journal article·2026-01

On the role of weak interface in the high cycle fatigue damage mechanism at elevated temperature in forged TNM-TiAl alloy

Guanze Sun, Jiale He, Rui Cao, Xingshui Luo, Jinghuan Chang, Zihua Zhao

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced materials and composites · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Advances in gammalloy materials–processes–application technology: successes, dilemmas, and future10.1007/s11837-018-2747-x ↗
2. Advances and challenges of TiAl base alloys
3. Effects of high niobium addition on the mechanical properties and high-temperature deformability of gamma TiAl alloy10.1016/S0966-9795(01)00121-2 ↗
4. Gamma Ti aluminides for non-aerospace applications
5. Gamma titanium aluminides as prospective structural materials10.1016/S0966-9795(00)00073-X ↗
6. Oehring · 2011
7. Fatigue crack growth behaviour of a gamma-titanium-aluminide alloy prepared by casting and powder metallurgy10.1016/S1359-6462(03)00482-2 ↗
8. Mechanisms of ambient temperature fatigue crack growth in Ti−46.5Al−3Nb−2Cr−0.2W
9. The effect of microstructure on fracture toughness and fatigue crack growth behavior in gamma-titanium aluminide based intermetallics10.1007/s11661-999-0048-2 ↗
10. Polysynthetic twinned TiAl single crystals for high-temperature applications10.1038/nmat4677 ↗
11. On the origin of superior high strength of Ti–45Al–10Nb alloys10.1016/S0966-9795(02)00008-0 ↗
12. Fracture and R-curve behavior of an intermetallic β-stabilized TiAl alloy with different nearly lamellar microstructures10.1016/j.intermet.2014.04.005 ↗
13. The cavitation of high Nb-containing TiAl alloys during tensile tests around BDTT10.1016/j.msea.2018.05.028 ↗
14. TiAI alloys in commercial aircraft engines10.1080/09603409.2016.1183068 ↗
15. Leyens C, Titanium PM, Weinheim TA. WILEY-VCH Verlag GmbH & Co; 2003.
16. High cycle fatigue in a single crystal superalloy: time dependence at elevated temperature10.7449/2004/Superalloys_2004_657_666 ↗
17. The behavior of crack initiation and early growth in high-cycle and very-high-cycle fatigue regimes for a titanium alloy10.1016/j.ijfatigue.2018.03.021 ↗
18. Effect of the microstructure on the deformation and fatigue damage in a gamma-TiAl produced by additive manufacturing
19. On the fatigue behavior of g-based titanium aluminides: role of small cracks10.1016/S1359-6454(98)00409-1 ↗
20. In situ observation of fatigue crack initiation and propagation behavior of a high-Nb TiAl alloy at 750◦C10.1016/j.msea.2015.04.062 ↗
21. The significance of acoustic emission during stressing of TiAl-based alloys. Part I: detection of cracking during loading up in tension10.1016/S1359-6454(01)00091-X ↗
22. Processing, microstructure and tensile properties of a Ti-48 AT.% Al alloy10.1016/0956-716X(95)00088-D ↗
23. Temperature dependent anisotropic mechanical behavior of TiAl based alloys10.1016/j.ijplas.2021.103175 ↗
24. Deformation-induced internal stresses in multiphase titanium aluminide alloys10.1016/j.actamat.2013.10.024 ↗
25. Slip bands in lamellar TiAl during high cycle fatigue micro compression by correlative total strain mapping, diffraction orientation mapping and transmission electron imaging10.1016/j.ijfatigue.2019.03.016 ↗
26. Site occupation in the ordered beta phase ternary Ti-Al-Nb alloys10.1016/0036-9748(87)90367-X ↗
27. Microstructures and mechanical properties of a multi-phase β-solidifying TiAl alloy densified by spark plasma sintering10.1016/j.actamat.2014.03.058 ↗
28. The cavitation of high Nb-containing TiAl alloys during tensile tests around BDTT10.1016/j.msea.2018.05.028 ↗
29. Alloying mechanism of beta stabilizers in a TiAl alloy10.1007/s11661-001-0136-4 ↗
30. Microstructure determined fracture behavior of a high Nb containing TiAl alloy10.1016/j.msea.2016.04.074 ↗
31. Evolution of fatigue crack growth and fracture behavior in gamma titanium aluminide Ti-43.5Al-4Nb-1Mo-0.1B (TNM) forgings10.1016/j.ijfatigue.2018.01.026 ↗
32. Fatigue crack growth and fracture behavior of as-cast Ti-43.5Al-4Nb-1Mo-0.1B (TNM) compared to Ti-48Al-2Nb-2Cr (4822)10.1016/j.intermet.2017.08.015 ↗
33. Effect of stress ratio on high cycle fatigue behavior of TNM‐TiAl alloy10.1111/ffe.13835 ↗
34. Study on high cycle fatigue properties of TNM-TiAl alloy at room temperature
35. Plasticity and brittleness of the ordered βo phase in a TNM-TiAl alloy10.1016/j.intermet.2022.107653 ↗
36. On the role of nanocrystallization and cavitation to early damage of VHCF in selective laser melting Ti-6Al-4V alloy10.1016/j.ijfatigue.2024.108506 ↗
37. Cross-scale early damage mechanism of VHCF based on the initiation and evolution of fine granular area in selective laser melting Ti-6Al-4V alloy10.1016/j.ijfatigue.2024.108641 ↗
38. Gas pore-based fatigue strength and fatigue life prediction models of laser additive manufactured Ti-6Al-4V alloy in very high cycle fatigue regime10.1016/j.msea.2024.147640 ↗
39. Nanograin formation and cracking mechanism in Ti alloys under very high cycle fatigue loading10.1016/j.ijfatigue.2022.107331 ↗
40. Propensities of crack interior initiation and early growth for very-high-cycle fatigue of high strength steels10.1016/j.ijfatigue.2013.02.023 ↗
41. High-temperature structural intermetallics10.1016/S1359-6454(99)00301-8 ↗
42. Deformation mechanisms in TiAl intermetallics-experiments and modeling10.1016/S0749-6419(01)00036-5 ↗
43. Ordered domains in TiAl coexisting with Ti3Al in the lamellar structure of Ti-rich TiAl compounds10.1080/01418619208201574 ↗
44. On the role of microstructure in fatigue-crack growth of γ-based titanium aluminides
45. Effects of stress concentrations on the fatigue life of a gamma-based titanium aluminide10.1016/0921-5093(94)03245-9 ↗
46. Effect of composition on grain refinement in TiAl-based alloys10.1016/S0966-9795(01)00079-6 ↗
47. High cycle fatigue properties of Ti-48Al-2Cr-2Nb alloy additively manufactured via twin-wire directed energy deposition-arc
48. High-temperature tensile and fatigue properties of Ti-48Al-2Cr-2Nb alloy additively manufactured via twin-wire directed energy deposition-arc10.1016/j.intermet.2025.108833 ↗
49. Effects of test orientation on fracture and fatigue crack growth behavior of third generation as-cast Ti–48Al–2Nb–2Cr10.1016/j.intermet.2014.10.005 ↗
50. In situ observation of fatigue crack initiation and propagation behavior of a high-Nb TiAl alloy at 750°C
51. Temperature dependence of the mechanical properties of equiatomic solid solution alloys with face-centered cubic crystal structures10.1016/j.actamat.2014.08.026 ↗
52. Temperature dependence of the flow stress of Fe-18Mn-0.6C-xAl twinning-induced plasticity steel10.1016/j.actamat.2013.07.042 ↗
53. Realistic constitutive relations for metal plasticity10.1016/S0921-5093(01)01174-1 ↗
54. A “universal” temperature scale for plastic flow10.1016/0001-6160(86)90088-X ↗
55. A constitutive description of the deformation of copper based on the use of the mechanical threshold stress as an internal state variable10.1016/0001-6160(88)90030-2 ↗