Porosity related defects within metal additive manufactured components has made it challenging to certify their use in fatigue critical applications. In this study, the fatigue behaviour of selective electron beam melted (SEBM) Ti-6Al-4V specimens following hot isostatic pressing (HIP’ing) and finish machining has been investigated. Employing a sufficient material removal depth during machining was shown to significantly improve fatigue performance. This was attributed to be a direct result of removing material rich in lack-of-fusion defects, concentrated in the sub-surface. HIP’ing was shown to enhance fatigue performance to a lesser degree, as the treatment was only effective at reducing gas porosity.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (39)

Show source-provided references
1. A review of powdered additive manufacturing techniques for Ti-6Al-4V biomedical applications10.1016/j.powtec.2018.03.010 ↗
2. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
3. Near Net Shape Manufacture of Titanium Alloy Components from Powder and Wire: A Review of State-of-the-Art Process Routes10.3390/met9060689 ↗
4. Influence of Material-Related Aspects of Additive and Subtractive Ti-6Al-4V Manufacturing on Energy Demand and Carbon Dioxide Emissions
5. AM and aerospace: an ideal combination10.1016/j.mprp.2015.06.005 ↗
6. Additive Manufacturing of Titanium Alloy for Aircraft Components10.1016/j.procir.2015.08.061 ↗
7. A review on the fatigue behavior of Ti-6Al-4V fabricated by electron beam melting additive manufacturing10.1016/j.ijfatigue.2018.09.022 ↗
8. Additive Manufacturing of Titanium Alloys by Electron Beam Melting: A Review
9. Körner C. Additive manufacturing of metallic components by selective electron beam melting a review. Int Mater Rev 6608(May). doi: 10.1080/09506608.2016.1176289.10.1080/09506608.2016.1176289 ↗
10. Galati M, Minetola P, Rizza G. Surface roughness characterisation and analysis of the Electron Beam Melting (EBM) process. Materials 12(13). doi: 10.3390/ma12132211.10.3390/ma12132211 ↗
11. Beam speed effects on Ti-6Al-4V microstructures in electron beam additive manufacturing10.1557/jmr.2014.125 ↗
12. Caiazzo F, Cardaropoli F, Alfieri V, Sergi V, Cuccaro L. Experimental analysis of selective laser melting process for Ti-6Al-4V turbine blade manufacturing. In: XIX International Symposium on High-Power Laser Systems and Applications 86771 (January 2013); 2013. p. 86771H. doi: 10.1117/12.2010577.10.1117/12.2010577 ↗
13. Electron Beam Additive Manufacturing of Titanium Components: Properties and Performance10.1115/1.4025773 ↗
14. Effect of process parameters settings and thickness on surface roughness of EBM produced Ti-6Al-4V10.1108/13552541211250391 ↗
15. A Review on Abrasive Flow Machining (AFM)10.1016/j.protcy.2016.08.224 ↗
16. Recent developments in abrasive flow finishing process: A review of current research and future prospects10.1177/0954405417731466 ↗
17. Impact of chemical polishing on surface roughness and dimensional quality of electron beam melting process (EBM) parts10.1063/1.5034999 ↗
18. Effect of laser ablation parameters on surface improvement of electron beam melted parts10.1007/s00170-016-8533-4 ↗
19. Metal Additive Manufacturing: A Review of Mechanical Properties10.1146/annurev-matsci-070115-032024 ↗
20. Microstructure and mechanical properties of Ti-6Al-4V manufactured by electron beam melting process10.1179/1432891713Z.000000000302 ↗
21. Effects of the microstructure and porosity on properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)10.1016/j.addma.2016.02.003 ↗
22. Effects of post-processing on cyclic fatigue response of a titanium alloy additively manufactured by electron beam melting10.1016/j.msea.2016.10.059 ↗
23. The Influence of Porosity on Fatigue Crack Initiation in Additively Manufactured Titanium Components10.1038/s41598-017-06504-5 ↗
24. Evaluating the Effect of Processing Parameters on Porosity in Electron Beam Melted Ti-6Al-4V via Synchrotron X-ray Microtomography10.1007/s11837-015-1802-0 ↗
25. The Effectiveness of Hot Isostatic Pressing for Closing Porosity in Titanium Parts Manufactured by Selective Electron Beam Melting10.1007/s11661-016-3429-3 ↗
26. Surface Roughness and HIP on Fatigue Strength of Ti-6Al-4V manufactured by Additive Manufacturing10.1016/j.prostr.2017.11.055 ↗
27. Microstructure and mechanical properties of Ti-6Al-4V produced by electron beam melting of pre-alloyed powders10.1108/13552540910960262 ↗
28. XCT analysis of the influence of melt strategies on defect population in Ti-6Al-4V components manufactured by Selective Electron Beam Melting10.1016/j.matchar.2015.02.008 ↗
29. Fatigue properties of a titanium alloy (Ti-6Al-4V) fabricated via electron beam melting (EBM): Effects of internal defects and residual stress10.1016/j.ijfatigue.2016.04.022 ↗
30. ASTM International. ASTM Standard F2924: Standard specification for additive manufacturing titanium-6 aluminum-4 vanadium with powder bed fusion. In: ASTM book of standards, West Conshohocken, PA; 2014.
31. Analyzing the effects of powder and post- processing on porosity and properties of electron beam melted Ti-6Al-4V10.1080/21663831.2017.1340911 ↗
32. Defect distribution and microstructure heterogeneity effects on fracture resistance and fatigue behavior of EBM Ti-6Al-4V10.1016/j.ijfatigue.2016.06.001 ↗
33. The effect of machining and induced surface deformation on the fatigue performance of a high strength metastable βtitanium alloy10.1016/j.ijfatigue.2019.02.033 ↗
34. The effect of forging texture and machining parameters on the fatigue performance of titanium alloy disc components10.1016/j.ijfatigue.2020.105949 ↗
35. Childerhouse T. Defect characterisation on SEBM fracture surfaces; 2021. https://github.com/TChilderhouse/Defect-characterisation-on-SEBM-fracture-surfaces.
36. Material defects as the basis of fatigue design10.1016/j.ijfatigue.2011.12.001 ↗
37. What is fatigue damage? A view point from the observation of low cycle fatigue process10.1016/j.ijfatigue.2004.10.009 ↗
38. Fatigue performance of additive manufactured Ti-6Al-4V using electron and laser beam melting10.1016/j.ijfatigue.2016.05.001 ↗
39. Build orientation, surface roughness, and scan path influence on the microstructure, mechanical properties, and flexural fatigue behavior of Ti - 6Al - 4V fabricated by electron beam melting10.1016/j.msea.2019.138740 ↗