Abstract

Ceramic coatings were produced on AA7075-T6 alloy by micro-arc oxidation (MAO). The MAO treatment was performed at different duty cycles (8, 10, 15, and 20%). Effects of duty cycle on microstructure and fatigue behavior of the coated samples were investigated. Surface features and cross-section morphology, and fatigue fracture were observed by SEM and laser microscope. Phase structure and residual stress in the coatings were analyzed by X-ray diffraction. The nature and relaxation mechanism of the residual stress were revealed. Finally, the influence of the residual stress relaxation on the fatigue life at high and low cyclic stresses was explored.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (74)

Show source-provided references
1. Strategies to improve the corrosion resistance of microarc oxidation (MAO) coated magnesium alloys for degradable implants: Prospects and challenges10.1016/j.pmatsci.2013.08.002 ↗
2. A universal electrolyte for the plasma electrolytic oxidation of aluminum and magnesium alloys10.1016/j.matdes.2015.08.071 ↗
3. Review of antibacterial activity of titanium-based implants' surfaces fabricated by micro-arc oxidation10.3390/coatings7030045 ↗
4. Hudson CM. Effect of stress ratio on fatigue-crack growth in 7075-T6 and 2024-T3 aluminum-alloy specimens, New York; 1969.10.1016/0013-7944(69)90003-4 ↗
5. Effect of inclusion on subsurface crack initiation and gigacycle fatigue strength10.1016/S0142-1123(02)00037-3 ↗
6. Active protective PEO coatings on AA2024: Role of voltage on in-situ LDH growth10.1016/j.matdes.2017.01.097 ↗
7. The effect of oxide coatings on fatigue properties of 7475–T6 aluminium alloy10.1016/j.surfcoat.2006.02.002 ↗
8. Influence of microarc oxidation and hard anodizing on plain fatigue and fretting fatigue behaviour of Al-Mg-Si alloy10.1016/j.surfcoat.2007.06.058 ↗
9. Effect of combined shot-peening and PEO treatment on fatigue life of 2024 Al alloy10.1016/j.tsf.2006.07.123 ↗
10. High-cycle fatigue behavior of microarc oxidation coatings deposited on a 6061–T6 Al alloy10.1007/s11661-009-0057-1 ↗
11. Influence of prior shot peening variables on the fatigue life of micro arc oxidation coated 6061–T6 Al alloy10.1016/j.ijfatigue.2017.09.020 ↗
12. Influence of micro arc oxidation coating thickness and prior shot peening on the fatigue behavior of 6061–T6 Al alloy10.1016/j.ijfatigue.2019.05.013 ↗
13. Enhancing the high cycle fatigue life of high strength aluminum alloys for aerospace applications10.1111/ffe.12944 ↗
14. Influence of combined shot peening and PEO treatment on corrosion fatigue behavior of 7A85 aluminum alloy10.1016/j.apsusc.2019.04.242 ↗
15. The influence of the coating technique on the high cycle fatigue life of alumina coated Al 6061 alloy10.1007/s12666-010-0028-7 ↗
16. Effect of microarc oxidation coating on fatigue performance of Ti-Al-Zr alloy10.1016/j.apsusc.2009.06.038 ↗
17. Enhanced fatigue performance of modified plasma electrolytic oxidation coated Ti-6Al-4V alloy: Effect of residual stress and gradient nanostructure10.1016/j.apsusc.2019.06.006 ↗
18. In vitro fatigue behavior of surface oxidized Ti35Zr10Nb biomedical alloy10.1016/j.msec.2011.08.010 ↗
19. Improvement on the fatigue performance of 2024–T4 alloy by synergistic coating technology10.3390/ma7053533 ↗
20. Microarc oxidation coating combined with surface pore-sealing treatment enhances corrosion fatigue performance of 7075–T7351 Al alloy in different media10.3390/ma10060609 ↗
21. The effect of surface roughness of the substrate on fatigue life of coated aluminum alloy by micro-arc oxidation10.1016/j.jallcom.2018.06.290 ↗
22. Effects of pulse duty cycles on microarc oxidation formed on Al
23. Influence of frequency and duty cycle on microstructure of plasma electrolytic oxidized AA7075 and the correlation to its corrosion behavior10.1016/j.surfcoat.2015.08.043 ↗
24. Effect of duty cycle and applied current frequency on plasma electrolytic oxidation (PEO) coating growth behavior10.1016/j.surfcoat.2013.03.041 ↗
25. Influence of duty cycle on the growth behavior and wear resistance of micro arc oxidation coatings on hot dip aluminized cast iron10.1016/j.surfcoat.2017.12.064 ↗
26. High-frequency-induced cathodic breakdown during plasma electrolytic oxidation10.1103/PhysRevApplied.8.031001 ↗
27. Growth kinetics and morphology of microarc oxidation coating on titanium10.1016/j.surfcoat.2017.03.002 ↗
28. Mechanisms underlying the formation of thick alumina coatings through the MAO coating technology10.1016/S0257-8972(02)00918-0 ↗
29. Tailored aluminium oxide layers by bipolar current adjustment in the Plasma Electrolytic Oxidation (PEO) process10.1016/j.surfcoat.2006.09.005 ↗
30. Fatigue response of porous coated titanium biomedical alloys10.1016/j.scriptamat.2009.03.017 ↗
31. The role of cathodic current in plasma electrolytic oxidation of aluminum: phenomenological concepts of the “soft sparking” mode10.1021/acs.langmuir.7b02284 ↗
32. A mechanism for the growth of a plasma electrolytic oxide coating on Al10.1016/j.electacta.2016.04.186 ↗
33. Evolution process of the plasma electrolytic oxidation (PEO) coating formed on aluminum in an alkaline sodium hexametaphosphate ((NaPO3)6) electrolyte10.1016/j.jallcom.2019.05.253 ↗
34. Effects of honeycomb pretreatment on MAO coating fabricated on aluminum10.1016/j.surfcoat.2019.02.047 ↗
35. Microstructural characteristic, outward-inward growth behavior and formation mechanism of MAO ceramic coating on the surface of ADC12 Al alloy with micro-groove10.1016/j.ceramint.2018.01.189 ↗
36. An investigation of ceramic coating growth mechanisms in plasma electrolytic oxidation (PEO) processing10.1016/j.electacta.2013.08.137 ↗
37. A review of recent work on discharge characteristics during plasma electrolytic oxidation of various metals10.1080/09506608.2018.1466492 ↗
38. Effect of individual discharge cascades on the microstructure of plasma electrolytic oxidation coatings10.1016/j.apsusc.2016.07.106 ↗
39. Analysis of phase distribution for ceramic coatings formed by microarc oxidation on aluminum alloy10.1111/j.1151-2916.1998.tb02493.x ↗
40. Characterisation of ceramic coatings produced by plasma electrolytic oxidation of aluminum alloy10.1016/j.msea.2006.09.004 ↗
41. Effects of pulse current mode on plasma electrolytic oxidation of 7075 Al in Na2WO4 containing solution: From unipolar to soft-sparking regime10.1016/j.electacta.2018.07.200 ↗
42. Surface characterisation of DC plasma electrolytic oxidation treated 6082 aluminium alloy Effect of current density and electrolyte concentration10.1016/j.surfcoat.2010.04.052 ↗
43. Thermo-physical properties of plasma electrolytic oxide coatings on aluminium10.1016/j.surfcoat.2004.09.037 ↗
44. Investigation of the growth processes of coatings formed by AC plasma electrolytic oxidation of aluminium10.1016/j.electacta.2009.06.088 ↗
45. Evaluation of residual stress levels in plasma electrolytic oxidation coatings using a curvature method10.1016/j.surfcoat.2014.11.006 ↗
46. Effects of micro arc oxidation on fatigue limits and fracture morphologies of 7475 high strength aluminum alloy10.1016/j.jallcom.2015.07.262 ↗
47. Residual stress distribution in burnishing solution treated and aged 7075 aluminium alloy10.1016/0890-6955(89)90062-X ↗
48. Thin film materials: stress, defect formation and surface evolution
49. Properties of aluminium oxide coating on aluminium alloy produced by micro-arc oxidation10.1016/j.surfcoat.2004.11.044 ↗
50. Residual stress relaxation and low- and high-cycle fatigue behavior of shot-peened medium-carbon steel10.1016/j.ijfatigue.2013.07.001 ↗
51. Microstructure, temperature estimation and thermal shock resistance of PEO ceramic coatings on aluminum10.1016/j.jmatprotec.2007.11.209 ↗
52. Preparation and properties of composite ceramic coating containing Al2O3-ZrO2-Y2O3 on AZ91D magnesium alloy by plasma electrolytic oxidation10.1016/j.cap.2009.02.017 ↗
53. Influence of duty cycle on fatigue life of AA2024 with thin coating fabricated by micro-arc oxidation10.1016/j.surfcoat.2018.12.118 ↗
54. Schijve J. Fatigue of structures and materials, New York; 2004.
55. Fatigue mediated lattice rotation in Al alloys10.1016/j.actamat.2017.02.061 ↗
56. Fatigue life of micro-arc oxidation coated AA2024-T3 and AA7075-T6 alloys10.1016/j.ijfatigue.2019.03.028 ↗
57. Micromechanisms of multistage fatigue crack growth in a high-strength aluminum alloy10.1016/j.actamat.2006.11.009 ↗
58. Fracture and fatigue-crack growth along aluminum-alumina interfaces10.1016/S1359-6454(96)00126-7 ↗
59. High cycle fatigue behavior of the severely plastically deformed 6082 aluminum alloy with an anodic and plasma electrolytic oxide coating10.1016/j.surfcoat.2018.06.044 ↗
60. Fracture of porous materials - Influence of the pore size10.1016/j.engfracmech.2006.12.002 ↗
61. Reinforcement by crack-tip blunting in porous ceramics10.1016/S0955-2219(03)00365-0 ↗
62. Indirect estimation of critical frontal process-zone size using a single-edge V-notched-beam technique10.2109/jcersj.109.1271_591 ↗
63. Fatigue crack propagation in steels10.1016/0013-7944(83)90070-X ↗
64. The science and engineering of materials
65. Fracture normal to a bimaterial interface: Effects of plasticity on crack-tip shielding and amplification10.1016/0956-7151(94)00295-S ↗
66. Brittle coating effects on fatigue cracks behavior in Ti alloys10.1016/j.ijfatigue.2019.04.017 ↗
67. A dislocation model for fatigue crack initiation10.1115/1.3157599 ↗
68. Residual stress and its role in failure10.1088/0034-4885/70/12/R04 ↗
69. Effect of microarc discharge surface treatment on the tensile properties of Al-Cu-Mg alloy10.1016/S0167-577X(02)00605-5 ↗
70. Microstructure and properties of ceramic coatings produced on 2024 aluminum alloy by microarc oxidation10.1023/A:1017988024099 ↗
71. Twin boundary: Stronger or weaker interface to resist fatigue cracking?10.1016/j.scriptamat.2012.01.028 ↗
72. Brittle film-induced cracking of ductile substrates10.1016/j.actamat.2015.07.059 ↗
73. Cleavage cracking of ductile-metal substrates induced by brittle coating fracture10.1016/j.actamat.2018.04.017 ↗
74. Microstructure, bonding strength and thermal shock resistance of ceramic coatings on steels prepared by plasma electrolytic oxidation10.1016/j.apsusc.2009.08.036 ↗