journal article·2020-11Open access

Influence of graphite morphology on the corrosion-fatigue properties of the ferritic Si-Mo-Al cast iron SiMo1000

Shengmei Xiang, Peter Hedström, Baohua Zhu, Jan Linder, Joakim Odqvist

Abstract

The influence of graphite morphology on the corrosion-fatigue mechanism in the cast compacted graphite iron SiMo1000 is investigated. Two batches of SiMo1000 with the same chemical composition but different nodularity are tested using low-cycle-fatigue tests in argon and a synthetic exhaust atmosphere at 800 °C. Decreased graphite nodularity is found to significantly reduce the corrosion resistance of SiMo1000, causing severe decarburization on the sample surface. Besides, the fatigue life is also dramatically reduced with decreased graphite nodularity. The synergy of decarburization and fatigue is found to reduce fatigue life in one of the batches.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Aluminum Alloys Composites Properties · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Ekström · 2015
2. High temperature materials for heavy duty diesel engines: historical and future trends10.1016/j.pmatsci.2018.10.004 ↗
3. High-temperature mechanical-and fatigue properties of cast alloys intended for use in exhaust manifolds10.1016/j.msea.2014.08.014 ↗
4. Simo1000 ein aluminiumlegiertes gusseisen für hochtemperaturanwendungen
5. Norman · 2018
6. High-temperature corrosion-fatigue behavior of ductile cast irons for exhaust manifolds applications10.4028/www.scientific.net/MSF.925.369 ↗
7. Effect of graphite morphology on the fatigue and fracture resistance of ferritic ductile cast iron10.1016/j.engfracmech.2018.12.019 ↗
8. Corrosion fatigue of austenitic cast iron ni-resist d5s and austenitic cast steel hk30 in argon and synthetic diesel exhaust at 800°c10.1016/j.ijfatigue.2019.105396 ↗
9. Holtzer · 2015
10. Microstructure and dimensional stability in si-mo ductile irons for elevated temperature applications
11. Kleiner S. Internal gf report nr. 11222; 2008.
12. Mechanical properties of α+ κtwo-phase lamellar structure in fe-mn-al-c alloy10.2320/matertrans.44.1679 ↗
13. Phase equilibria in fe-mn-al-c alloys10.2355/isijinternational.30.680 ↗
14. ISO, Iso 16112: Compacted (vermicular) graphite cast irons — classification; 2017.
15. Domeij · 2019
16. Xiang · 2018
17. ISO. Iso 21608: Corrosion of metals and alloys — test method for isothermal-exposure oxidation testing under high-temperature corrosion conditions for metallic materials; 2012.
18. Hähner P, Affeldt E, et al. Validated code-of-practice for strain-controlled thermo-mechanical fatigue testing. Institute for Energy, Petten; 2006.
19. Campbell · 2008
20. Stefanescu · 2017
21. Microstructure and hot oxidation resistance of simo ductile cast irons containing si-mo-al10.1007/s11663-016-0871-y ↗
22. Mampaey F. In: AFS Transactions; 2005. p. 1–21.10.17159/1947-9417/2017/1492 ↗
23. Boeri R, Weinberg F. In: AFS Transactions. Vol. 97; 1989. p. 179–84.
24. Datta NK, Engel NN. In: AFS Transactions. Vol. 84; 1976. p. 431–6.
25. Liu PC, Loper CR. In: AFS Transactions. Vol. 84; 1976. p. 131–40.
26. Effect of graphite morphology on decarburized cast iron10.1080/13640461.2003.11819572 ↗
27. On the micro-and macroscopic elastoplastic deformation behaviour of cast iron when subjected to cyclic loading10.1016/j.ijplas.2018.11.019 ↗