journal article·2023-10

High temperature VHCF of a 3rd generation Ni-based single crystal superalloy with different casting pore sizes

Yawei Li, Dong Wang, Yufeng He, Luciana Maria Bortoluci Ormastroni, Li Wang, Jonathan Cormier, Jian Zhang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Reed · 2006
2. Ultrasonic fatigue of a single crystal Ni-base superalloy at 1000 °C10.1016/j.msea.2006.08.028 ↗
3. High temperature ultrasonic fatigue testing of single-crystal superalloys10.1016/j.matlet.2011.11.066 ↗
4. LCF, HCF and VHCF life sensitivity to solution heat treatment of a third generation Ni-based single crystal superalloy10.1016/j.ijfatigue.2019.105247 ↗
5. Effect of inclusion on subsurface crack initiation and gigacycle fatigue strength10.1016/S0142-1123(02)00037-3 ↗
6. Study of thermal effects associated with crack propagation during very high cycle fatigue tests10.1016/j.actamat.2008.04.023 ↗
7. Subsurface crack initiation and propagation mechanisms in gigacycle fatigue10.1016/j.actamat.2010.07.022 ↗
8. Initiation and early-stage growth of internal fatigue cracking under very-high-cycle fatigue regime at high temperature10.1007/s11661-020-05633-3 ↗
9. Very high cycle fatigue of Ni-based single-crystal superalloys at high temperature10.1007/s11661-018-4672-6 ↗
10. Crack initiation mechanisms during very high cycle fatigue of Ni-based single crystal superalloys at high temperature10.1016/j.actamat.2020.02.012 ↗
11. Damage mechanisms during very high cycle fatigue of a coated and grit-blasted Ni-based single-crystal superalloy10.1016/j.ijfatigue.2020.105962 ↗
12. VHCF life of AM1 Ni-based single crystal superalloy after pre-deformation10.1016/j.ijfatigue.2021.106224 ↗
13. Elliot AJ, Karney GB, Gigliotti MFX, Pollock TM. Issues in processing by the liquid-Sn assisted directional solidification technique. In: Green KA, Pollock TM, Harada H, Howson TE, Reed RC, Schirra JJ, Walston S (Eds.). Superalloys 2004, TMS, 2004, pp. 421-30.10.7449/2004/Superalloys_2004_421_430 ↗
14. Directional solidification assisted by liquid metal cooling
15. Fritzemeier LG. The Influence of high thermal gradient casting, hot isostatic pressing and alternate heat treatment on the structure and properties of a single crystal nickel base superalloy. In: Reichman S, Duhl DN, Maurer G, Antolovich S, Lund C (Eds.). Superalloys 1988, TMS, 1988, pp. 265-74.10.7449/1988/Superalloys_1988_265_274 ↗
16. Pore annihilation in a single-crystal nickel-base superalloy during hot isostatic pressing: Experiment and modelling10.1016/j.msea.2013.08.034 ↗
17. Review on additive manufacturing of single-crystal nickel-based superalloys
18. Very high cycle fatigue durability of an additively manufactured single-crystal Ni-based superalloy
19. On the impact of an integrated HIP treatment on the very high cycle fatigue life of Ni-based SX superalloys10.1007/s11661-022-06882-0 ↗
20. VHCF life evolution after microstructure degradation of a Ni-based single crystal superalloy10.1016/j.ijfatigue.2017.07.021 ↗
21. Transition from internal to surface crack initiation of a single-crystal superalloy in the very-high-cycle fatigue regime at 1100 °C10.1016/j.ijfatigue.2021.106343 ↗
22. Mechanism of fatigue crack initiation and propagation in the very high cycle fatigue regime of high-strength steels
23. On the formation mechanisms of fine granular area (FGA) on the fracture surface for high strength steels in the VHCF regime10.1016/j.ijfatigue.2015.08.021 ↗
24. On the crystallographic, stage I-like, character of fine granular area formation in internal fish-eye fatigue cracks10.1016/j.ijfatigue.2017.09.013 ↗
25. A general scenario of fish-eye crack initiation on the life of high-strength steels in the very high-cycle fatigue regime10.1111/ffe.13104 ↗
26. Interior initiation and early growth of very high cycle fatigue crack in an additively manufactured Ti-alloy10.1016/j.ijfatigue.2022.106862 ↗
27. Low-cycle fatigue properties of nickel-based superalloys processed by high-gradient directional solidification10.1007/s40195-017-0563-x ↗
28. Measurements of cell and primary dendrite arm spacings in directionally solidified aluminium alloys10.1016/0001-6160(81)90111-5 ↗
29. Synchrotron tomography of porosity in single-crystal nickel-base superalloys10.1016/j.msea.2006.03.005 ↗
30. Brundidge · 2011
31. Brundidge CL, Pollock TM. Processing to fatigue properties: benefits of high gradient casting for single crystal airfoils. In: Huron ES, Reed RC, Hardy MC, Mills MJ, Montero RE, Portella PD, Telesman J (Eds.). Superalloys 2012, TMS, 2012, pp. 379-85.10.7449/2012/Superalloys_2012_379_385 ↗
32. Zhao Z, Liang Z, Li Q, Zhang F, Chen B. Crack initiation and propagation behaviour under high-temperature very-high-cycle fatigue: Directionally solidified columnar-grained vs. single-crystal superalloys. Mater Sci Eng A 2022;836:142711.10.1016/j.msea.2022.142711 ↗
33. Crack initiation anisotropy of Ni-based SX superalloys in the very high cycle fatigue regime10.1016/j.msea.2021.141920 ↗
34. Stacking faults in gamma prime Ni3(Al, Ti) precipitation hardened nickel-base alloys10.1007/BF03038373 ↗
35. Primary creep in single crystal superalloys: Origins, mechanisms and effects10.1016/j.actamat.2006.09.026 ↗
36. Shearing of γʹ precipitates by single a/2<110> matrix dislocations in a γ/γʹ Ni-based superalloy10.1016/0036-9748(87)90369-3 ↗
37. On precipitate shearing by superlattice stacking-faults in superalloys10.1080/01418618808204522 ↗
38. Development of γ phase stacking faults during high temperature creep of Ru-containing single crystal superalloys10.1016/j.actamat.2007.06.042 ↗
39. Mechanisms of high-temperature creep of nickel-based superalloys under low applied stresses10.1080/14786430410001663240 ↗
40. High-temperature dislocation climb in the γʹ rafts of single-crystal superalloys: The hypothesis of a control by dislocation entry into the rafts10.1007/s11661-018-4770-5 ↗
41. Intrinsic stacking fault energy and mechanism for deformation twin formation of solid solution matrix in Ni-based superalloys10.1016/j.vacuum.2022.111322 ↗
42. Oxygen diffusion and crack growth for a nickel-based superalloy under fatigue-oxidation conditions10.1016/j.msea.2012.12.088 ↗
43. In-situ environmental TEM study of γ-γʹ phase transformation induced by oxidation in a nickel-based single crystal superalloy10.1016/j.jallcom.2015.07.017 ↗
44. High temperature oxidation of a single crystal nickel-base superalloy (in Chinese)
45. Chemically oriented γ′ plate development in a nickel base superalloy10.1016/0036-9748(89)90475-4 ↗
46. The effect of cast microstructure and crystallography on rafting, dislocation plasticity and creep anisotropy of single crystal Ni-base superalloys10.1016/j.msea.2014.12.030 ↗
47. Effect of Ta on microstructural evolution of NiCrAlYSi coated Ni-base single crystal superalloys10.1016/j.jallcom.2020.154440 ↗