Toward developing remanufactured Ti6Al4V alloys with high fatigue crack growth resistance by in-situ cooling during laser remanufacturing

Wanli Ling, Xiaoping Wang, Qiyu Gao, Zhuanni Gao, Xiaoming Wang, Xiaohong Zhan

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Technology Assessment and Management

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (65)

Show source-provided references
1. Fatigue limit prediction model and fatigue crack growth mechanism for selective laser melting Ti6Al4V samples with inherent defects10.1016/j.ijfatigue.2020.106008 ↗
2. Effects of build direction on tensile and fatigue performance of selective laser melting Ti6Al4V titanium alloy10.1016/j.ijfatigue.2019.105260 ↗
3. Quasi-static and dynamic loading responses and constitutive modeling of titanium alloys10.1016/j.ijplas.2003.06.005 ↗
4. Enhanced tensile ductility of an additively manufactured near-α titanium alloy by microscale shear banding10.1016/j.ijplas.2022.103387 ↗
5. Improving the high cycle fatigue property of Ti6Al4V ELI alloy by optimizing the surface integrity through electric pulse combined with ultrasonic surface rolling process10.1016/j.jmst.2023.06.029 ↗
6. Strengthening mechanism in thermomechanical fatigue properties of Ti6Al4V titanium alloy by laser shock peening10.1016/j.ijfatigue.2023.107631 ↗
7. Component design optimisation based on artificial intelligence in support of additive manufacturing repair and restoration: Current status and future outlook for remanufacturing10.1016/j.jclepro.2021.126401 ↗
8. Environmental life cycle assessment of remanufactured engines with advanced restoring technologies10.1016/j.rcim.2019.04.005 ↗
9. Environmental benefits of remanufacturing: a case study of cylinder heads remanufactured through laser cladding10.1016/j.jclepro.2016.06.049 ↗
10. MIL-STD-1530D. Department of Defense Standard Practice Aircraft Structural Integrity Program (ASIP) 2016. http://everyspec.com/MIL-STD/MIL-STD-1500-1599/MIL-STD-1530D_55392/ (accessed May 13, 2024).
11. Structures Bulletin EZ-SB-19-01, Durability and Damage Tolerance Certification for Additive Manufacturing of Aircraft Structural Metallic Parts, Dayton Aerospace 2019. https://daytonaero.com/usaf-structures-bulletins-library/ (accessed May 13, 2024).
12. Microstructures and mechanical properties of Ti6Al4V alloy repaired by the technology of point-mode forging and laser repairing10.1016/j.optlastec.2021.107410 ↗
13. Nanocrystallization of interfacial microstructure of deformed particles in cold sprayed Ti6Al4V deposits10.1016/j.matdes.2021.110117 ↗
14. Evaluation of electron beam wire-fed deposition technology for titanium compressor blade repair
15. Microstructure of a coated single crystalline René N5 part repaired by epitaxial laser deposition
16. Investigation of a novel functionally graded material for the repair of premium hypereutectoid rails using laser cladding technology10.1016/j.compositesb.2017.07.089 ↗
17. Investigation of the underwater laser directed energy deposition technique for the on-site repair of HSLA-100 steel with excellent performance
18. Microstructure formation of Ti-6Al-4 V in synchronous induction assisted laser deposition10.1016/j.matdes.2018.11.008 ↗
19. Laser cladding as repair technology for Ti–6Al–4V alloy: Influence of building strategy on microstructure and hardness10.1016/j.matdes.2015.07.035 ↗
20. Fracture toughness and fatigue crack growth rate properties of AM repaired Ti–6Al–4V by Direct Energy Deposition10.1016/j.msea.2021.141701 ↗
21. Achieving fully-equiaxed fine β-grains in titanium alloy produced by additive manufacturing10.1080/21663831.2022.2115323 ↗
22. In-situ investigation on tensile deformation and fracture behaviors of inhomogeneous microstructure during laser repair of Ti-6Al-4V titanium alloy10.1016/j.engfracmech.2023.109538 ↗
23. Synergetic strengthening of additively manufactured (CoCrFeMnNi)99C1 high-entropy alloy by heterogeneous anisotropic microstructure
24. Designing against phase and property heterogeneities in additively manufactured titanium alloys10.1038/s41467-022-32446-2 ↗
25. Crack path selection at the interface of wrought and wire+arc additive manufactured Ti–6Al–4V10.1016/j.matdes.2016.05.027 ↗
26. Heterogeneous precipitate microstructure design in β-Ti alloys by regulating the cooling rate10.1016/j.actamat.2024.119810 ↗
27. Underlying factors determining grain morphologies in high-strength titanium alloys processed by additive manufacturing10.1038/s41467-023-38885-9 ↗
28. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
29. Beyond the orthogonal: on the influence of build orientation on fatigue crack growth in SLM Ti-6Al-4V10.1016/j.ijfatigue.2018.06.038 ↗
30. Modelling the variability and the anisotropic behaviour of crack growth in SLM Ti-6Al-4V10.3390/ma14061400 ↗
31. Further studies into crack growth in additively manufactured materials10.3390/ma13102223 ↗
32. Deposition of Ti–6Al–4V using laser and wire, part I: microstructural properties of single beads10.1016/j.surfcoat.2011.07.095 ↗
33. Effect of different welding procedures on microstructure and mechanical property of TA15 titanium alloy joint10.1515/htmp-2022-0022 ↗
34. Lütjering G, Williams JC. Titanium. Berlin, Heidelberg: Springer; 2003. DOI: 10.1007/978-3-540-71398-2.10.1007/978-3-540-71398-2 ↗
35. Enriched analytical solutions for additive manufacturing modeling and simulation
36. Influence of 2D forging processes and boron contents on the microstructures and mechanical properties of near α titanium alloys10.1016/j.intermet.2021.107181 ↗
37. Enhanced extra-long life fatigue resistance of a bimodal titanium alloy by laser shock peening10.1016/j.ijfatigue.2020.105868 ↗
38. Micro-crystallographically unraveling strength-enhanced behaviors of the heavy-thick Ti-6Al-4V welded joint10.1016/j.matchar.2022.111893 ↗
39. The interface effect on crack nucleation under dwell fatigue loading in dual-phase Ti alloy10.1016/j.ijplas.2023.103816 ↗
40. Effects of rapid heating on non-equilibrium microstructure evolution and strengthening mechanisms of titanium alloy10.1016/j.msea.2023.145337 ↗
41. Laser surface treatment of α-β titanium alloy to develop a β-rich phase with very high hardness10.1016/j.jmatprotec.2020.116873 ↗
42. Variant selection within one β grain in laser solid formed Ti-6Al-4V alloys10.1016/j.matchar.2022.111744 ↗
43. Effect of cooling rate on α variant selection and microstructure evolution in a near β Ti–5Al–3Mo–3V–2Cr–2Zr–1Nb–1Fe alloy10.1016/j.jallcom.2020.155728 ↗
44. Fatigue crack growth behavior of an additively manufactured titanium alloy: effects of spatial and crystallographic orientations of α lamellae10.1016/j.ijplas.2023.103819 ↗
45. Effect of primary α phase on the fatigue crack path of laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe near β titanium alloy10.1016/j.ijfatigue.2018.06.041 ↗
46. Effect of multi-stage heat treatment on the microstructure and mechanical properties of Ti–6Al–4V alloy deposited by high-power laser melting deposition10.1016/j.msea.2024.146226 ↗
47. Effect of HIP post-processing at 850 °C/200 MPa in the fatigue behavior of Ti-6Al-4V alloy fabricated by Selective Laser Melting10.1016/j.ijfatigue.2022.107097 ↗
48. Hierarchical nano-martensite-engineered a low-cost ultra-strong and ductile titanium alloy10.1038/s41467-022-33710-1 ↗
49. Defect formation mechanism of laser additive manufacturing joint for large-thickness Ti6Al4V titanium alloy with Y2O3 nanoparticles10.1016/j.optlastec.2022.108648 ↗
50. Texture induced planar anisotropy of dwell fatigue response in titanium: Insights from experiments and crystal plasticity simulations10.1016/j.ijplas.2021.103140 ↗
51. Long fatigue crack growth behavior of Ti–6Al–4V produced via high-power laser directed energy deposition10.1016/j.msea.2021.141392 ↗
52. The influence of the microtexture and orientation of columnar grains on the fatigue crack growth of directed energy deposited Ti-6.5Al-2Zr-Mo-V alloys
53. Unravelling the competitive effect of microstructural features on the fracture toughness and tensile properties of near beta titanium alloys10.1016/j.jmst.2021.04.032 ↗
54. Effects of compressive residual stress on short fatigue crack growth in a nickel-based superalloy10.1016/j.ijfatigue.2017.11.010 ↗
55. The effect of laser shock peening, shot peening and their combination on the microstructure and fatigue properties of Ti-6Al-4V titanium alloy10.1016/j.ijfatigue.2021.106465 ↗
56. Fatigue crack growth in residual stress fields of laser shock peened Ti6Al4V titanium alloy10.1016/j.jallcom.2021.161427 ↗
57. Residual stress evaluation in selective-laser-melting additively manufactured titanium (Ti-6Al-4V) and inconel 718 using the contour method and numerical simulation
58. Assessment of residual stresses in welded T-joints using contour method10.1016/j.tws.2023.110966 ↗
59. Distribution characteristics of residual stresses in typical wall and pipe components built by wire arc additive manufacturing10.1016/j.jmapro.2022.08.010 ↗
60. Experimental-numerical study of laser-shock-peening-induced retardation of fatigue crack propagation in Ti-17 titanium alloy10.1016/j.ijfatigue.2020.106081 ↗
61. Combining manufacturing of titanium alloy through direct energy deposition and laser shock peening processes10.1016/j.matdes.2021.109626 ↗
62. A critical analysis of crack propagation laws10.1115/1.3656900 ↗
63. Subcritical crack growth: the microscopic origin of Paris’ law10.1103/PhysRevLett.100.195503 ↗
64. Fatigue crack growth behavior and microstructural mechanisms in Ti-6Al-4V manufactured by laser engineered net shaping10.1016/j.ijfatigue.2016.08.009 ↗
65. Effect of deposition strategies on fatigue crack growth behaviour of wire + arc additive manufactured titanium alloy Ti–6Al–4V10.1016/j.msea.2021.141194 ↗