journal article·2016-06

Role of microstructure on initiation and propagation of fatigue cracks in precipitate strengthened Cu–Ni–Si alloy

M. Goto, S.Z. Han, S.H. Lim, J. Kitamura, T. Fujimura, J.-H. Ahn, T. Yamamoto, S. Kim, J. Lee

Publisher page

Abstract

Abstract Fatigue tests were conducted on round-bar specimens to understand the fatigue behavior of precipitate-strengthened Cu–6Ni–1.5Si alloy. Aging at 500 °C for 0.5 h produced δ-Ni 2 Si precipitates in the matrix, homogeneously and heterogeneously precipitated δ-Ni 2 Si particles, and a precipitate-free zone around the grain boundaries. The cracks were initiated at the grain boundaries, followed by growth along the crystallographic slip planes in the adjacent grains. Crack propagation from the crack origin along the grain boundaries was occasionally observed. The physical background of fatigue damage is discussed in light of the role of microstructure on the behavior of fatigue cracks.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Electrical conductor alloys
2. Effect of alloy composition on precipitation behavior in Cu–Ni–Si alloys10.2320/jinstmet1952.62.4_301 ↗
3. Fatigue of precipitate strengthened Cu–Ni–Si alloy10.1179/026708399101505194 ↗
4. Structure and strength of the age hardened Cu–Ni–Si alloy10.1016/S0254-0584(02)00451-0 ↗
5. Effect of thermomechanical treatment on spray formed Cu–Ni–Si alloy10.1179/026708304225017265 ↗
6. Improvement in strength and electrical conductivity of Cu–Ni–Si alloys by aging and cold rolling10.1016/j.jallcom.2005.09.037 ↗
7. Dynamic embrittlement at intermediate temperature in a Cu–Ni–Si alloy10.1016/j.msea.2007.05.013 ↗
8. Microstructure and mechanical properties of Cu–Ni–Si alloys10.1016/j.msea.2006.12.163 ↗
9. Microstructure and solidification behavior of Cu–Ni–Si alloys10.1016/j.matchar.2008.07.008 ↗
10. The crystallographic and morphological evolution of the strengthening precipitates in Cu–Ni–Si alloys10.1016/j.actamat.2012.10.031 ↗
11. Dynamic embrittlement during fatigue of a Cu–Ni–Si alloy10.1016/j.msea.2011.04.069 ↗
12. Cyclic softening of Cu–Ni–Si alloy single crystals under low-cycle fatigue10.4028/www.scientific.net/MSF.654-656.1287 ↗
13. Effects of Ti addition and heat treatments on mechanical and electrical properties of Cu–Ni–Si alloys10.1007/s12540-013-1011-8 ↗
14. Discontinuous (cellular) precipitation10.1023/A:1006510228181 ↗
15. Significance of initiation, propagation and closure of microcracks in high cycle fatigue of ductile metals10.1016/0013-7944(81)90070-9 ↗
16. Goto M, DuQuesnay DL. Fatigue behavior of 6061-T6 aluminum alloy plain specimens. SAE tech paper ser 1997; No. 970703. p. 1–7.10.4271/970703 ↗
17. Statistical description of the effect of Zr addition on the behavior of microcracks in Cu–6Ni–2Mn–2Sn–2Al Alloy10.1007/s10853-011-5935-4 ↗
18. Fatigue crack initiation and microcrack propagation in X7091 type aluminum P/M alloys10.1007/BF02659866 ↗
19. The initiation and growth of intergranularly initiated short fatigue cracks in an aluminium 4.5 per cent copper alloy
20. Fatigue of aluminium–lithium alloys10.1179/imr.1992.37.1.153 ↗
21. Fatigue crack initiation and early propagation behavior of 2A97 Al−Li alloy10.1016/S1003-6326(14)63061-2 ↗
22. Tensile and electrical properties of direct aged Cu–Ni–Si–x%Ti alloys10.1007/s12540-013-2007-0 ↗
23. A small-crack growth law and its related phenomena10.1016/0013-7944(92)90297-R ↗
24. Fatigue life prediction of heat-treated carbon steels and low alloy steels based on a small-crack growth law10.1111/j.1460-2695.1994.tb00799.x ↗