Low cycle fatigue behaviour of a precipitation hardened Cu-Ni-Si alloy
Source abstract
Abstract
Low cycle fatigue tests were performed at room temperature to investigate the role of the microstructure of a Cu-Ni-Si alloy on the stress response to strain cycling and on the fatigue resistance. The cyclic accommodation consisted in a hardening followed by a softening. TEM analysis showed that in some grains dislocations remained isolated and confined between precipitates while in other grains dislocations piled up at δ-Ni 2 Si precipitates and then cut them. Repetitive cutting allows their dissolution and formation of precipitate-free bands where the plastic deformation is localised. The Manson-Coffin diagram exhibited two regimes according to the proportion of grains involved in the plastic deformation accommodation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Copper alloys
2. 2001
3. Anisotropy effects on the tensile and fatigue behaviour of an oxide dispersion strengthened copper alloy10.1016/j.msea.2011.12.021 ↗
4. 4.20 Physical and mechanical properties of copper and copper alloys10.1016/B978-0-08-056033-5.00122-1 ↗
5. Material properties of high-strength beryllium-free copper alloys10.1504/IJMPT.2015.067820 ↗
6. Properties of high performance alloys for electromechanical connectors
7. Precipitate structure in a Cu–Ni–Si alloy10.1007/BF00356596 ↗
8. Microstructure and mechanical properties of Cu–Ni–Si alloys10.1016/j.msea.2006.12.163 ↗
9. The crystallographic and morphological evolution of the strengthening precipitates in Cu–Ni–Si alloys10.1016/j.actamat.2012.10.031 ↗
10. Orientation and diffraction patterns of δ-Ni2Si precipitates in Cu–Ni–Si alloy10.1016/j.jallcom.2012.12.154 ↗
11. Microstructure and properties of Cu–2.8Ni–0.6Si alloy10.1007/s12598-013-0056-7 ↗
12. Effect of thermomechanical treatments on microstructure and properties of Cu-base leadframe alloy10.1023/A:1004830000742 ↗
13. Effect of thermomechanical treatment on spray formed Cu–Ni–Si alloy10.1179/026708304225017265 ↗
14. Improvement in strength and electrical conductivity of Cu–Ni–Si alloys by aging and cold rolling10.1016/j.jallcom.2005.09.037 ↗
15. An examination of microstructural evolution in a Cu–Ni–Si alloy processed by HPT and ECAP10.1016/j.msea.2013.04.004 ↗
16. Improvement in Mechanical Properties of a Cu–2.0 mass%Ni–0.5 mass%Si–0.1 mass%Zr alloy by combining both accumulative roll-bonding and cryo-rolling with aging10.2320/matertrans.M2012207 ↗
17. Strengthening of Cu–Ni–Si alloy using high-pressure torsion and aging10.1016/j.matchar.2014.01.006 ↗
18. Effects of heat treatment processes on the microstructures and properties of powder metallurgy produced Cu–Ni–Si–Cr alloy10.1016/j.msea.2014.09.098 ↗
19. Effect of heat treatment on precipitation behaviour in a Cu–Ni–Si–P alloy10.1007/BF00553275 ↗
20. Precipitation in Cu–Ni–Si–Zn alloy for lead frame10.1016/S0167-577X(02)01212-0 ↗
21. Microstructure and properties of high-conductivity, super-high-strength Cu–8.0Ni–1.8Si–0.6Sn–0.15Mg alloy10.1557/jmr.2009.0251 ↗
22. Aging behavior of Cu–Ni–Si alloy10.1016/S0921-5093(03)00496-9 ↗
23. Mechanical properties of Cu–4.0wt%Ni–0.95wt%Si alloys with and without P and Cr addition10.4028/www.scientific.net/MSF.561-565.2321 ↗
24. Microstructure and properties of a high-strength Cu–Ni–Si–Co–Zr alloy10.1007/s11665-013-0482-6 ↗
25. Effect of aluminum on microstructure and property of Cu–Ni–Si alloys10.1016/j.msea.2013.02.024 ↗
26. Tensile and electrical properties of direct aged Cu–Ni–Si–x%Ti alloys10.1007/s12540-013-2007-0 ↗
27. Effect of V addition on hardness and electrical conductivity in Cu–Ni–Si alloys10.1007/s12540-013-4002-x ↗
28. Effects of small addition of ti on strength and microstructure of a Cu–Ni–Si alloy10.1007/s11661-015-2870-z ↗
29. Fatigue of precipitate strengthened Cu–Ni–Si alloy10.1179/026708399101505194 ↗
30. Dynamic embrittlement during fatigue of a Cu–Ni–Si alloy10.1016/j.msea.2011.04.069 ↗
31. Cyclic softening of Cu–Ni–Si alloy single crystals under low-cycle fatigue10.4028/www.scientific.net/MSF.654-656.1287 ↗
32. Role of microstructure on initiation and propagation of fatigue cracks in precipitate strengthened Cu–Ni–Si alloy10.1016/j.ijfatigue.2016.01.004 ↗
33. NanoMEGAS. website. http://www.nanomegas.com/.
34. Automated crystal orientation and phase mapping in TEM10.1016/j.matchar.2014.08.010 ↗
35. Calculation of Cu-rich part of Cu–Ni–Si phase diagram
36. Effect of Al2O3 dispersed nanoparticles on the fatigue behaviour of copper
37. Cyclic stress–strain response of two-phase alloys Part I. Microstructures containing particles penetrable by dislocations10.1016/0025-5416(74)90182-7 ↗
38. Dislocation-precipitate interaction and cyclic stress–strain behavior of a γ′ strengthened superalloy10.1016/0025-5416(78)90060-5 ↗
39. Atomic force microscopy of the intense slip localization causing fatigue crack initiation in polycrystalline brass10.1016/j.msea.2003.12.095 ↗
40. Development of fatigue testing system for in-situ observation by an atomic force microscope and small fatigue crack growth behavior in α-brass10.1299/jsmea.49.382 ↗
41. Dislocation microstructures in fatigued copper polycrystals10.1016/0001-6160(81)90117-6 ↗
42. Low-cycle fatigue of dispersion-strengthened copper10.1007/BF02652324 ↗
43. Coarsening of δ-Ni2Si precipitates in a Cu–Ni–Si alloy10.1007/s10853-011-5261-x ↗
44. Martin · 1998
45. Particle dissolution during fatigue softening of age hardened Cu–Co single crystals10.1016/0036-9748(83)90483-0 ↗
46. The fatigue behaviour of age-hardened Cu–2at.%Co alloy10.1016/0025-5416(86)90224-7 ↗
47. Persistent slip bands in fatigued peak aged Al–Zn–Mg single crystals—I. Development of dislocation microstructure and change of precipitation distribution10.1016/0001-6160(82)90040-2 ↗
48. Persistent slip bands in fatigued peak aged Al–Zn–Mg single crystals—II. Persistent slip bands in front of stage I fatigue cracks10.1016/0001-6160(82)90041-4 ↗
49. TEM investigation of γ′ free bands in nimonic PE16 under LCF loading at room temperature10.1016/0956-7151(90)90293-P ↗