journal article·2024-03

Very high cycle fatigue rupture mode at high temperatures of Ni-based superalloys coated with a slurry aluminide

Luciana Maria Bortoluci Ormastroni, Thomas Kepa, Alice Cervellon, Patrick Villechaise, Fernando Pedraza, Jonathan Cormier

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High Temperature Alloys and Creep · Nuclear Materials and Properties · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Caron P, Ohta Y, Nakagawa YG, Khan T. Creep deformation anisotropy in single crystal superalloys. Proceedings of the International Symposium on Superalloys 1988 1988:215–24.10.7449/1988/Superalloys_1988_215_224 ↗
2. Reed · 2006
3. Nickel-Based Superalloys for Advanced Turbine Engines: Chemistry, Microstructure, and Properties10.2514/1.18239 ↗
4. Microstructural characteristics and mechanical properties of HVOF sprayed NiCrAl coating on superalloys10.1016/j.jallcom.2008.01.025 ↗
5. Evaluation of hot corrosion behaviour of HVOF sprayed NiCrAl coating on superalloys at 900 °C10.1016/j.matchemphys.2008.05.006 ↗
6. Effect of hot corrosion on the mechanical performances of superalloys and coating systems10.1016/0010-938X(93)90331-A ↗
7. Oxidation and hot corrosion resistance of HVOF WC-NiCrFeSiB coating on Ni- and Fe-based superalloys at 800 °C10.1007/s11666-007-9106-8 ↗
8. A Review of the Behavior of Aluminide-Coated Superalloys10.1007/BF00609929 ↗
9. Walston WS, Schaeffer JC, Murphy WH. A new type of microstructural instability in superalloys - SRZ. In: Cetel AD, Nathal M V., Pollock TM, Woodford DA, editors. Proceedings of International Symposium on Superalloys 1996, Seven Springs, PA, USA: TMS (The Minerals, Metals & Materials Society); 1996, p. 9–18.10.7449/1996/Superalloys_1996_9_18 ↗
10. Slurry aluminizing mechanisms of Ni-based superalloys incorporating an electrosynthesized ceria diffusion barrier10.1016/j.matchemphys.2013.09.022 ↗
11. Potential thermal barrier coating systems from Al microparticles. Mechanisms of coating formation on pure nickel10.1016/j.matchemphys.2012.03.053 ↗
12. Influence of annealing conditions on the formation of hollow Al2O3 microspheres studied by in situ ESEM10.1016/j.matchar.2016.01.018 ↗
13. Comparative isothermal oxidation behavior of new aluminide coatings from slurries containing Al particles and conventional out-of-pack aluminide coatings10.1007/s11085-013-9427-6 ↗
14. Microstructural analysis of the role of rhenium in advanced MCrAlY coatings10.1016/0257-8972(95)02546-4 ↗
15. Mechanisms of formation of diffusion aluminide coatings on nickel-base superalloys10.1007/BF00604047 ↗
16. Damage mechanisms during very high cycle fatigue of a coated and grit-blasted Ni-based single-crystal superalloy10.1016/j.ijfatigue.2020.105962 ↗
17. Diffusion barrier behaviors of (Ru, Ni)Al/NiAl coatings on Ni-based superalloy substrate10.1016/j.intermet.2010.08.016 ↗
18. The precipitation of topologically close-packed phases in rhenium-containing superalloys10.1016/S1359-6454(01)00265-8 ↗
19. The effect of TCP morphology on the development of aluminide coated superalloys10.1016/j.msea.2005.01.005 ↗
20. Intermediate temperature, low-cycle fatigue behavior of coated and uncoated nickel base superalloys in air and corrosive sulfate environments10.1115/1.3225675 ↗
21. A comparison of the effect of inward and outward diffusion aluminide coatings on the fatigue behavior of nickel-base superalloys10.1007/BF00612167 ↗
22. Damage evolution during thermo-mechanical fatigue of a coated monocrystalline nickel-base superalloy10.1016/j.ijfatigue.2007.01.045 ↗
23. Dynamic recrystallization in the particle/particle interfacial region of cold-sprayed nickel coating: Electron backscatter diffraction characterization10.1016/j.scriptamat.2009.07.020 ↗
24. Influence of surface recrystallization on the low cycle fatigue behaviour of a single crystal superalloy10.1111/ffe.12236 ↗
25. Pt-Al bond coat dependence on the high-cycle fatigue rupture and deformation mechanisms of a fourth-generation single crystal superalloy at various temperatures10.1016/j.matdes.2023.111880 ↗
26. Effect of Pt-Al bond coat on the high-cycle fatigue behaviour of a second-generation single crystal nickel-based superalloy at different temperatures10.1016/j.jmrt.2021.06.091 ↗
27. Reed · 2006
28. Nickel-Based Superalloys for Advanced Turbine Engines: Chemistry, Microstructure and Properties10.2514/1.18239 ↗
29. VHCF life evolution after microstructure degradation of a Ni-based single crystal superalloy10.1016/j.ijfatigue.2017.07.021 ↗
30. Crack initiation mechanisms during very high cycle fatigue of Ni-based single crystal superalloys at high temperature10.1016/j.actamat.2020.02.012 ↗
31. Very high cycle fatigue of Ni-based single crystal superalloys at high temperature10.1007/s11661-018-4672-6 ↗
32. Bortoluci Ormastroni LM, Utada S, Rame J, Mataveli Suave L, Kawagishi K, Harada H, et al. Tensile, Low Cycle Fatigue, and Very High Cycle Fatigue characterizations of advanced single crystal Nickel-based superalloys. In: Tin S, Hardy M, Clews J, Cormier J, Feng Q, Marcin J, et al., editors. Proceedings of the International Symposium on Superalloys 2020, Seven Springs, PA, USA: Springer US; 2020, p. 341–51.10.1007/978-3-030-51834-9_33 ↗
33. LCF, HCF and VHCF life sensitivity to solution heat treatment of a third-generation Ni-based single crystal superalloy10.1016/j.ijfatigue.2019.105247 ↗
34. Cervellon A, Yi JZ, Corpace F, Hervier Z, Rigney J, Wright PK, et al. Creep, fatigue, and oxidation interactions during High and very high cycle fatigue at elevated temperature of nickel-base single crystal superalloys. In: Tin S, Hardy M, Clews J, Cormier J, Feng Q, Marcin J, et al., editors. Proceedings of the International Symposium on Superalloys 2020, Seven Springs, PA, USA: Springer US; 2020, p. 185–95.10.1007/978-3-030-51834-9_18 ↗
35. VHCF life of AM1 Ni-based single crystal superalloy after pre-deformation10.1016/j.ijfatigue.2021.106224 ↗
36. Transition from internal to surface crack initiation of a single-crystal superalloy in the very-high-cycle fatigue regime at 1100 °C10.1016/j.ijfatigue.2021.106343 ↗
37. Very high cycle fatigue durability of an additively manufactured single-crystal Ni-based superalloy
38. Saboundji A, Jaquet V, Mataveli L, Rame J. Development of a new coating compatible with third-generation Nickel-based superalloys and thermal barrier coatings. In: Tin S, Hardy M, Clews J, Cormier J, Feng Q, Marcin J, et al., editors. Proceedings of International Symposium on Superalloys 2020, Seven Springs, PA, USA: Springer US; 2020, p. 804–12.10.1007/978-3-030-51834-9_79 ↗
39. Cervellon A. Propriétés en fatigue à grand et très grand nombre de cycles et à haute température des superalliages base nickel monogranulaires. PhD Thesis - Ecole Nationale Superieure de Mecanique et d’Aerotechnique (ISAE-ENSMA), Poitiers, France. https://theses.fr/2018ESMA0009, 2018.
40. High-temperature ultrasonic fatigue testing of single-crystal superalloys10.1016/j.matlet.2011.11.066 ↗
41. Fatigue strength of a single crystal in the gigacycle regime10.1016/j.ijfatigue.2007.04.003 ↗
42. Ultrasonic fatigue of a single crystal Ni-base superalloy at 1000 °C10.1016/j.msea.2006.08.028 ↗
43. Crystallographic fatigue crack initiation in nickel-based superalloy René 88DT at elevated temperature10.1016/j.actamat.2009.08.022 ↗
44. High temperature VHCF of a 3rd generation Ni-based single crystal superalloy with different casting pore sizes
45. Damage mechanisms in an EB-PVD thermal barrier coating system during TMF and TGMF testing conditions under combustion environment10.1016/j.ijfatigue.2016.08.001 ↗
46. High Temperature Micromechanical Behavior of a Pt-Modified Nickel Aluminide Bond-Coating and of Its Interdiffusion Zone with the Superalloy Substrate10.1007/s11661-020-05634-2 ↗
47. Efficiency of a-alumina as diffusion barrier between bond coat and bulkmaterial of gas turbine blades10.1016/S0042-207X(02)00746-7 ↗
48. The role of oxidation damage in fatigue crack initiation of an advanced Ni-based superalloy10.1016/j.ijfatigue.2015.08.016 ↗
49. Mataveli Suave L. High temperature durability of DS200+Hf alloy. PhD Thesis - Ecole Nationale Superieure de Mecanique et d’Aerotechnique (ISAE-ENSMA), Poitiers, France. https://theses.fr/2017ESMA0032, 2017.
50. Perruchaut P. Étude des interactions fatigue-fluage-oxydation sur l’endommagement du superalliage monocristallin AM1. PhD Thesis - Ecole Nationale Superieure de Mecanique et d’Aerotechnique (ISAE-ENSMA), Poitiers, France, 1997.
51. Model for the porosity growth in single-crystal nickel-base superalloys during homogenization10.1016/j.scriptamat.2007.07.012 ↗
52. Damage accumulation during creep deformation of a single crystal superalloy at 1150 °C10.1016/j.msea.2006.11.101 ↗
53. Fedelich B. Nickel Base Single Crystals Across Length Scales. vol. 1. 2022.
54. On the Impact of an Integrated HIP Treatment on the Very High Cycle Fatigue Life of Ni-Based SX Superalloys10.1007/s11661-022-06882-0 ↗
55. Initiation and early-stage growth of internal fatigue cracking under very-high cycle fatigue regime at high temperature10.1007/s11661-020-05633-3 ↗