The role of crack origin size and early stage crack growth on high cycle fatigue of powder metallurgy Ti-6Al-4V alloy

Fei Cao, K.S. Ravi Chandran

Abstract

Abstract In this work, fatigue failure mode, crack initiation, and early stage crack growth mechanism in Ti-6Al-4V alloys with different levels of microstructural inhomogeneity were investigated. The quantitative correlations between fatigue life, crack origin size, and early stage short crack growth, were analyzed and discussed. The interior early stage short crack growth rate was determined to be 10−12–10−10 m/cycle. The high and very high cycle fatigue lives predicted based on crack initiation site size and early stage short crack growth rate agree well with real fatigue data.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Titanium Alloys Microstructure and Properties · Fatigue and fracture mechanics · Additive Manufacturing Materials and Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Fatigue crack initiation in hot isostatically pressed Ti-6Al-4V castings10.1007/BF00551032 ↗
2. Microstructure evolution and mechanical properties of powder metallurgy Ti-6Al-4V alloy based on heat response10.1016/j.msea.2015.05.041 ↗
3. Mechanical properties of titanium-based Ti-6Al-4V alloys manufactured by powder bed additive manufacture10.1080/02670836.2016.1172787 ↗
4. On the mechanical behavior of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
5. Influence of defects on mechanical properties of Ti-6Al-4V components produced by selective laser melting and electron beam melting10.1016/j.matdes.2015.07.147 ↗
6. Internal fatigue origins in α-β titanium alloys10.1016/0001-6160(76)90147-4 ↗
7. Subsurface crack initiation in high cycle fatigue in Ti6A14V and in a typical martensitic stainless steel10.1016/0036-9748(83)90385-X ↗
8. Understanding competing fatigue mechanisms in powder metallurgy Ti-6Al-4V alloy: role of crack initiation and duality of fatigue response10.1016/j.msea.2015.02.028 ↗
9. Gigacycle fatigue properties of Ti-6Al-4V alloy under tensile mean stress10.1016/j.msea.2014.01.019 ↗
10. Materials science perspective of metal fatigue resistance10.1179/mst.1993.9.6.453 ↗
11. Propagation behaviour of microstructural short fatigue cracks in the high-cycle fatigue regime10.1016/j.commatsci.2009.01.019 ↗
12. The twisting mechanism of subsurface fatigue cracking in Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy10.1016/j.engfracmech.2010.04.011 ↗
13. Subsurface crack generation in high-cycle fatigue for high strength alloys10.2355/isijinternational.37.1170 ↗
14. Fatigue crack propagation properties of Ti-6Al-4V in vacuum environments10.1016/j.ijfatigue.2012.02.012 ↗
15. Effects of stress ratio on high-cycle and very-high-cycle fatigue behavior of a Ti-6Al-4V alloy10.1016/j.msea.2014.09.115 ↗
16. Deformation heterogeneities and their role in life-limiting fatigue failures in a two-phase titanium alloy10.1016/j.actamat.2014.08.034 ↗
17. Characteristic S-N properties of high –carbon-chromium-bearing steel under axial loading in long-life fatigue10.1046/j.1460-2695.2002.00574.x ↗
18. Propensities of crack interior initiation and early growth for very-high-cycle fatigue of high strength steels10.1016/j.ijfatigue.2013.02.023 ↗
19. Hydrogen sintering of titanium to produce high density fine grain titanium alloy10.1002/adem.201100269 ↗
20. Phase transformation and formation of ultra-fine microstructure during hydrogen sintering and phase transformation (HSPT) processing of Ti-6Al-4V10.1007/s11661-015-3141-8 ↗
21. New powder metallurgical approach to achieve high fatigue strength in Ti-6Al-4V alloy10.1007/s11661-016-3409-7 ↗
22. Fatigue crack growth in miniature specimens: the equivalence of ΔK-correlation and that based on the change in net-section strain energy density10.1016/j.scriptamat.2016.05.018 ↗
23. Effect of load ratio and maximum stress intensity on the fatigue threshold in Ti-6Al-4V10.1016/S0013-7944(00)00099-0 ↗
24. Influence of microstructure on high-cycle fatigue of Ti-6Al-4V: bimodal vs. lamellar structures10.1007/s11661-002-0160-z ↗
25. Modeling the fatigue crack growth behavior of Ti-6Al-4V by considering grain size and stress ratio10.1016/j.msea.2011.04.046 ↗
26. Factors influencing the mechanism of super long fatigue failure in steels10.1046/j.1460-2695.1999.00187.x ↗
27. McClung RC, Lawless BH, Gorelik M, Date C, Gill Y, Piascik RS. Fatigue crack growth of titanium rotor alloys in vacuum and air. TMS Fall Meeting, Symposium on Fatigue Behavior of Titanium Alloys, Chicago, IL October 1998. In: Boyer RR, Eylon D, Luetjering G, editors. Fatigue behavior of titanium alloys; 1999.
28. The effect of air and vacuum environments on fatigue crack growth rates in Ti-6Al-4V10.1007/BF02644106 ↗
29. On the mechanism of very high cycle fatigue in Ti–6Al–4V10.1016/j.scriptamat.2008.08.012 ↗
30. An argument for a cycle-by-cycle propagation of fatigue cracks at small stress intensity ranges10.1016/S1359-6454(97)00366-2 ↗
31. Low Delta K faceted crack growth in titanium alloys10.1016/j.ijfatigue.2008.03.036 ↗
32. Modeling the threshold conditions for the propagation of a stage I fatigue crack10.1016/S1359-6454(97)00290-5 ↗
33. Microstructurally short fatigue crack initiation and growth in Ti-6.8 Mo-4.5 Fe-1.5 Al10.1016/S0921-5093(99)00575-4 ↗
34. Simulation of stage I-short crack propagation in forged Ti-6Al-4V10.1016/j.engfracmech.2007.02.018 ↗
35. Local plasticity exhaustion in a very high cycle fatigue regime10.1016/j.scriptamat.2012.02.003 ↗
36. On fatigue crack initiation in the matrix in very high cycle fatigue regime10.4028/www.scientific.net/MSF.783-786.2266 ↗
37. Experimental and crystal plasticity studies of deformation and crack nucleation in a titanium alloy10.1243/03093247JSA594 ↗
38. The high-cycle fatigue behavior of Ti-6Al-4V alloy10.1016/0013-7944(76)90075-8 ↗
39. Effects of vacuum environment on small fatigue crack propagation in Ti-6Al-4V10.1016/j.ijfatigue.2016.05.024 ↗
40. Non-destructive observation of internal fatigue crack growth in Ti–6Al–4V by using synchrotron radiation μCT imaging10.1016/j.ijfatigue.2016.05.028 ↗