Multiaxial fatigue behavior and modelling of additive manufactured Ti-6Al-4V parts: The effects of layer orientation and surface texture
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (77)
Show source-provided references
1. The role of the national science foundation in the origin and evolution of additive manufacturing in the United States
2. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
3. Additive manufacturing of fatigue resistant materials: challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
4. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
5. A review of the as-built SLM Ti-6Al-4V mechanical properties towards achieving fatigue resistant designs10.3390/met8010075 ↗
6. Effect of build angle on surface properties of nickel superalloys processed by selective laser melting10.1007/s11837-017-2706-y ↗
7. Shrestha · 2016
8. Effects of building orientation and heat treatment on fatigue behavior of selective laser melted 17–4 PH stainless steel10.1016/j.ijfatigue.2016.03.014 ↗
9. Strain energy-based fatigue failure analyses of LB-PBF Inconel 718: effect of build orientation
10. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗
11. Effect of build orientation on the microstructure and mechanical properties of selective laser-melted Ti-6Al-4V Alloy
12. Surface roughness and directional fatigue behavior of as-built EBM and DMLS Ti6Al4V
13. Effect of build orientation on the fatigue properties of as-built Electron Beam Melted Ti-6Al-4V alloy10.1016/j.ijfatigue.2018.08.006 ↗
14. Influence of build direction on the fatigue behaviour of Ti6Al4V alloy produced by direct metal laser sintering10.1016/j.matpr.2016.03.021 ↗
15. Torries · 2017
16. Effects of defects in laser additive manufactured Ti-6Al-4V on fatigue properties10.1016/j.phpro.2014.08.120 ↗
17. Fatigue crack growth mechanisms at the microstructure scale in as-fabricated and heat treated Ti-6Al-4V ELI manufactured by electron beam melting (EBM)10.1016/j.engfracmech.2017.03.024 ↗
18. Significance of hot isostatic pressing (HIP) on multiaxial deformation and fatigue behaviors of additive manufactured Ti-6Al-4V including build orientation and surface roughness effects10.1016/j.ijfatigue.2018.07.035 ↗
19. Effects of layer orientation on the multiaxial fatigue behavior of additively manufactured Ti-6Al-4V
20. Fatigue behaviour of additive manufactured materials: An overview of some recent experimental studies on Ti-6Al-4V considering various processing and loading direction effects10.1111/ffe.13000 ↗
21. Characterization and analysis of surface notches on Ti-alloy plates fabricated by additive manufacturing techniques10.1088/2051-672X/3/4/044006 ↗
22. Application of mechanical surface finishing processes for roughness reduction and fatigue improvement of additively manufactured Ti-6Al-4V parts10.1016/j.ijfatigue.2017.05.008 ↗
23. Analysis of stress intensity factors of modes I, II and III for inclined surface cracks of arbitrary shape10.1016/0013-7944(85)90163-8 ↗
24. Murakami · 2002
25. Orientation-dependent fatigue assessment of Ti6Al4V manufactured by L-PBF: size of surface features and shielding effect10.1016/j.ijfatigue.2022.107401 ↗
26. Predicting the fatigue performance of an additively manufactured Ti-6Al-4V component from witness coupon behavior
27. Multiaxial fatigue behavior of wrought and additive manufactured Ti-6Al-4V including surface finish effect10.1016/j.ijfatigue.2017.03.044 ↗
28. Torsional fatigue behavior of wrought and additive manufactured Ti-6Al-4V by powder bed fusion including surface finish effect10.1016/j.ijfatigue.2017.03.002 ↗
29. Multiaxial fatigue of titanium including step loading and load path alteration and sequence effects10.1016/j.ijfatigue.2010.05.006 ↗
30. Multiaxial fatigue life prediction for titanium alloy TC4 under proportional and nonproportional loading10.1016/j.ijfatigue.2013.08.028 ↗
31. Fatigue crack initiation and growth behavior of Ti–6Al–4V under non-proportional multiaxial loading10.1016/j.ijfatigue.2010.12.013 ↗
32. Multiaxial fatigue: an overview and some approximation models for life estimation10.1016/j.ijfatigue.2011.01.003 ↗
33. Stephens · 2000
34. Fatigue life estimation of additive manufactured parts in the as-built surface condition
35. Fatigue design with additive manufactured metals: issues to consider and perspective for future research10.1016/j.proeng.2018.02.002 ↗
36. ASTM E2207-15 Standard Practice for Strain-Controlled Axial-Torsional Fatigue Testing with Thin-Walled Tubular Specimens, ASTM International, West Conshohocken, PA, 2015.
37. Slicing procedures in layered manufacturing: a review10.1108/13552540310502185 ↗
38. Surface roughness effects on the fatigue strength of additively manufactured Ti-6Al-4V10.1016/j.ijfatigue.2018.07.013 ↗
39. Metal additive manufacturing: a review of mechanical properties10.1146/annurev-matsci-070115-032024 ↗
40. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
41. Powder recycling effects on the tensile and fatigue behavior of additively manufactured Ti-6Al-4V parts10.1007/s11837-018-3248-7 ↗
42. Gas flow effects on selective laser melting (SLM) manufacturing performance10.1016/j.jmatprotec.2011.09.020 ↗
43. Influence of the shielding gas flow on the removal of process by-products in the selective laser melting process
44. An overview of direct laser deposition for additive manufacturing; part II: mechanical behavior, process parameter optimization and control
45. Effect of crystallographic orientation on mechanical anisotropy of selective laser melted Ti-6Al-4V alloy10.1016/j.matchar.2017.01.014 ↗
46. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V10.1016/j.msea.2013.04.099 ↗
47. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
48. Differences in microstructure and properties between selective laser melting and traditional manufacturing for fabrication of metal parts: a review10.1007/s11465-015-0341-2 ↗
49. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
50. Fatigue behavior of Ti-6Al-4V ELI including mean stress effects10.1016/j.ijfatigue.2017.02.013 ↗
51. Texture evolution during laser direct metal deposition of Ti-6Al-4V10.1007/s11837-015-1797-6 ↗
52. ASTM E739-10 Standard Practice for Statistical Analysis of Linear or Linearized Stress-Life (S-N) and Strain-Life (ε-N) Fatigue Data, ASTM International, West Conshohocken, PA, 2015.
53. Effect of process parameters on the surface roughness of overhanging structures in laser powder bed fusion additive manufacturing10.1016/j.procir.2016.02.347 ↗
54. A comparison of fatigue strength sensitivity to defects for materials manufactured by AM or traditional processes10.1016/j.ijfatigue.2016.06.020 ↗
55. Fatigue properties of AlSi10Mg obtained by additive manufacturing: defect-based modelling and prediction of fatigue strength10.1016/j.engfracmech.2017.11.002 ↗
56. Killer notches: the effect of as-built surface roughness on fatigue failure in AlSi10Mg produced by laser powder bed fusion
57. High cycle fatigue behavior and life prediction for additively manufactured 17–4 PH stainless steel: effect of sub-surface porosity and surface roughness10.1016/j.tafmec.2020.102477 ↗
58. Effect of surface roughness on fatigue performance of additive manufactured Ti–6Al–4V10.1179/1743284715Y.0000000053 ↗
59. Fatigue performance of additive manufactured TiAl6V4 using electron and laser beam melting10.1016/j.ijfatigue.2016.05.001 ↗
60. Surface roughness effect on multiaxial fatigue behavior of additive manufactured metals and its modeling10.1016/j.tafmec.2019.102260 ↗
61. Southwest Research Institute. NASGRO Fracture Mechanics and Fatigue Crack Growth Software V9.2 2020.
62. A crack opening stress equation for fatigue crack growth10.1007/BF00020751 ↗
63. Notch fatigue and crack growth resistance of Ti-6Al-4V ELI additively manufactured via selective laser melting: a critical distance approach to defect sensitivity10.1016/j.ijfatigue.2018.12.020 ↗
64. Wycisk E, Emmelmann C, Siddique S, Walther F. High cycle fatigue (HCF) performance of Ti-6Al-4V alloy processed by selective laser melting. Adv. Mater. Res., vol. 816, Trans Tech Publ; 2013, p. 134–9.10.4028/www.scientific.net/AMR.816-817.134 ↗
65. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
66. Fatigue failure mechanisms for AlSi10Mg manufactured by L-PBF under axial and torsional loads: the role of defects and residual stresses10.1016/j.ijfatigue.2022.106903 ↗
67. SIF and threshold for small cracks at small notches under torsion10.1046/j.1460-2695.2000.00260.x ↗
68. Multiaxial fatigue limit for defective materials: mechanisms and experiments10.1016/j.actamat.2004.05.006 ↗
69. Small fatigue crack growth under multiaxial stresses10.1016/j.ijfatigue.2013.02.002 ↗
70. A critical plane approach to multiaxial fatigue damage including out-of-phase loading10.1111/j.1460-2695.1988.tb01169.x ↗
71. Fatigue performance and life prediction of cast aluminum under axial, torsion, and multiaxial loadings10.1016/j.tafmec.2020.102842 ↗
72. Prediction of non propagating cracks10.1016/0013-7944(79)90081-X ↗
73. Analysis of fatigue strength of L-PBF AlSi10Mg with different surface post-processes: effect of residual stresses10.3390/met12060898 ↗
74. A benchmark activity on the fatigue life assessment of AlSi10Mg components manufactured by L-PBF10.1016/j.matdes.2022.110713 ↗
75. An empirical stress-intensity factor equation for the surface crack10.1016/0013-7944(81)90116-8 ↗
76. McClung RC, Enright MP, Lee Y-D, Huyse LJ, Fitch SHK. Efficient Fracture Design for Complex Turbine Engine Components. GT2004, Volume 6: Turbo Expo 2004: 2004, p. 291–300. 10.1115/GT2004-53323.10.1115/GT2004-53323 ↗
77. Analysis of prospective SIF and shielding effect for cylindrical rough surfaces obtained by L-PBF10.1016/j.engfracmech.2021.107983 ↗