journal article·2022-11

Fatigue performance of zirconia-reinforced Ti-6Al-4V nanocomposite processed by laser powder bed fusion: An improvement by hot isostatic pressing

Benjamin Guennec, Amine Hattal, Azziz Hocini, Kamilla Mukhtarova, Takahiro Kinoshita, Noriyo Horikawa, Jenő Gubicza, Madjid Djemaï, Guy Dirras

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Titanium Alloys Microstructure and Properties · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (54)

Show source-provided references
1. Laser Additive Manufacturing and Bionics: Redefining Lightweight Design10.1016/j.phpro.2011.03.046 ↗
2. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
3. Review on machining of additively manufactured nickel and titanium alloys10.1016/j.jmrt.2021.09.088 ↗
4. Additive manufacturing of titanium-based alloys- A review of methods, properties, challenges, and prospects10.1016/j.heliyon.2022.e09041 ↗
5. Energy and material efficiency strategies enabled by metal additive manufacturing – A review for the aeronautics and aerospace sectors10.1016/j.egyr.2022.01.035 ↗
6. Steady-state creep of in situ TiB plus La2O3 reinforced high temperature titanium matrix composite10.1016/j.msea.2008.09.002 ↗
7. Effect of aspect ratios of in situ formed TiB whiskers on the mechanical properties of TiBw/Ti–6Al–4V composites10.1016/j.scriptamat.2011.12.024 ↗
8. Effect of B4C particle size on microstructure of in situ titanium matrix composites prepared by reactive processing of Ti–B4C system10.1016/j.scriptamat.2006.05.024 ↗
9. Balance of strength and plasticity of additive manufactured Ti-6Al-4V alloy by forming TiB whiskers with gradient distribution
10. Production and mechanical properties of nano SiC particle reinforced Ti–6Al–4V matrix composite10.1016/S1003-6326(17)60009-8 ↗
11. Effect of nano-yttria stabilized zirconia addition on the microstructure and mechanical properties of Ti6Al4V parts manufactured by selective laser melting10.1016/j.matdes.2019.107909 ↗
12. Titanium Ti6Al4V alloy reinforced by the addition of nano yttria stabilized zirconia fabricated by selective additive manufacturing: microstructure and mechanical investigations10.1051/matecconf/202032103018 ↗
13. Effect of hot isostatic pressing on microstructure and mechanical properties of Ti6Al4V-zirconia nanocomposites processed by laser-powder bed fusion10.1016/j.matdes.2022.110392 ↗
14. Microstructures and mechanical properties of Ti6Al4V parts fabricated by selective laser melting and electron beam melting10.1007/s11665-013-0658-0 ↗
15. Mechanical behavior of additive manufactured, power-bed laser-fused materials10.1016/j.msea.2015.10.068 ↗
16. Application of mechanical surface finishing processes for roughness reduction and fatigue improvement of additively manufactured Ti-6Al-4V parts10.1016/j.ijfatigue.2017.05.008 ↗
17. A comparative study on mechanical properties of Ti-6Al-4V alloy by additive manufacturing vs. traditional processing10.1016/j.msea.2021.141384 ↗
18. Additive manufacturing of titanium alloys
19. Fatigue performance evaluation of selective laser meltedTi-6Al-4V10.1016/j.msea.2014.01.041 ↗
20. Influence of defects on mechanical properties of Ti-6Al-4V components produced by selective laser melting and electron beam melting
21. Critical assessment of the fatigue performance of additively manufactured Ti-6Al-4V and perspective for future research10.1016/j.ijfatigue.2015.12.003 ↗
22. A review of the fatigue properties of additively manufactured Ti-6Al-4V10.1007/s11837-017-2728-5 ↗
23. Influence of processing parameters of selective laser melting on high-cycle and very-high-cycle fatigue behaviour of Ti-6Al-4V10.1111/ffe.13361 ↗
24. Ultrasonic fatigue testing in as-built and polished Ti6Al4V alloy manufactured by SLM10.1016/j.finmec.2021.100024 ↗
25. Fatigue limit prediction model and fatigue crack growth mechanism for selective laser melting Ti6Al4V samples with inherent defects10.1016/j.ijfatigue.2020.106008 ↗
26. Fatigue performance of laser additive manufactured Ti-6Al-4V in very high cycle fatigue regime up to 109 cycles10.3389/fmats.2015.00072 ↗
27. Fatigue performance of additive manufactured TiAl6V4 using electron and laser beam melting10.1016/j.ijfatigue.2016.05.001 ↗
28. Fatigue life of additively manufactured Ti-6Al-4V in the very high cycle fatigue regime10.1016/j.ijfatigue.2016.05.018 ↗
29. Characteristic and mechanism of crack initiation and early growth of an additively manufactured Ti-6Al-4V in very high cycle fatigue regime10.1016/j.ijmecsci.2021.106591 ↗
30. Improved fatigue strength of additively manufactured Ti6Al4V by surface post processing10.1016/j.ijfatigue.2020.105497 ↗
31. Effects of stress ratio on high-cycle and very-high-cycle fatigue behavior of a Ti-6Al-4V alloy10.1016/j.msea.2014.09.115 ↗
32. Internal fatigue origins in α-β titanium alloys10.1016/0001-6160(76)90147-4 ↗
33. Data related to spectrum analyzes for phases identification, microstructure and mechanical properties of additive manufactured Ti6Al4V reinforce with nano yttria stabilized zirconia10.1016/j.dib.2020.105249 ↗
34. Effect of bimodal grain size distribution on fatigue properties of Ti-6Al-4V alloy with harmonic structure under four-point bending10.1016/j.msea.2017.01.076 ↗
35. Investigation on the durability of Ti-6Al-4V alloy designed in a harmonic structure via powder metallurgy: fatigue behavior and specimen size parameter issue10.3390/met10050636 ↗
36. Industrial AIP and UBMS coating deposition: static and fatigue performances of TiAlN coated SKH51 tool steel10.1007/s11665-022-06917-y ↗
37. Effects of defects, inclusions and inhomogeneities on fatigue strength10.1016/0142-1123(94)90001-9 ↗
38. A comparative study of the porosity of doped graphites by small angle neutron scattering, nitrogen adsorption and helium pycnometry10.1016/j.micromeso.2010.05.019 ↗
39. Gubicza J. X-ray line profile analysis in Materials Science, IGI-Global, Hershey, PA, USA.
40. Correlation between strength and microstructure of ball-milled Al-Mg alloys determined by X-ray diffraction10.1016/j.msea.2004.01.089 ↗
41. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
42. JSMS Committee of Reliability Engineering. Standard Evaluation Method of Fatigue Reliability for Metallic Materials – Standard Regression Method of S-N Curves
43. Stress gradient as a size effect in fatigue life determination for alternating bending10.1016/j.ijfatigue.2021.106461 ↗
44. Fatigue behavior of PBF additive manufactured TI6AL4V alloy shot and laser peening
45. Fatigue behavior of notched additive manufactured Ti6Al4V with as-built surface10.1016/j.ijfatigue.2017.04.009 ↗
46. Additive manufactured AlSi10Mg samples using Selective Laser Melting (SLM): Microstructure, high cycle fatigue and fracture behavior10.1016/j.matdes.2011.07.067 ↗
47. Fatigue strength estimation methodology of additively manufactured metallic bulk material
48. A new approach to correlate the defect population with the fatigue life of selective laser melted Ti-6Al-4V10.1016/j.ijfatigue.2020.105584 ↗
49. Dislocation interactions and crack nucleation in a fatigued near-alpha titanium alloy10.1016/j.ijplas.2018.06.009 ↗
50. Influence of microstructure on high-cycle fatigue of Ti-6Al-4V: Bimodal vs. Lamellar structure10.1007/s11661-002-0160-z ↗
51. Investigation of fatigue crack initiation in Ti-6Al-4V during tensile-tensile fatigue10.1361/105994902770344312 ↗
52. Influence of microstructure [alpha + beta and beta] on very high cycle fatigue behavior of Ti-6Al-4V10.1016/j.ijfatigue.2016.10.002 ↗
53. Fatigue crack initiation on slip bands: theory and experiment10.1016/0001-6160(86)90177-X ↗
54. Experimental evaluation of critical resolved shear stress for the first-order pyramidal c+a slip in commercially pure Ti by micropillar compression method10.1016/j.actamat.2020.06.043 ↗