This work aims to analyze the sensitivity of the very high-cycle fatigue behavior of LPBF-Ti-6Al-4V to microstructure and porosity variations. To do so ultrasonic fatigue testing is performed on five grades of LPBF-Ti-6Al-4V. These grades were generated using different LPBF process parameters and different thermal post-treatments allowing to separately investigate the sensitivity to microstructure and porosity variations. It was found that both material features highly influenced the VHCF properties of LPBF-Ti-6Al-4V revealing the sensitivity to these features. Furthermore, the largest defect (pore or grain) controls fatigue crack initiation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
2. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti6Al4V10.1016/j.actamat.2018.05.044 ↗
3. Interpretation of the fatigue anisotropy of additively manufactured TA6V alloys via a fracture mechanics approach10.1016/j.engfracmech.2019.03.048 ↗
4. Applicability of fracture mechanics to very small cracks or the cracks in the early stage
5. Murakami · 2019
6. In-process sensing in selective laser melting (SLM) additive manufacturing10.1186/s40192-016-0045-4 ↗
7. Optimisation of process parameters to address fundamental challenges during selective laser melting of Ti6Al4V: A review10.1016/j.ijmachtools.2018.01.003 ↗
8. Fatigue crack growth behavior of laser powder bed fusion additive manufactured Ti6Al4V: Roles of post heat treatment and build orientation10.1016/j.ijfatigue.2020.105955 ↗
9. Heat treatment of Ti6Al4V produced by selective laser melting: Microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
10. The formation of alpha + beta microstructure in as-fabricated selective laser melting of Ti–6Al–4V10.1557/jmr.2014.166 ↗
11. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
12. Formation and control of martensite in Ti6Al4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
13. Optimization and comparison of porosity rate measurement methods of selective laser melted metallic parts
14. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: Fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
15. An experimental study of residual stress and direction-dependence of fatigue crack growth behaviour in as-built and stress-relieved selective-laser-melted Ti6Al4V10.1016/j.msea.2019.04.023 ↗
16. In-situ XRD study on the effects of stress relaxation and phase transformation heat treatments on mechanical and microstructural behaviour of additively manufactured Ti6Al4V10.1016/j.msea.2021.141534 ↗
17. Heat treatment of Ti6Al4V alloy manufactured by laser-based powder-bed fusion: Process, microstructures, and mechanical properties correlations10.1016/j.jallcom.2021.162618 ↗
18. As-fabricated and heat-treated microstructures of the Ti6Al4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
19. Influence of heat treatments on the microstructure and tensile behavior of selective laser melting-produced Ti6Al4V parts
20. Development of heat treatments for selective laser melting Ti6Al4V alloy: Effect on microstructure, mechanical properties, and corrosion resistance10.1002/adem.202000359 ↗
21. Hot isostatic pressing for fatigue critical additively manufactured Ti6Al4V10.3390/ma15062051 ↗
22. Effect of heat treatment on the tensile behavior of selective laser melted Ti6Al4V by in situ X-ray characterization10.1016/j.actamat.2020.03.003 ↗
23. Bathias · 2005
24. Critical assessment of the fatigue performance of additively manufactured Ti–6Al–4V and perspective for future research10.1016/j.ijfatigue.2015.12.003 ↗
25. On the fatigue properties of metals manufactured by selective laser melting – the role of ductility10.1557/jmr.2014.157 ↗
26. Ultrasonic fatigue testing in as-built and polished Ti6Al4V alloy manufactured by SLM10.1016/j.finmec.2021.100024 ↗
27. Fatigue life of additively manufactured Ti–6Al–4V in the very high cycle fatigue regime10.1016/j.ijfatigue.2016.05.018 ↗
28. Crack initiation mechanisms under two stress ratios up to very-high-cycle fatigue regime for a selective laser melted Ti6Al4V10.1016/j.ijfatigue.2021.106294 ↗
29. VHCF response of heat-treated SLM Ti6Al4V Gaussian specimens with large loaded volume10.1016/j.prostr.2019.08.171 ↗
30. Fatigue performance of laser additive manufactured Ti–6Al–4V in very high cycle fatigue regime up to 109 cycles10.3389/fmats.2015.00072 ↗
31. Very-high-cycle fatigue behavior of Ti6Al4V manufactured by selective laser melting: Effect of build orientation10.1016/j.ijfatigue.2020.105628 ↗
32. Staircase testing of a titanium alloy in the gigacycle regime
33. A new approach to correlate the defect population with the fatigue life of selective laser melted Ti6Al4V alloy10.1016/j.ijfatigue.2020.105584 ↗
34. Interior initiation and early growth of very high cycle fatigue crack in an additively manufactured Ti-alloy10.1016/j.ijfatigue.2022.106862 ↗
35. On ‘multi-stage’ fatigue life diagrams and the relevant life-controlling mechanisms in ultrahigh-cycle fatigue10.1046/j.1460-2695.2002.00550.x ↗
36. High-cycle fatigue behavior of a laser powder bed fusion additive manufactured Ti6Al4V titanium: Effect of pores and tested volume size10.1016/j.ijfatigue.2021.106206 ↗
37. Estimation of stress in specimens loaded with ultrasonic fatigue machines10.1016/j.ijfatigue.2021.106474 ↗
38. Influence of defects, surface roughness and HIP on the fatigue strength of Ti6Al4V manufactured by additive manufacturing10.1016/j.ijfatigue.2018.07.020 ↗
39. Mechanism of stress relaxation and phase transformation in additively manufactured Ti6Al4V via in situ high temperature XRD and TEM analyses10.1016/j.actamat.2020.02.056 ↗
40. Influence of tempering temperature and time on the alpha’-Ti6Al4V martensite10.1016/0925-8388(95)02057-8 ↗
41. Analysis of fatigue properties and failure mechanisms of Ti6Al4V in the very high cycle fatigue regime using ultrasonic technology and 3D laser scanning vibrometry
42. Prediction of non propagating cracks10.1016/0013-7944(79)90081-X ↗
43. Fatigue life estimation of additively manufactured Ti6Al4V: Sensitivity, scatter and defect description in damage-tolerant models10.1016/j.actamat.2022.118189 ↗
44. Effects of defects in laser additive manufactured Ti6Al4V on fatigue properties
45. Fatigue strength prediction for titanium alloy TiAl6V4 manufactured by selective laser melting10.1007/s11661-015-2864-x ↗
46. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti6Al4V alloy10.1016/j.actamat.2019.03.003 ↗
47. Influence of microstructure on high-cycle fatigue of Ti6Al4V: Bimodal vs. lamellar structures10.1007/s11661-002-0160-z ↗
48. Interaction between a surface defect and grain size under high cycle fatigue loading: Experimental approach for Armco iron10.1016/j.ijfatigue.2016.01.013 ↗
49. An engineering estimation of fatigue thresholds from a microstructural size and vickers hardness: Application to wrought and additively manufactured metals10.1016/j.ijfatigue.2020.105796 ↗