Understanding of the fatigue crack nucleation in metallic sealing rings by explicitly incorporating the deformation history from manufacturing to service

Zebang Zheng, Pandi Zhao, Mei Zhan, Hongwei Li, Yudong Lei, M.W. Fu

Abstract

202309 bcch ; RGC ; Others ; Shenzhen Science and Technology Program; Hong Kong Scholar Program; National Natural Science Foundation of China; The Hong Kong Polytechnic University; GRF; National Science and Technology Major Project ; Published ; 24 months ; Green (AAM)
The source flagged this abstract for review. Check formulas and completeness against the original publication.
Source: openaire · Quality: needs review · Source record ↗
Source flags: short_text

Research context

OpenAlex topics: Fatigue and fracture mechanics · Mechanical stress and fatigue analysis · Metal Forming Simulation Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Microstructural and geometrical size effects on the fatigue of metallic materials10.1016/j.ijmecsci.2021.107058 ↗
2. The roles of rise and fall time in load shedding and strain partitioning under the dwell fatigue of titanium alloys with different microstructures10.1016/j.ijplas.2021.103161 ↗
3. Cyclic plasticity and thermomechanical alleviation in titanium alloys
4. The Structure Optimization Design for the W-Type Metallic Sealing Ring Based on the MOGA Algorithm10.4028/www.scientific.net/AMM.727-728.541 ↗
5. Wall thickness variation of a superalloy thin-walled w-section seal ring during roll forming
6. Enhanced fatigue resistance of Cu with a gradient nanograined surface layer10.1016/j.scriptamat.2013.01.031 ↗
7. Crystal plasticity modelling and HR-DIC measurement of slip activation and strain localization in single and oligo-crystal Ni alloys under fatigue10.1016/j.ijplas.2016.10.001 ↗
8. Experimental and computational studies of low cycle fatigue crack nucleation in a polycrystal10.1016/j.ijplas.2006.07.001 ↗
9. The role of heterogeneous deformation on damage nucleation at grain boundaries in single phase metals10.1016/j.ijplas.2008.09.002 ↗
10. Experimental study of the impact of geometrical defects on the high cycle fatigue behavior of polycrystalline aluminium with different grain sizes10.1016/j.ijfatigue.2017.12.009 ↗
11. Taylor DD. Sealing ring with e-shaped radial section 1965.
12. Formability enhancement in hot spinning of titanium alloy thin-walled tube via prediction and control of ductile fracture10.1016/j.cja.2021.01.002 ↗
13. Deformation mode and wall thickness variation in conventional spinning of metal sheets10.1016/j.ijmachtools.2021.103846 ↗
14. A comparative study of three forms of an uncoupled damage model as fracture judgment for thin-walled metal sheets10.1016/j.tws.2021.108321 ↗
15. An anisotropic constitutive model for forming of aluminum tubes under both biaxial tension and pure shear stress states10.1016/j.ijplas.2022.103259 ↗
16. On the determination of forming limits in thin-walled tubes10.1016/j.ijmecsci.2019.03.020 ↗
17. Zhang H, Zhan M, Zheng Z, Li R, Lyu W, Lei Y. A Systematic Study on the Effects of Process Parameters on Spinning of Thin-Walled Curved Surface Parts With 2195 Al-Li Alloy Tailor Welded Blanks Produced by FSW. Front Mater 2021;8. 10.3389/fmats.2021.809018.10.3389/fmats.2021.809018 ↗
18. Failure Analysis and Optimized Verification of Metal W-sealing Ring of Aero-engine at High Temperature
19. External-internal composite spinning technology for forming thin-walled Ω-sectioned ring of superalloy10.1016/j.jmatprotec.2020.117004 ↗
20. A study on the sealing performance of metallic C-rings in reactor pressure vessel10.1016/j.nucengdes.2014.07.006 ↗
21. Deformation Characteristics and Sealing Performance of Metallic O-rings for a Reactor Pressure Vessel10.1016/j.net.2015.11.009 ↗
22. Stress and thickness calculation of a bolted flat cover with double metal sealing rings10.1007/s41365-018-0457-2 ↗
23. Parametric Analysis of Wave-shaped Metal Sealing Ring Based on Hierarchical Solution Method
24. A model for reliability assessment of sealing performance of the C-shaped metal sealing ring at the outlet of the subsea tubing hanger10.1016/j.oceaneng.2021.110311 ↗
25. Sealing Failure Analysis on V-Shaped Sealing Rings of an Inserted Sealing Tool Used for Multistage Fracturing Processes10.3390/en11061432 ↗
26. Analysis of Influence of Structures and Strength about Corrugated Radius of Metallic Sealing Ring10.4028/www.scientific.net/AMR.971-973.872 ↗
27. Mechanical behavior and sealing performance of metal sealing system in roller cone bits10.1007/s12206-019-0533-5 ↗
28. Rate sensitivity in discrete dislocation plasticity in hexagonal close-packed crystals10.1016/j.actamat.2016.01.035 ↗
29. Lengthscale-dependent, elastically anisotropic, physically-based hcp crystal plasticity: Application to cold-dwell fatigue in Ti alloys10.1016/j.ijplas.2006.10.013 ↗
30. Discrete dislocation, crystal plasticity and experimental studies of fatigue crack nucleation in single-crystal nickel
31. Microstructurally-sensitive fatigue crack nucleation in Ni-based single and oligo crystals10.1016/j.jmps.2017.05.012 ↗
32. Is stored energy density the primary meso-scale mechanistic driver for fatigue crack nucleation?10.1016/j.ijplas.2017.11.005 ↗
33. Crystal plasticity and high-resolution electron backscatter diffraction analysis of full-field polycrystal Ni superalloy strains and rotations under thermal loading10.1016/j.actamat.2014.07.036 ↗
34. Slip localization and fatigue crack nucleation near a non-metallic inclusion in polycrystalline nickel-based superalloy10.1016/j.msea.2015.06.070 ↗
35. Statistically Equivalent Representative Volume Elements for Unidirectional Composite Microstructures: Part I - Without Damage10.1177/0021998305055273 ↗
36. Statistically Equivalent Representative Volume Elements for Unidirectional Composite Microstructures: Part II - With Interfacial Debonding10.1177/0021998305055274 ↗
37. Microstructure and Property-Based Statistically Equivalent Representative Volume Elements for Polycrystalline Ni-Based Superalloys Containing Annealing Twins10.1007/s11661-018-4858-y ↗
38. Microstructure and property based statistically equivalent RVEs for polycrystalline-polyphase aluminum alloys10.1016/j.ijplas.2018.12.002 ↗
39. A microstructure-based porous crystal plasticity FE model for additively manufactured Ti-6Al-4V alloys10.1016/j.ijplas.2022.103254 ↗
40. A stored energy criterion for fatigue crack nucleation in polycrystals10.1016/j.ijfatigue.2014.06.001 ↗
41. On the Macroscopic Description of Stored Energy and Self Heating During Plastic Deformation10.1016/S0749-6419(97)00063-6 ↗
42. A microstructure-sensitive driving force for crack growth10.1016/j.jmps.2018.07.005 ↗
43. A mechanistic modelling methodology for microstructure-sensitive fatigue crack growth10.1016/j.jmps.2018.11.023 ↗
44. Microstructurally-sensitive fatigue crack growth in HCP, BCC and FCC polycrystals10.1016/j.jmps.2019.02.012 ↗
45. Microstructure-interacting short crack growth in blocky alpha Zircaloy-4
46. The dislocation configurational energy density in discrete dislocation plasticity10.1016/j.jmps.2019.04.015 ↗
47. He Y, Li Z. Personal communication 2021.10.1155/2021/5568351 ↗
48. The effect of strain rate asymmetry on the Bauschinger effect: A discrete dislocation plasticity analysis10.1016/j.jmrt.2021.12.107 ↗