Fatigue crack branching in laser melting deposited Ti–55511 alloy
Source abstract
Abstract
Abstract Significant crack branching was observed in constant amplitude fatigue crack growth test of laser melting deposited Ti–55511 alloy. Fracture microscopic observations indicate that the orderly distributed αp laths is the most important factor as it contributes a lot to the initiation of secondary cracks and coalescence of microcracks. Propagation of subsurface secondary cracks led to remarkable crack branching observed on the specimen surface. The crack tip strain fields were measured by digital image correlation method, which gave a good monitoring of the crack branching process and helps a lot to understand the mechanism of crack branching behavior.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Practical considerations and capabilities for laser assisted direct metal deposition10.1016/S0261-3069(99)00078-3 ↗
2. Microstructure and mechanical properties of laser melting deposited γ-tial intermetallic alloys10.1016/j.msea.2007.02.073 ↗
3. Characterization of microstructure and mechanical properties of laser melting deposited Ti–6.5Al–3.5Mo–1.5Zr–0.3Si titanium alloy10.1016/j.matdes.2013.11.044 ↗
4. Microstructural characterization of laser melting deposited Ti–5Al-5Mo–5V–1Cr–1Fe near β titanium alloy10.1016/j.jallcom.2013.03.243 ↗
5. The influences of anneal temperature and cooling rate on microstructure and tensile properties of laser deposited Ti–4Al–1.5Mn titanium alloy10.1016/j.jallcom.2014.04.058 ↗
6. Preliminary investigation on selective laser melting of Ti-5Al-2.5Sn α-Ti alloy: from single tracks to bulk 3D components10.1016/j.jmatprotec.2017.01.032 ↗
7. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti-6Al-4V10.1016/j.msea.2013.04.099 ↗
8. An overview of Direct Laser Deposition for additive manufacturing; Part II: Mechanical behavior, process parameter optimization and control
9. Comparison on mechanical anisotropies of selective laser melted Ti-6Al-4V alloy and 304 stainless steel10.1016/j.msea.2017.04.031 ↗
10. Selective laser melting-wire arc additive manufacturing hybrid fabrication of Ti-6Al-4V alloy: microstructure and mechanical properties10.1016/j.msea.2016.12.065 ↗
11. Plastic anisotropy of laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe titanium alloy10.1016/j.msea.2019.01.031 ↗
12. Anisotropy of fatigue crack growth in wire arc additive manufactured Ti-6Al-4V10.1016/j.msea.2017.10.064 ↗
13. Fatigue crack growth behaviour in laser melting deposited Ti-6.5Al-3.5Mo-1.5Zr-0.3Si alloy10.1016/j.msea.2017.03.001 ↗
14. Fatigue crack tip strain evolution and crack growth prediction under single overload in laser melting deposited Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy10.1016/j.ijfatigue.2018.07.011 ↗
15. Leyens · 2003
16. Study on the fatigue crack growth rates of Ti-5Al-5Mo-5V-1Cr-1Fe titanium alloy with basket-weave microstructure10.1016/j.msea.2014.10.022 ↗
17. Effects of microstructure on fatigue crack propagation behavior in a bi-modal TC11 titanium alloy fabricated via laser additive manufacturing
18. Brittle fracture behavior of a laser additive manufactured near-β titanium alloy after low temperature aging10.1016/j.msea.2017.05.050 ↗
19. Hot deformation of Ti-5Al-5Mo-5V-1Cr-1Fe near β titanium alloys containing thin and thick lamellar α phase10.1016/j.msea.2013.02.033 ↗
20. Development of a pre-heat treatment for obtaining discontinuous grain boundary α in laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe alloy10.1016/j.msea.2014.03.028 ↗
21. Microstructure and tensile properties of laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe near β titanium alloy10.1016/j.msea.2013.08.032 ↗
22. Effect of primary α phase on the fatigue crack path of laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe near β titanium alloy10.1016/j.ijfatigue.2018.06.041 ↗
23. Effect of micromorphology at the fatigue crack tip on the crack growth in electron beam welded Ti-4Al-4Mo-2Sn-0.5Si joint10.1016/j.matchar.2016.08.029 ↗
24. Effect of trace solute hydrogen on the fatigue life of electron beam welded Ti-6Al-4V alloy joints10.1016/j.msea.2016.12.102 ↗
25. Effect of α-phase morphology on low-cycle fatigue behavior of TC21 alloy10.1016/j.ijfatigue.2015.01.010 ↗
26. Standard test method for measurement of fatigue crack growth rates; ASTM International; 2015.
27. Digital imaging techniques in experimental stress analysis10.1117/12.7972925 ↗
28. Evaluation of crack-tip fields from DIC data: a parametric study10.1016/j.ijfatigue.2016.03.006 ↗
29. Full field measurements of anisotropic stress intensity factor ranges in fatigue10.1016/j.engfracmech.2012.06.002 ↗
30. Crack tip deformation fields and fatigue crack growth rates in Ti-6Al-4V10.1016/j.ijfatigue.2009.02.043 ↗