the high-temperature oxidation behavior of 22Cr25NiWCoCu stainless steel in air10.3390/met9090975 ↗
11. Role of Nb addition on microstructural stability and deformation behaviors of FeMnAlC lightweight steels at 400 °C10.1007/s11661-021-06379-2 ↗
12. Manganese as an austenite stabilizer in Fe Cr Mn C steels10.1016/0025-5416(88)90539-3 ↗
13. On the austenite stability of cryogenic Ni steels: microstructural effects: a review10.1007/s10853-021-06068-w ↗
14. Element partitioning effect on microstructure and mechanical property of the micro-laminated Fe-Mn-Al-C dual phase steel10.1016/j.msea.2015.12.029 ↗
15. A Literature review of age hardening Fe-Mn-Al-C alloys
16. Electron microscope observations of phase decompositions in an austenitic Fe-8.7Al-29.7Mn-1.04C alloy10.1016/1044-5803(90)90055-O ↗
17. Atomistic investigations of κ-carbide precipitation in austenitic Fe-Mn-Al-C lightweight steels and the effect of Mo addition10.1016/j.scriptamat.2016.08.036 ↗
18. Simulation of κ-carbide precipitation kinetics in aged low-density Fe-Mn-Al-C steels and its effects on strengthening10.1007/s12540-018-0089-4 ↗
19. Phase transformation of the L12 phase to kappa-carbide after spinodal decomposition and ordering in an Fe-C-Mn-Al austenitic steel10.1016/j.msea.2015.06.096 ↗
20. Stacking fault energy in austenitic steels determined by using in situ X-ray diffraction during bending10.1107/S1600576714007109 ↗
21. Correlations between the calculated stacking fault energy and the plasticity mechanisms in Fe-Mn-C alloys10.1016/j.msea.2004.01.059 ↗
22. Influence of original austenite grain size on tensile properties of a high-manganese transformation-induced plasticity (TRIP) steel10.1016/j.msea.2017.12.107 ↗
23. The influence of aluminum content to the stacking fault energy in Fe-Mn-Al-C alloy system10.1007/BF01045392 ↗
24. Stacking fault energy determination in Fe-Mn-Al-C austenitic steels by X-ray diffraction10.3390/met11111701 ↗
25. On the origin of planar slip in f.c.c. alloys10.1016/0001-6160(89)90143-0 ↗
26. Microstructural evolution of Cr-Mn-N austenitic steels during cold work hardening10.1016/j.msea.2006.04.020 ↗
27. Direct observation of chemical short-range order in 25 wt% Mn steel via transmission electron microscopy10.1016/j.scriptamat.2022.114642 ↗
28. An ab initio study of carbon-induced ordering in austenitic Fe-Mn-Al-C alloys
29. Origin of extended tensile ductility of a Fe-28Mn-10Al-1C steel10.1007/s11661-009-9862-9 ↗
30. Atomistic study of nano-sized κ-carbide formation and its interaction with dislocations in a cast Si added FeMnAlC lightweight steel10.1016/j.msea.2016.07.029 ↗
31. Microband induced plasticity and the temperature dependence of the mechanical properties of a carbon-doped FeNiMnAlCr high entropy alloy10.1016/j.matchar.2018.03.017 ↗
32. Microband-induced plasticity in a high Mn-Al-C light steel10.1016/j.msea.2008.05.042 ↗
33. Microstructures and mechanical properties of high-strength Fe-Mn-Al-C light-weight TRIPLEX steels10.1002/srin.200606440 ↗
34. Investigations of the microstructure evolution and tensile deformation behavior of austenitic Fe-Mn-Al-C lightweight steels and the effect of Mo addition10.1016/j.actamat.2018.01.051 ↗
35. Tensile deformation of low-density Fe-Mn-Al-C austenitic steels at ambient temperature10.1016/j.scriptamat.2012.09.031 ↗
36. Effect of aging on the microstructure and deformation behavior of austenite base lightweight Fe–28Mn–9Al–0.8C steel10.1016/j.scriptamat.2010.07.036 ↗
37. On the influence of κ-carbides on the low-cycle fatigue behavior of high-Mn light-weight steels10.1016/j.ijfatigue.2021.106327 ↗
38. Serrated plastic flow10.1007/BF02743993 ↗
39. Serrated plastic flow revisited10.4028/www.scientific.net/SSP.42-43.257 ↗
40. Serrated flow and tensile properties of a Mg-Y-Nd alloy10.1016/j.scriptamat.2003.09.039 ↗
41. Effects of temperature and strain rate on tensile properties and dynamic strain aging behaviour of LPBF Hastelloy X
42. Dynamic strain aging behavior of accident tolerance fuel cladding FeCrAl-based alloy for advanced nuclear energy10.1007/s10853-021-05820-6 ↗
43. Fatigue performance improvement in AISI 4140 steel by dynamic strain aging and dynamic precipitation during warm laser shock peening10.1016/j.actamat.2010.10.032 ↗
44. Cyclic deformation behavior and dynamic strain aging of 316LN stainless steel under low cycle fatigue loadings at 550 °C10.1016/j.msea.2021.141411 ↗
45. Mechanistic modeling of dynamic strain aging in austenitic stainless steels10.1016/S1044-5803(98)00031-X ↗
46. Effect of dynamic strain aging on high temperature properties of austenitic stainless steel10.1016/j.msea.2004.03.004 ↗
47. Effects of aging heat-treatment on dynamic strain aging behavior in high-Mn lightweight steel10.1016/j.matchar.2020.110316 ↗
48. Dynamic strain aging in Fe-Mn-Al-C lightweight steel10.1080/09500839.2020.1768603 ↗
49. Micro-structure refinement in low carbon high manganese steels through Ti-deoxidation: austenite grain growth and decomposition10.2355/isijinternational.49.1036 ↗
50. Effect of Mg-Ti deoxidation on the formation behavior of equiaxed crystals during rapid solidification of iron alloys10.1002/srin.201300203 ↗
51. Thermodynamic analysis of inclusions in Ti-deoxidized steels10.1034/j.1600-0692.2000.d01-24.x ↗
52. Direct observation of dislocation plasticity in high-Mn lightweight steel by in-situ TEM10.1038/s41598-019-51586-y ↗
53. Tensile deformation of low density duplex Fe-Mn-Al-C steel10.1016/j.matdes.2015.03.043 ↗
54. Effect of dynamic strain aging on isotropic hardening in low cycle fatigue for carbon manganese steel10.1016/j.msea.2013.09.058 ↗
55. A new strengthening mechanism driven by disruptive shear and solute segregation during warm rolling in 1.4 GPa class 12.5 wt% Al added-FeMnC ultra-lightweight steel10.1016/j.jmst.2023.01.047 ↗
56. Dynamic strain aging effect on the fatigue resistance of type 316L stainless steel10.1016/j.ijfatigue.2005.06.037 ↗
57. Role of dynamic strain aging on low cycle fatigue and crack propagation of type 316L(N) stainless steel10.1016/S0142-1123(03)00120-8 ↗
58. The low-cycle fatigue property, damage mechanism and life prediction of compacted graphite iron: influence of strain rate10.1016/j.ijfatigue.2020.105576 ↗
59. Mechanism of dynamic strain aging and characterization of its effect on the low-cycle fatigue behavior in type 316L stainless steel10.1016/j.jnucmat.2004.12.012 ↗
60. Serrated flow behavior in AL6XN austenitic stainless steel10.1016/j.jnucmat.2009.08.002 ↗
61. Creep and low-cycle fatigue behavior of ferritic Fe-24Cr-4Al alloy in the dynamic strain aging regime: effect of aluminum addition10.1007/s11661-997-0271-7 ↗
62. Serration behavior and negative strain rate sensitivity of Al0.1CoCrFeNi high entropy alloy10.1016/j.intermet.2016.12.016 ↗
63. Negative strain rate sensitivity in bulk metallic glass and its similarities with the dynamic strain aging effect during deformation10.1063/1.2234309 ↗
64. A new explanation for the effect of dynamic strain aging on negative strain rate sensitivity in Fe–30Mn–9Al–1C steel10.3390/ma12203426 ↗
65. High strain rate behavior of metals10.1115/1.3120862 ↗
66. Strain hardening and strain rate sensitivity behaviors of advanced high strength steels10.1016/S1006-706X(13)60114-4 ↗