Tensile and fatigue behavior of electron beam welded TC17 titanium alloy joint
Source abstract
Abstract
Abstract The tensile fracture was originated from the strain concentration in equiaxed grain region adjacent to the fusion center, where a lower micro-hardness occurred when compared to the columnar grain region in the fusion zone. A higher stress level was more potential to fabricate a fatal fatigue crack initiating from the intrinsic metallic deficiencies. At a lower stress of 180 MPa, fatigue crack appeared to initiate from the intergranular welding pores other than the intrinsic metallic deficiencies. Furthermore, intergranular welding pores induced fatal crack initiation became the major fatigue crack initiation mechanisms when the fatigue stress amplitude down to 140 MPa.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Electron beam welding, laser beam welding and gas tungsten arc welding of titanium sheet10.1016/S0921-5093(99)00662-0 ↗
2. Effect of electron beam welding on the microstructures and mechanical properties of thick TC4-DT alloy10.1016/j.matdes.2011.09.004 ↗
3. Effects of the heterogeneity in the electron beam welded joint on fatigue crack growth in Ti–6Al–4V alloy10.1016/j.msea.2011.09.014 ↗
4. Mechanical properties of electron beam welded dissimilar joints of TC17 and Ti60 alloys10.1016/j.jmst.2018.02.014 ↗
5. Effect of welding speed on butt joint quality of Ti–6Al–4V alloy welded using a high-power Nd: YAG laser10.1016/j.optlaseng.2009.05.010 ↗
6. The origin of microstructural diversity, texture, and mechanical properties in electron beam melted Ti-6Al-4V10.1007/s11661-010-0397-x ↗
7. Plastic anisotropy of laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe titanium alloy10.1016/j.msea.2019.01.031 ↗
8. Wang S, Wu X. Investigation on the microstructure and mechanical properties of Ti–6Al–4V alloy joints with electron beam welding. Mater Design (1980-2015) 2012;36:663–70.10.1016/j.matdes.2011.11.068 ↗
9. Internal crack initiation characteristics and early growth behaviors for very-high-cycle fatigue of a titanium alloy electron beam welded joints10.1016/j.msea.2017.08.106 ↗
10. Beam oscillation, porosity formation and fatigue properties of electron beam welded Ti-6Al-4V alloy10.1016/j.jmatprotec.2018.10.040 ↗
11. Correlation of fatigue properties and microstructure in investment cast Ti-6Al-4V welds10.1016/S0921-5093(02)00176-4 ↗
12. The Kitagawa-Takahashi fatigue diagram to hybrid welded AA7050 joints via synchrotron X-ray tomography10.1016/j.ijfatigue.2019.04.002 ↗
13. Cyclic deformation of dissimilar welded joints between Ti–6Al–4V and Ti17 alloys: Effect of strain ratio10.1016/j.msea.2014.01.022 ↗
14. Very high cycle fatigue failure mechanism of TC17 alloy10.3724/SP.J.1037.2010.00046 ↗
15. Effect of stress ratio on VHCF behavior for a compressor blade titanium alloy10.1016/j.ijfatigue.2016.05.004 ↗
16. Dynamic globularization and restoration mechanism of Ti–5Al–2Sn–2Zr–4Mo–4Cr alloy during isothermal compression10.1016/j.jallcom.2014.10.043 ↗
17. Modification of alpha morphology in Ti-6Al-4V by thermo mechanical processing10.1007/BF02644991 ↗
18. Effect of aging heat treatment on microstructure and tensile properties of a new β high strength titanium alloy10.1016/j.jallcom.2013.10.096 ↗
19. Microstructure and mechanical properties of electron beam welded titanium alloy Ti-624610.1016/j.jmst.2016.10.007 ↗
20. Segregation and grain refinement in cast titanium alloys10.1557/jmr.2009.0173 ↗
21. Trace carbon addition to refine microstructure and enhance properties of additive-manufactured Ti-6Al-4V10.1007/s11837-018-2994-x ↗
22. Columnar to equiaxed grain transition in as solidified alloys10.1179/174328006X102493 ↗
23. Microstructure study of direct laser fabricated Ti alloys using powder and wire10.1016/j.apsusc.2006.02.028 ↗
24. Grain-refinement mechanisms in titanium alloys10.1557/JMR.2008.0002 ↗
25. Phase transformations during cooling in α+ β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
26. Effect of the metastable beta-phase transformations in the Ti-6Al-4V alloy
27. In situ analysis of plasticity and damage nucleation in a Ti-6Al-4V alloy and laser weld10.1016/j.matchar.2018.09.039 ↗
28. Laser welding of Ti6Al4V titanium alloys10.1016/j.jmatprotec.2008.08.026 ↗
29. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
30. Reducing arc heat input and obtaining equiaxed grains by hot-wire method during arc additive manufacturing titanium alloy10.1016/j.msea.2018.11.022 ↗
31. Microstructure and tensile properties of laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe near β titanium alloy10.1016/j.msea.2013.08.032 ↗
32. Influence of continuous grain boundary α on ductility of laser melting deposited titanium alloys10.1016/j.msea.2016.03.034 ↗
33. Localized tensile strain distribution and metallurgy of electron beam welded Ti–5Al–5V–5Mo–3Cr titanium alloys10.1016/j.jmatprotec.2012.06.023 ↗
34. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗