journal article·2022-09Open access

Effect of heat treatment temperature and turning residual stresses on the plain and notch fatigue strength of Ti-6Al-4V additively manufactured via laser powder bed fusion

L. Emanuelli, A. Molinari, L. Facchini, E. Sbettega, S. Carmignato, M. Bandini, M. Benedetti

Abstract

This paper investigates the fatigue strength of plain and notched specimens produced via laser powder bed fusion and heat-treated at different temperatures ranging between 800 °C and 950 °C. The effects of internal defectiveness and turning residual stresses are explored through computed tomography and X-ray diffraction. Residual stresses are eliminated in part of the experimental batches through a stress relief. The surface compressive residual stresses push the fatigue crack initiation site below the outer surface and increase the fatigue strength of the notched specimens. The heat-treatment temperature affects mostly the total elongation and the energy consumption, whereas its influence on the fatigue strength is less evident.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. An overview on the use of titanium in the aerospace industry10.1016/0921-5093(96)10233-1 ↗
2. Alpha + Beta Alloys
3. Influence of sharp microstructural gradients on the fatigue crack growth resistance of α + β and near-α titanium alloys10.1111/j.1460-2695.2005.00932.x ↗
4. Metal additive manufacturing: a review of mechanical properties10.1146/annurev-matsci-070115-032024 ↗
5. Properties and applications of additively manufactured metallic cellular materials: A review10.1016/j.pmatsci.2021.100918 ↗
6. Microstructure and mechanical properties of titanium alloys
7. Role of molten pool mode on formability, microstructure and mechanical properties of selective laser melted Ti-6Al-4V alloy10.1016/j.matdes.2016.08.036 ↗
8. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
9. Additive manufacturing of Ti6Al4V alloy: A review10.1016/j.matdes.2018.107552 ↗
10. American Society for Testing Materials. ASTM F2924-14. Standard specification for additive manufacturing titanium-6 aluminum-4 vanadium ELI with powder bed fusion, West Conshohocken, PA, USA; 2014.
11. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
12. Ductility improvement due to martensite α′ decomposition in porous Ti–6Al–4V parts produced by selective laser melting for orthopedic implants10.1016/j.jmbbm.2015.09.020 ↗
13. Microstructural evolution and microhardness of a selective-laser-melted Ti–6Al–4V alloy after post heat treatments10.1016/j.jallcom.2016.02.183 ↗
14. Critical assessment of the fatigue performance of additively manufactured Ti–6Al–4V and perspective for future research10.1016/j.ijfatigue.2015.12.003 ↗
15. Influence of defects, surface roughness and HIP on the fatigue strength of Ti-6Al-4V manufactured by additive manufacturing10.1016/j.ijfatigue.2018.07.020 ↗
16. Anisotropic high cycle fatigue behavior of Ti–6Al–4V obtained by powder bed laser fusion10.1016/j.ijfatigue.2016.04.032 ↗
17. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
18. High Cycle Fatigue (HCF) Performance of Ti-6Al-4V Alloy Processed by Selective Laser Melting10.4028/www.scientific.net/AMR.816-817.134 ↗
19. Multiaxial fatigue behavior of wrought and additive manufactured Ti-6Al-4V including surface finish effect10.1016/j.ijfatigue.2017.03.044 ↗
20. Application of mechanical surface finishing processes for roughness reduction and fatigue improvement of additively manufactured Ti-6Al-4V parts10.1016/j.ijfatigue.2017.05.008 ↗
21. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: Fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
22. Evaluation of fatigue crack propagation behaviour in Ti-6Al-4V manufactured by selective laser melting10.1016/j.ijfatigue.2017.07.014 ↗
23. A comparison of fatigue strength sensitivity to defects for materials manufactured by AM or traditional processes10.1016/j.ijfatigue.2016.06.020 ↗
24. Effects of Defects in Laser Additive Manufactured Ti-6Al-4V on Fatigue Properties10.1016/j.phpro.2014.08.120 ↗
25. Defect analysis and fatigue design basis for Ni-based superalloy 718 manufactured by selective laser melting10.1016/j.ijfatigue.2018.08.002 ↗
26. Low- and high-cycle fatigue resistance of Ti-6Al-4V ELI additively manufactured via selective laser melting: Mean stress and defect sensitivity10.1016/j.ijfatigue.2017.10.021 ↗
27. Fatigue life of additively manufactured Ti–6Al–4V in the very high cycle fatigue regime10.1016/j.ijfatigue.2016.05.018 ↗
28. Significance of hot isostatic pressing (HIP) on multiaxial deformation and fatigue behaviors of additive manufactured Ti-6Al-4V including build orientation and surface roughness effects10.1016/j.ijfatigue.2018.07.035 ↗
29. The effect of post-sintering treatments on the fatigue and biological behavior of Ti-6Al-4V ELI parts made by selective laser melting10.1016/j.jmbbm.2017.03.024 ↗
30. Fatigue Assessment of Ti–6Al–4V Circular Notched Specimens Produced by Selective Laser Melting10.3390/met7080291 ↗
31. Fatigue strength of blunt V-notched specimens produced by selective laser melting of Ti-6Al-4V10.1016/j.tafmec.2017.06.021 ↗
32. Notch fatigue and crack growth resistance of Ti-6Al-4V ELI additively manufactured via selective laser melting: A critical distance approach to defect sensitivity10.1016/j.ijfatigue.2018.12.020 ↗
33. Fatigue behaviour of notched additive manufactured Ti6Al4V with as-built surfaces10.1016/j.ijfatigue.2017.04.009 ↗
34. Experimental determination and sensitivity analysis of the fatigue critical distance obtained with rounded V-notched specimens10.1016/j.ijfatigue.2018.03.037 ↗
35. Determination of the fatigue critical distance according to the Line and the Point Methods with rounded V-notched specimen10.1016/j.ijfatigue.2017.10.002 ↗
36. A profile refinement method for nuclear and magnetic structures10.1107/S0021889869006558 ↗
37. Traceable Porosity Measurements in Industrial Components Using X-Ray Computed Tomography10.1115/1.4043192 ↗
38. Reference object for evaluating the accuracy of porosity measurements by X-ray computed tomography10.1016/j.csndt.2016.05.003 ↗
39. Residual stresses reconstruction in shot peened specimens containing sharp and blunt notches by experimental measurements and finite element analysis10.1016/j.ijfatigue.2016.01.020 ↗
40. Murakami · 2002
41. Statistical analysis of defects for fatigue strength prediction and quality control of materials10.1046/j.1460-2695.1998.00104.x ↗
42. High- and very high-cycle plain fatigue resistance of shot peened high-strength aluminum alloys: The role of surface morphology10.1016/j.ijfatigue.2014.07.002 ↗
43. Non-destructive observation of internal fatigue crack growth in Ti–6Al–4V by using synchrotron radiation μCT imaging10.1016/j.ijfatigue.2016.05.028 ↗
44. Taylor · 2007
45. Characterization of microshrinkage casting defects of Al–Si alloys by X-ray computed tomography and metallography10.1016/j.ijfatigue.2012.01.006 ↗
46. Statistical properties of threshold and notch derived estimations of the critical distance according to the line method of the theory of critical distances10.1016/j.ijfatigue.2020.105656 ↗