Study on the anisotropic high cycle fatigue performance of L-DEDed Ni-based superalloy: Microstructure, failure mechanism and fatigue limit evaluation
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Temperature Alloys and Creep · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Modeling the effect of temperature on the yield strength of precipitation strengthening Ni-base superalloys10.1016/j.ijplas.2019.01.002 ↗
2. Crystal plasticity analysis of cylindrical indentation on a Ni-base single crystal superalloy10.1016/j.ijplas.2013.05.004 ↗
3. The machinability of inconel 71810.1016/S0924-0136(96)02624-6 ↗
4. Laser-assisted machining of Inconel 718 with an economic analysis10.1016/j.ijmachtools.2005.11.005 ↗
5. Addressing the challenges in remanufacturing by laser-based material deposition techniques10.1016/j.optlastec.2021.107404 ↗
6. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
7. An overview of Direct Laser Deposition for additive manufacturing. Part II: Mechanical behavior, process parameter optimization and control
8. Effects of build orientation and heat treatment on the evolution of microstructure and mechanical properties of alloy Mar-M-509 fabricated via laser powder bed fusion10.1016/j.ijplas.2019.06.002 ↗
9. Variation of hardness, microstructure, and Laves phase distribution in direct laser deposited alloy 718 cuboids10.1016/j.matdes.2017.01.031 ↗
10. A critical review on the microstructure and mechanical properties correlation of additively manufactured nickel-based superalloys10.1016/j.jallcom.2022.164530 ↗
11. Nanoindentation based properties of Inconel 718 at elevated temperatures: A comparison of conventional versus additively manufactured samples10.1016/j.ijplas.2019.04.018 ↗
12. Influence of heat treatments on plastic flow of laser deposited Inconel 718: Testing and microstructural based constitutive modeling10.1016/j.ijplas.2020.102865 ↗
13. Scanning strategy dependent tensile properties of selective laser melted GH416910.1016/j.msea.2020.139616 ↗
14. Microstructure and residual stress of laser rapid formed Inconel 718 nickel-base superalloy10.1016/j.optlastec.2010.06.015 ↗
15. Laser powder deposition10.1016/B978-0-08-096532-1.01005-0 ↗
16. Laser cladding10.2351/1.521888 ↗
17. Microstructural and mechanical anisotropy of selective laser melted IN718 superalloy at room and high temperatures using small punch test10.1016/j.matchar.2020.110200 ↗
18. The effect of energy density on texture and mechanical anisotropy in selective laser melted Inconel 71810.1016/j.matdes.2020.108642 ↗
19. Investigation of HP turbine blade failure in a military turbofan engine10.1515/tjj-2015-0049 ↗
20. L. Gan, H. Huang, S.P. Zhu, Y. Li, Y. Yang, Fatigue reliability analysis of turbine disk alloy using saddlepoint approximation, in: L. Gan, H. Huang, S.P. Zhu, Y. Li, Y. Yang (Eds.), (2013).10.1515/tjj-2013-0020 ↗
21. Notched fatigue testing of Inconel 718 prepared by selective laser melting10.1111/ffe.12880 ↗
22. Effect of anisotropy and texture on the low cycle fatigue behavior of Inconel 718 processed via electron beam melting10.1016/j.ijfatigue.2017.08.021 ↗
23. Fatigue behaviour of direct metal laser sintered Inconel 71810.1504/IJPTECH.2016.080001 ↗
24. Low cycle fatigue behavior of direct metal laser sintered Inconel alloy 71810.1016/j.ijfatigue.2016.08.019 ↗
25. Microstructure, fatigue behavior, and failure mechanisms of direct laser-deposited Inconel 71810.1007/s11837-016-2225-2 ↗
26. On the microstructural and mechanical properties of post-treated additively manufactured Inconel 718 superalloy under quasi-static and cyclic loading10.1016/j.msea.2016.05.089 ↗
27. Long fatigue crack growth in Inconel 718 produced by selective laser melting10.1016/j.ijfatigue.2016.03.012 ↗
28. Effects of building orientation and heat treatment on fatigue behavior of selective laser melted 17-4 PH stainless steel10.1016/j.ijfatigue.2016.03.014 ↗
29. Role of grain structure, grain boundaries, crystallographic texture, precipitates, and porosity on fatigue behavior of Inconel 718 at room and elevated temperatures10.1016/j.matchar.2019.01.028 ↗
30. Alloy 718 at Pratt & Whitney: historical perspective and future
31. Paulonis · 1969
32. Some aspects of the precipitation of metastable intermetallic phases in INCONEL 71810.1007/BF02647549 ↗
33. A comprehensive study of the anisotropic tensile properties of laser additive manufactured Ni-based superalloy after heat treatment10.1016/j.ijplas.2021.103147 ↗
34. Microstructures and mechanical behavior of Inconel 718 fabricated by selective laser melting10.1016/j.actamat.2011.12.032 ↗
35. Effect of heat treatment on the microstructure and mechanical properties of Inconel 718 processed by selective laser melting10.1016/j.msea.2015.05.035 ↗
36. Effect of heat treatment on microstructure evolution of Inconel 718 alloy fabricated by selective laser melting10.1016/j.jallcom.2018.06.112 ↗
37. Kurz · 1998
38. Textures formed in a CoCrMo alloy by selective laser melting10.1016/j.jallcom.2015.01.096 ↗
39. High cycle fatigue and ratcheting interaction of laser powder bed fusion stainless steel 316L: Fracture behaviour and stress-based modelling10.1016/j.ijfatigue.2018.12.016 ↗
40. Epitaxial laser deposition of single crystal Ni-based superalloys: Repair of complex geometry10.1016/j.jmatprotec.2020.116782 ↗
41. Failure of metals II: Fatigue10.1016/j.actamat.2015.05.050 ↗
42. E.A. Loria, M. Minerals, M. Society, A. International, N.A.o.C. Engineers, Superalloy 718: Metallurgy and Applications: Proceedings of the International Symposium on the Metallurgy and Applications of Superalloy 718, Minerals, Metals & Materials Society, 1989.
43. Strengthening mechanisms in Inconel 718 superalloy10.1179/030634583790421032 ↗
44. Low cycle fatigue behavior of inconel 718 at 298 K and 823 K10.1007/BF02667395 ↗
45. Fatigue and fracture behavior of nickel-based superalloy Inconel 718 up to the very high cycle regime10.1631/jzus.A1000171 ↗
46. Subsurface crack initiation during fatigue as a result of residual stresses10.1111/j.1460-2695.1979.tb00388.x ↗
47. Role of retained austenite with different morphologies on sub-surface fatigue crack initiation in advanced bainitic steels10.1016/j.scriptamat.2020.03.036 ↗
48. Fatigue behavior and failure mechanisms of direct laser deposited Ti–6Al–4V10.1016/j.msea.2015.12.026 ↗
49. The influence of Laves phases on the high-cycle fatigue behavior of laser additive manufactured Inconel 71810.1016/j.msea.2017.03.098 ↗
50. The effects of grain size, dendritic structure and crystallographic orientation on fatigue crack propagation in IN713C nickel-based superalloy10.1016/j.ijplas.2019.09.010 ↗
51. T.P. Gabb, J. Telesman, P. Kantzos, P. Bonacuse, R. Barrie, Initial Assessment of the Effects of Nonmetallic Inclusions on Fatigue Life of Powder-Metallurgy-Processed Udimet (TM) 720, in: Advanced Materials and Processes for Gas Turbines Symposium, 2002.
52. The effect of defects on the fatigue crack initiation process in two p/m superalloys: Part I. Fatigue origins10.1007/BF02642413 ↗
53. Fatigue crack growth resistant microstructures in polycrystalline Ni-base superalloys for aeroengines10.1016/S0142-1123(98)00087-5 ↗
54. Modelling the optimum grain size on the low cycle fatigue life of a Ni based superalloy in the presence of two possible crack initiation sites10.1016/j.scriptamat.2003.09.043 ↗
55. Mechanics of fatigue crack propagation by crack-tip plastic blunting10.1016/0013-7944(84)90163-2 ↗
56. Experimental investigation of grain size effect on fatigue crack growth rate in turbine disc superalloy GH4169 under different temperatures10.1016/j.msea.2016.05.063 ↗
57. Small and long fatigue crack growth behaviour of a PM Ni-based superalloy, Udimet 72010.1016/S0142-1123(03)00139-7 ↗
58. Long fatigue crack propagation behavior of Inconel 625 processed by laser powder bed fusion: Influence of build orientation and post-processing conditions10.1016/j.ijfatigue.2018.07.008 ↗
59. The formation of cracks as a result of plastic flow10.1098/rspa.1954.0124 ↗
60. Microstructurally sensitive crack nucleation around inclusions in powder metallurgy nickel-based superalloys10.1016/j.actamat.2016.07.023 ↗
61. Slip and fatigue crack formation processes in an α/β titanium alloy in relation to crystallographic texture on different scales10.1016/j.actamat.2008.04.036 ↗
62. Effect of crystallographic orientation and geometrical compatibility on fatigue crack initiation and propagation in rolled Ti-6Al-4V alloy10.1016/j.actamat.2019.07.025 ↗
63. Small fatigue crack initiation and growth mechanisms of nickel-based superalloy GH4169 at 650°C in air10.1016/j.engfracmech.2015.12.014 ↗
64. Short crack initiation and growth at 600°C in notched specimens of Inconel71810.1016/S0921-5093(02)00169-7 ↗
65. Ravichandran · 1999
66. Roles of microstructure in fatigue crack initiation10.1016/j.ijfatigue.2009.10.005 ↗
67. Effects of defects in laser additive manufactured Ti-6Al-4V on fatigue properties10.1016/j.phpro.2014.08.120 ↗
68. The effect of cooling rate on the solidification of INCONEL 71810.1007/s11663-005-0009-0 ↗
69. Microstructure and tensile properties of Inconel 718 pulsed Nd-YAG laser welds10.1016/j.jmatprotec.2004.09.081 ↗
70. 6 - Effects of nonmetallic inclusions on fatigue strength
71. Murakami · 2002
72. Quantitative evaluation of effects of non-metallic inclusions on fatigue strength of high strength steels. I: Basic fatigue mechanism and evaluation of correlation between the fatigue fracture stress and the size and location of non-metallic inclusions10.1016/0142-1123(89)90054-6 ↗
73. Growth and stability of interacting surface flaws of arbitrary shape10.1016/0013-7944(83)90027-9 ↗
74. Mechanism of cementite decomposition in 100Cr6 bearing steels during high pressure torsion10.1016/j.actamat.2020.09.069 ↗
75. Alloy, Nickel Corrosion and Heat-Resistant, Investment Castings, 52.5 Ni-19Cr-3.0 Mo-5.1 Cb (Nb)-0.90 Ti-0.60 Al-18Fe, Vacuum Melted Homogenization and Solution Heat Treated, in.
76. Physical properties of the NbC Carbide10.3390/met6100250 ↗
77. Electronic, magnetic and mechanical properties of (Fe, Ni)2Nb from density functional theory10.1016/j.jmmm.2017.12.079 ↗
78. A critical of carbide cracking mechanisms in ferride/carbide aggregates10.1016/0001-6160(70)90103-3 ↗
79. Inclusion-induced fatigue crack initiation in powder bed fusion of Alloy 718
80. Effect of a large population of seeded alumina inclusions on crack initiation and small crack fatigue crack growth in Udimet 720 nickel-base disk superalloy10.1016/j.ijfatigue.2020.105953 ↗
81. Competing mechanisms of particle fracture, decohesion and slip-driven fatigue crack nucleation in a PM nickel superalloy10.1016/j.ijfatigue.2020.105573 ↗
82. Cyclic slip irreversibilities and the evolution of fatigue damage10.1007/s11661-009-9839-8 ↗
83. Crystallographic fatigue crack initiation in nickel-based superalloy René 88DT at elevated temperature10.1016/j.actamat.2009.08.022 ↗
84. Crack initiation during high cycle fatigue of an austenitic steel10.1016/0956-7151(90)90305-Z ↗
85. The effects of crystallographic orientation on fatigue crack initiation behavior in Ti-6Al-4V10.1016/j.ijfatigue.2018.07.039 ↗
86. Microstructural mechanisms and advanced characterization of long and small fatigue crack growth in cast A356–T61 aluminum alloys10.1016/j.ijfatigue.2016.12.029 ↗
87. Effects of inclusions, grain boundaries and grain orientations on the fatigue crack initiation and propagation behavior of 2524–T3 Al alloy10.1016/j.msea.2013.05.053 ↗
88. Compatibility of deformation in two-phase Ti-Al alloys: Dependence on microstructure and orientation relationships10.1007/BF02670762 ↗
89. 4.05 - Small Fatigue Cracks
90. Fatigue crack initiation in WASPALOY at 20 °C10.1007/s11661-007-9178-6 ↗
91. Microstructural influences on very-high-cycle fatigue-crack initiation in Ti-624610.1007/s11661-008-9633-z ↗
92. Selective laser melting of a high strength AlMnSc alloy: Alloy design and strengthening mechanisms10.1016/j.actamat.2019.04.014 ↗
93. Anisotropy in fatigue crack propagation behavior of Al-Cu-Li alloy thick plate10.1016/j.matchar.2017.07.025 ↗
94. Influence of grain size on the small fatigue crack initiation and propagation behaviors of a nickel-based superalloy at 650 °C10.1016/j.jmst.2019.03.023 ↗
95. The role of δ phase for fatigue crack propagation behavior in a Ni base superalloy at room temperature10.1016/j.msea.2016.12.029 ↗
96. High cycle fatigue of a die cast AZ91E-T4 magnesium alloy10.1016/j.actamat.2003.11.018 ↗
97. Fatigue strength and fracture mechanics – A general perspective10.1016/j.engfracmech.2017.04.030 ↗
98. Prediction of fatigue crack propagation in friction stir welds
99. Mechanical properties of AlSi10Mg produced by selective laser melting10.1016/j.phpro.2012.10.059 ↗
100. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗