journal article·2025-08

Effect of oxidation on the competition between internal and external fatigue crack initiation of Ni-based single crystal superalloy

Yang Meng, Chungen Zhou, Zihua Zhao, Yuliang Shen, Haonan Pei, Ming Zhao

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Reed RC. The Superalloys: Fundamentals and Applications n.d.:390. https://doi.org/10.1017/CBO9780511541285.10.1017/CBO9780511541285 ↗
2. A “universal” temperature scale for plastic flow10.1016/0001-6160(86)90088-X ↗
3. Crack initiation anisotropy of Ni-based SX superalloys in the very high cycle fatigue regime10.1016/j.msea.2021.141920 ↗
4. Crack initiation mechanisms during very high cycle fatigue of Ni-based single crystal superalloys at high temperature10.1016/j.actamat.2020.02.012 ↗
5. Fatigue strength of a single crystal in the gigacycle regime10.1016/j.ijfatigue.2007.04.003 ↗
6. Furuya Y, Kobayashi K, Hayakawa M, Sakamoto M, Koizumi Y, Harada H. High-Temperature Ultrasonic Fatigue Testing at 1000 degrees C. In: Clark G, Wang CH, editors. 11th International Fatigue Congress, Pts 1 and 2, vol. 891–892, Stafa-Zurich: Trans Tech Publications Ltd; 2014, p. 1413–8. https://doi.org/10.4028/www.scientific.net/AMR.891-892.1413.10.4028/www.scientific.net/AMR.891-892.1413 ↗
7. High-temperature ultrasonic fatigue testing of single-crystal superalloys10.1016/j.matlet.2011.11.066 ↗
8. Ultrasonic fatigue of a single crystal Ni-base superalloy at 1000°C10.1016/j.msea.2006.08.028 ↗
9. Very high cycle fatigue of Ni-based single-crystal superalloys at high temperature10.1007/s11661-018-4672-6 ↗
10. Crack initiation and propagation behaviour under high-temperature very-high-cycle fatigue: Directionally solidified columnar-grained vs. single-crystal superalloys
11. HCF and VHCF life sensitivity to solution heat treatment of a third-generation Ni-based single crystal superalloy
12. VHCF life evolution after microstructure degradation of a Ni-based single crystal superalloy10.1016/j.ijfatigue.2017.07.021 ↗
13. Benefits of high gradient solidification for creep and low cycle fatigue of AM1 single crystal superalloy10.1016/j.msea.2015.07.045 ↗
14. High-temperature ultra-high cycle fatigue damage of notched single crystal superalloys at high mean stresses10.1016/j.ijfatigue.2005.06.006 ↗
15. Degradation of microstructural and mechanical properties with serviced turbine blades10.1016/j.matchar.2021.111582 ↗
16. Failure and lesson of turbo rotation blades for aero-engines
17. China Aeronautical Materials Handbook (Vol.2, In Chinese), The Editorial Committee of China Aeronautical Materials Handbook, China Standard Press, Beijing, China, 2002.
18. High temperature VHCF of a 3rd generation Ni-based single crystal superalloy with different casting pore sizes10.1016/j.ijfatigue.2023.107804 ↗
19. Transition from internal to surface crack initiation of a single-crystal superalloy in the very-high-cycle fatigue regime at 1100 degrees C10.1016/j.ijfatigue.2021.106343 ↗
20. On the impact of an integrated HIP treatment on the very high cycle fatigue life of Ni-based SX superalloys
21. Very high cycle fatigue durability of an additively manufactured single-crystal Ni-based superalloy
22. Unveiling the initial oxidation mechanism of a single crystal Ni-based superalloy with pre-deformation10.1016/j.corsci.2024.112146 ↗
23. Diffusion of alloying elements during high temperature oxidation in a low-cost third generation Ni-based single crystal superalloy10.1016/j.matchar.2024.113913 ↗
24. Effect of high temperature oxidation on creep behavior of Ni-based single crystal superalloy10.2139/ssrn.3762202 ↗
25. Long-term oxidation behavior and mechanism of DD6 Ni-based single crystal superalloy at 1050 degrees C and 1100 degrees C in air10.1016/j.jallcom.2017.02.031 ↗
26. The effect of tensile stress on oxidation behavior of nickel-base single crystal superalloy10.1016/j.corsci.2021.109737 ↗
27. Influence of microstructure on the oxidation behaviour of the Ni-based single crystal superalloy AM1 between 850 and 1050°C in air10.1016/j.corsci.2024.111872 ↗
28. Oxidation behavior and mechanism of a Ni-based single crystal superalloy with single alpha-Al2O3 film at 1000 degrees C10.1016/j.apsusc.2017.03.116 ↗
29. Oxidation micromechanics and contribution during the low-cycle fatigue failure of a Ni-based single crystal superalloy10.1016/j.ijfatigue.2024.108586 ↗
30. Anisotropic thermomechanical fatigue of a nickel-base single-crystal superalloy Part I: Effects of crystal orientations and damage mechanisms10.1016/j.ijfatigue.2022.107438 ↗
31. Oxidation-involved life prediction and damage assessment under generalized creep-fatigue loading conditions based on engineering damage mechanics10.1016/j.jmrt.2022.12.094 ↗
32. Elastic strain energy control of the precipitate free zone around primary carbides in nickel base alloy 72510.1016/j.actamat.2016.08.038 ↗
33. Very high cycle fatigue of a notched Ni-based single crystal superalloy at high temperature10.1016/j.ijfatigue.2024.108379 ↗
34. Initiation and early-stage growth of internal fatigue cracking under very-high-cycle fatigue regime at high temperature10.1007/s11661-020-05633-3 ↗
35. Modelling and analysis of the oxidation influence on creep behaviour of thin-walled structures of the single-crystal nickel-base superalloy Rene N5 at 980 degrees C10.1016/j.actamat.2009.11.004 ↗
36. On the development and investigation of quaternary Pt-based superalloys with Ni additions10.1007/s11661-005-0171-7 ↗
37. The influence of γ′-precipitation on the recrystallization of a nickel base superalloy10.1016/0001-6160(80)90039-5 ↗
38. Effect of cyclic oxidation on the tensile behavior of directionally solidified CM-247LC Ni-based superalloy at 870 degrees C10.1016/j.msea.2010.06.046 ↗
39. Effect of heat treatment atmosphere on surface recrystallization of a directionally solidified Ni-base superalloy10.1016/j.scriptamat.2008.06.032 ↗
40. Dynamic recrystallization behavior of a directionally solidified superalloy10.1002/adem.200700096 ↗
41. The influence of stress on the oxidation of a Ni-based superalloy10.1016/j.corsci.2019.04.023 ↗
42. Initial oxidation of Ni-based superalloy and its dynamic microscopic mechanisms: The interface junction initiated outwards oxidation10.1016/j.actamat.2021.116991 ↗
43. Orientation dependence of nickel-based single crystal superalloys in VHCF regime10.1016/j.ijfatigue.2024.108502 ↗
44. Oxidation behaviors and compressive strength evolution of DD6 Ni-based single-crystal superalloy at 1100℃
45. Growth stresses in thermally grown oxides on nickel-based single-crystal alloys10.1007/s11661-015-3273-x ↗
46. Concomitant oxidation-diffusion-creep processes for stress generation and suppression of oxide-alloy interfacial instabilities10.1016/j.jmps.2020.104218 ↗
47. The role of oxidation damage in fatigue crack initiation of an advanced Ni-based superalloy10.1016/j.ijfatigue.2015.08.016 ↗
48. Stress-assisted diffusion to dislocations and its role in strain aging10.1063/1.1709219 ↗
49. Predicting the oxidation kinetic rate and near-surface microstructural evolution of alumina-forming Ni-based single crystal superalloy based on machine learning10.1016/j.actamat.2024.119703 ↗
50. Oxidation ahead of a crack tip in an advanced Ni-based superalloy10.1016/j.actamat.2012.12.017 ↗
51. Ageing kinetics of Ni-base superalloys10.1080/09603409.2016.1176753 ↗
52. Modelling of kinetics of directional coarsening in Ni-superalloys10.1016/1359-6454(95)00349-5 ↗
53. Effects of crystal orientations on the cyclic deformation behavior in the low cycle fatigue of a single crystal nickel-base superalloy10.1016/j.matdes.2017.06.047 ↗
54. High temperature low cycle fatigue behavior of a directionally solidified Ni-base superalloy DZ95110.1016/j.msea.2007.11.045 ↗
55. Oxygen changes crack modes of Ni-based single crystal superalloy10.1080/21663831.2021.1993367 ↗
56. Inhomogeneities in single-crystal components10.1016/0921-5093(93)90185-H ↗
57. M. Mehdizadeh, H. Farhangi Corrigendum to “Effects of different elevated temperature and long-term exposure on microstructural evolution and mechanical characteristics of IN617 Ni-based superalloy” [Mater. Sci. Eng. A 841 (2022) 143025]. Materials Science and Engineering: A 2022;851:143508. https://doi.org/10.1016/j.msea.2022.143508.10.1016/j.msea.2022.143508 ↗
58. Orientation and temperature dependence of some mechanical properties of the single-crystal nickel-base superalloy René N4: Part II
59. Damage mechanisms during very high cycle fatigue of a coated and grit-blasted Ni-based single-crystal superalloy10.1016/j.ijfatigue.2020.105962 ↗
60. Effects of creep and oxidation to thermomechanical fatigue life assessment for nickel-based superalloy10.1016/j.ijfatigue.2023.107873 ↗
61. Transition behavior from Mode I cracking to crystallographic cracking in a Ni-base single crystal superalloy10.1016/j.ijfatigue.2019.105400 ↗