Calibration of the potential drop method for monitoring small crack growth from surface anomalies – Crack front marking technique and finite element simulations
Source abstract
Abstract
Abstract The Direct Current Potential Drop method is one of the possibilities to measure the crack growth during fatigue tests without optical access to the sample. The accuracy of this technique applied to short cracks mainly depends on the calibration curve. In the present work experimental and numerical approaches are proposed to calibrate the potential drop measurement. An optimization of the calibration procedure is supported by finite element calculations. The crack front shape and the location of the potential probes are found to be of great influence. An extensive study is conducted to identify all the mechanisms controlling the potential drop measurement. Plastic deformation remains the last parameter which is not directly considered in this study; therefore a calibration strategy is suggested to take into account this effect and achieve a calibration curve with high accuracy. This strategy shows a very good agreement between the obtained calibration curve and the experimental calibration.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fatigue and fracture mechanics · Structural Health Monitoring Techniques · Non-Destructive Testing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Experimental and numerical investigation of crack closure measurements with electrical potential drop technique10.1016/j.ijfatigue.2005.11.005 ↗
2. Characterization of crack tip and geometry induced closure10.1016/S0142-1123(97)00019-4 ↗
3. Automated visualization of surface morphology of cracks by means of induced current potential drop technique10.1016/j.ndteint.2012.04.005 ↗
4. An alternative method for crack interaction in NDE of multiple cracks by means of potential drop technique10.1016/j.ndteint.2004.02.003 ↗
5. A three-point electrical potential difference method for in situ monitoring mixed-mode cracks at high temperature10.1016/j.measurement.2010.03.012 ↗
6. Measurement of subcritical growth of defects in large components of nuclear power plants at elevated temperatures10.1016/S0013-7944(03)00012-2 ↗
7. Direct current potential difference correlation for open-hole, single-crack coupons
8. On the calibration of the electrical potential technique for monitoring crack growth using finite element methods10.1007/BF00115908 ↗
9. A comparison of theoretical and experimental methods of calibrating the electrical potential drop technique for crack length determination10.1007/BF01141259 ↗
10. Electrolytic tank simulation of the potential drop technique for crack length determinations10.1007/BF00020701 ↗
11. Crack growth monitoring: optimization of the electrical potential technique using an analogue method10.1007/BF00189118 ↗
12. Calibrating the electrical potential method for studying slow crack growth
13. Application of the electrical potential method to crack length measurements using Johnson’s formula10.1520/JTE11560J ↗
14. The use of DCPD method for measurement of growth of cracks in large components at normal and elevated temperatures10.1016/S0013-7944(03)00012-2 ↗
15. Measurement of fatigue cracks in notched specimens by means of theoretical electrical potential calibrations10.1016/0022-5096(75)90028-9 ↗
16. Analytic and analogue techniques for determining potential distributions around angled cracks10.1007/BF00017825 ↗
17. The potential drop method for monitoring crack growth in real components subjected to combined fatigue and creep conditions: application of FE techniques for deriving calibration curves10.1016/S0308-0161(01)00103-X ↗
18. Optimization of the electrical potential technique for crack growth monitoring in compact test pieces using finite element analysis10.1520/JTE11382J ↗
19. Growth and retardation of physically short fatigue cracks in an aircraft Al-alloy after shot peening10.1016/j.proeng.2011.04.562 ↗
20. Nouvelle méthode de mesure électrique de longueur de fissure
21. Détermination de fronts de fissure dans les pièces métalliques tridimensionnelles par mesure électrique
22. An electric potential drop technique for characterizing part-through surface cracks10.1016/0022-3115(92)90632-U ↗
23. Effect of stress on resistivity–strain relation of aluminium
24. Roux P. Etude de l’influence de la contrainte, du champ magnétique et de la température sur le pouvoir thermoélectrique des matériaux métalliques. PhD thesis. INSA Lyon; 2008 [in french].
25. Crack growth micro-mechanisms in the IN718 alloy under the combined influence of fatigue, creep and oxidation10.1016/j.ijfatigue.2009.01.023 ↗
26. Soria D. NI 210 YLEV. Internal Report Safran Snecma.
27. High-temperature, high-strength nickel base alloys. Nickel Development Institute; 1995.