Role of twinning and texture on fatigue resistance enhancement of Mg-6Gd-3Y-1Nd-0.5Zr alloys
Source abstract
Abstract
Abstract The fatigue crack propagation behavior of rolled magnesium alloys was studied and compared with as-cast alloys to unravel a relation between the early crack propagation and the fatigue resistance at the microstructural level. Grain structures results indicated that the geometric compatibility of grains and stress component on basal slip planes determine the propagation path of cracks. Twins are usually unfavorable for crack propagation, and the texture changes the stress component distribution in grains under the condition of unchanged loading. Both twins and textures increase the difficulty of crack propagation and improve the fatigue resistance at higher stress level.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. Towards the development of heat-treatable high-strength wrought Mg alloys10.1016/j.scriptamat.2010.01.038 ↗
2. A Review on Casting Magnesium Alloys: Modification of Commercial Alloys and Development of New Alloys10.1016/j.jmst.2016.07.001 ↗
3. What is going on in magnesium alloys?10.1016/j.jmst.2017.07.019 ↗
4. Structural aspects of high performance Mg alloys design10.1016/S0921-5093(01)01291-6 ↗
5. Mechanical Properties of Magnesium-Rare Earth Alloy Systems: A Review
6. Microstructure-sensitive investigation of magnesium alloy fatigue10.1016/j.ijplas.2014.10.010 ↗
7. Microstructural mechanisms of cyclic deformation, fatigue crack initiation and early crack growth
8. Effect of microstructure inhomogeneity and crack initiation environment on the very high cycle fatigue behavior of a magnesium alloy10.1016/j.ijfatigue.2019.105376 ↗
9. The fatigue behavior of I-phase containing as-cast Mg–Zn–Y–Zr alloy10.1016/j.actamat.2007.10.057 ↗
10. Crack initiation mechanism of extruded AZ31 magnesium alloy in the very high cycle fatigue regime10.1016/j.msea.2008.02.003 ↗
11. Study fatigue crack initiation in TiB2/Al-Cu-Mg composite by in-situ SEM and X-ray microtomography10.1016/j.ijfatigue.2020.105976 ↗
12. Damage morphology study of high cycle fatigued as-cast Mg–3.0Nd–0.2Zn–Zr (wt.%) alloy10.1016/j.matchar.2015.11.013 ↗
13. Influence of microstructure on fatigue crack propagation behaviors of an aluminum alloy: Role of sheet thickness10.1016/j.engfracmech.2017.05.038 ↗
14. Room-temperature low-cycle fatigue and fracture behaviour of asymmetrically rolled high-strength 7050 aluminium alloy plates10.1016/j.ijfatigue.2020.105919 ↗
15. Effects of thermal cycling and microstructure on the fatigue crack propagation in forged titanium–aluminide alloys under thermomechanical fatigue conditions10.1016/j.msea.2020.140248 ↗
16. Study of the interaction of a short fatigue crack with grain boundaries in a cast Al alloy using X-ray microtomography10.1016/S1359-6454(02)00320-8 ↗
17. Effect of microstructure on small fatigue crack initiation and early propagation behavior in Mg-10Gd-3Y-0.3Zr alloy10.1016/j.ijfatigue.2018.10.002 ↗
18. Small crack initiation and early propagation in an as-extruded Mg-10Gd-3Y-0.5Zr alloy in high cycle fatigue regime10.1016/j.msea.2018.10.015 ↗
19. Basal slip dominant fatigue damage behavior in a cast Mg-8Gd-3Y-Zr alloy10.1016/j.ijfatigue.2018.08.001 ↗
20. A study of fatigue damage development in extruded Mg–Gd–Y magnesium alloy10.1016/j.msea.2013.09.089 ↗
21. Cyclic deformation and fatigue of rolled AZ80 magnesium alloy along different material orientations10.1016/j.msea.2016.09.031 ↗
22. Fatigue damage development in extruded Mg-3Al-Zn magnesium alloy10.1016/j.msea.2016.05.009 ↗
23. Aging effects on cyclic deformation and fatigue of extruded Mg–Gd–Y–Zr alloy10.1016/j.msea.2015.06.001 ↗
24. Unveiling the formation of basal texture variations based on twinning and dynamic recrystallization in AZ31 magnesium alloy during extrusion10.1016/j.actamat.2018.07.014 ↗
25. Individual effect of recrystallisation nucleation sites on texture weakening in a magnesium alloy: Part 1- double twins10.1016/j.actamat.2017.06.015 ↗
26. Individual effect of recrystallisation nucleation sites on texture weakening in a magnesium alloy: Part 2- shear bands10.1016/j.actamat.2017.12.019 ↗
27. Statistic derivation of Taylor factors for polycrystalline metals with application to pure magnesium10.1016/j.msea.2013.06.025 ↗
28. First principles calculations of formation energies and elastic constants of inclusions α-Al2O3, MgO and AlN in aluminum alloy10.1142/S0217979216500855 ↗
29. Basal and non-basal dislocation slip in Mg–Y10.1016/j.msea.2013.03.006 ↗
30. Crystal orientation effect on fretting fatigue induced geometrically necessary dislocation distribution in Ni-based single-crystal superalloys10.1016/j.actamat.2019.08.035 ↗
31. EBSD analysis of fatigue crack initiation behavior in coarse-grained AZ31 magnesium alloy10.1016/j.ijfatigue.2015.11.010 ↗
32. Relationship between Fatigue Strength and Grain Size in AZ31 Magnesium Alloys10.2320/matertrans.MC2007101 ↗
33. Effect of grain size on fatigue-crack growth in 2524 aluminium alloy10.1016/j.ijfatigue.2015.11.011 ↗
34. Transmission electron microscopy investigations of AZ91 alloy deformed by equal-channel angular pressing10.1111/j.1365-2818.2006.01640.x ↗
35. Compatibility of deformation in two-phase Ti-Al alloys: Dependence on microstructure and orientation relationships10.1007/BF02670762 ↗
36. Dependence of intergranular fatigue cracking on the interactions of persistent slip bands with grain boundaries10.1016/S1359-6454(02)00399-3 ↗
37. The phenomena of rupture and flows in solids
38. High Cycle Fatigue Behaviour of Magnesium Alloys10.1016/j.proeng.2010.03.080 ↗
39. Effect of initial twins on the stress-controlled fatigue behavior of rolled magnesium alloy10.1016/j.msea.2016.10.093 ↗
40. Role of initial 10–12 twin in the fatigue behavior of rolled Mg–3Al–1Zn alloy10.1016/j.scriptamat.2010.01.021 ↗
41. Effects of initial 10–12 twins on cyclic deformation and fatigue of magnesium alloy at low strain amplitudes10.1016/j.matchar.2019.01.017 ↗
42. Gao, Lifang, Bai, Song, Luqing, Liu, Zhiyi, Xia, Peng. Enhanced fatigue crack propagation resistance in a super high strength Al-Zn-Mg-Cu alloy by modifying RRA treatment. MATER CHARACT 2016; 118: 438-445.10.1016/j.matchar.2016.06.023 ↗
43. Orientation dependence of the cyclic deformation behavior and the role of grain boundaries in fatigue damage in copper crystals10.1016/S0921-5093(01)01055-3 ↗