journal article·2019-03

Evolution and characterization of cyclic thermal shock-induced thermomechanical damage in oxide/oxide ceramics matrix composites

Zhengmao Yang, Huang Yuan, Hui Liu

Publisher page

Abstract

Abstract Thermal shock is a typical loading case for high temperature components in turbines. The ceramic matrix composites become attractive for their high temperature behavior. However, their low heat conductivity makes thermal shock damage a typical damage mechanism for the turbine application. In the present paper, microstructural evolutions of the oxide/oxide ceramic matrix composite under thermal shock are studied experimentally. The mechanical behavior is related to the thermal shock temperature and cycles. The thermomechanical damage is characterized by degradation of the macroscopic elastic modulus. A thermal shock damage model is introduced based on the continuum damage mechanics principle, which can describe monotonic as well as cyclic thermal shock damage processes.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Mechanical behavior of a notched oxide/oxide ceramic matrix composite in combustion environment: experiments and simulations10.1016/j.compstruct.2015.02.040 ↗
2. Assessment of three oxide/oxide ceramic matrix composites: Mechanical performance and effects of heat treatments10.1016/j.compositesa.2014.09.013 ↗
3. Cyclic loading of a sic-fiber reinforced ceramic matrix composite reveals damage mechanisms and thermal residual stress state10.1016/j.compositesa.2012.06.011 ↗
4. An experimental apparatus and procedure for the simulation of thermal stresses in gas turbine combustion chamber panels made of ceramic matrix composites10.1115/1.4035906 ↗
5. Thermal shock resistance of ceramics with temperature-dependent material properties at elevated temperature10.1016/j.actamat.2010.10.068 ↗
6. Thermal shock residual strength of functionally graded ceramics10.1016/j.msea.2006.07.011 ↗
7. High performance oxide fibers for metal and ceramic composites10.1016/S1359-835X(00)00176-7 ↗
8. Tension-compression fatigue of an oxide/oxide ceramic composite at elevated temperature10.1016/j.msea.2016.02.057 ↗
9. Creep mechanisms and microstructure evolution of Nextel™ 610 fiber in air and steam10.1016/j.jeurceramsoc.2014.01.032 ↗
10. Microstructure and mechanical behaviour of a Nextel610/alumina weak matrix composite subjected to tensile and compressive loadings10.1016/j.jeurceramsoc.2017.02.042 ↗
11. Thermal-shock resistance of laminated ceramic matrix composites10.1007/BF01124828 ↗
12. Carper DM, Nied HF. Thermal shock resistance of ceramic matrix composites. Report NASA-CR-189136, NASA; 1995.
13. Thermal shock behavior of two-dimensional woven fiber-reinforced ceramic composites10.1111/j.1151-2916.1996.tb07996.x ↗
14. Thermal shock fracture in unidirectional fibre-reinforced ceramic-matrix composites10.1016/j.compscitech.2005.04.004 ↗
15. Thermal shock fracture in cross-ply fibre-reinforced ceramic-matrix composites10.1080/14786431003785621 ↗
16. Cyclic thermal-shock in SiC-whisker-reinforced alumina composite10.1016/0921-5093(89)90530-3 ↗
17. Thermal shock fiber-reinforced ceramic matrix composites10.1002/9780470313831.ch43 ↗
18. Thermal-shock behavior of fiber-reinforced ceramic-matrix composites10.1016/0961-9526(95)00051-N ↗
19. Thermal shock damage in a two-dimensional woven-fiber-reinforced-CVI SiC-matrix composite10.1111/j.1151-2916.1996.tb08719.x ↗
20. Investigation of cyclic thermal shock behaviour of fibre reinforced glass matrix composites using non-destructive forced resonance technique10.1179/mst.1997.13.10.852 ↗
21. Influence of fiber orientation and matrix processing on the tensile and creep performance of Nextel 610 reinforced polymer derived ceramic matrix composites10.1016/j.msea.2014.07.027 ↗
22. Degradation ofoxidefibersbythermaloverloadandenvironmentaleffects10.1016/j.msea.2012.05.107 ↗
23. A continuum damage model for multi-axial low cycle fatigue of porous sintered metals based on the critical plane concept10.1016/j.mechmat.2016.09.013 ↗
24. Continuum damage mechanics for sintered powder metals10.1007/s11433-014-5529-7 ↗
25. Lemaitre · 2005
26. Vaccaro · 2002
27. Effect of microstructure on mechanical properties and residual stresses in interpenetrating aluminum-alumina composites fabricated by squeeze casting10.1016/j.msea.2017.12.091 ↗
28. Thermal shock behaviour of unidirectional silicon carbide fibre reinforced calcium aluminosilicate10.1023/A:1018588913469 ↗
29. Assessment of damage induced by thermal shock in SiC-fiber-reinforced borosilicate glass composites10.1016/S0266-3538(98)00053-0 ↗
30. Modification and validation of the thermal shock parameter for ceramic matrix composites under water quenching condition10.1016/j.matdes.2009.04.037 ↗
31. Factors affecting thermal stress resistance of ceramic materials10.1111/j.1151-2916.1955.tb14545.x ↗
32. Simon RA, Supancic P. Thermal shock resistance of Nextel610 and Nextel720 continuous fiber-reinforced mullite matrix composites. In: 28th International Conference Advanced Cerainics and Contposites: B. The American Ceramic Society; 2004. p. 105–10.10.1002/9780470291191.ch17 ↗
33. A non-linear continuous fatigue damage model10.1111/j.1460-2695.1988.tb01216.x ↗
34. A new formulation of continuum damage mechanics (CDM) for composite materials10.1016/S1270-9638(97)90035-3 ↗