Crack initiation behavior and fatigue performance up to very-high-cycle regime of AlSi10Mg fabricated by selective laser melting with two powder sizes

Z.M. Jian, G.A. Qian, D.S. Paolino, A. Tridello, F. Berto, Y.S. Hong

Abstract

Abstract The high-cycle and very-high-cycle fatigue (VHCF) behavior of AlSi10Mg specimens manufactured by selective laser melting with different printing powder sizes was investigated. The specimens with 20 μm powder size contained more defects than those with 50 μm powder size, and the latter have a higher fatigue property than the former. Unmelted powders were detected as the main source of crack initiation. The specimens printed with 50 μm powder size are more likely to feature subsurface crack initiation in the VHCF regime. Five different types of crack initiation modes were identified, and the fatigue strength was assessed by statistical model.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (59)

Show source-provided references
1. In-situ SEM investigation on fatigue behaviors of additive manufactured Al-Si10-Mg alloy at elevated temperature10.1016/j.engfracmech.2019.03.040 ↗
2. Additive manufacturing of fatigue resistant materials: Challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
3. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
4. Additive Manufacturing of Metallic Materials: A Review10.1007/s11665-017-2747-y ↗
5. Additive manufacturing of metals: a brief review of the characteristic microstructures and properties of steels, Ti-6Al-4V and high-entropy alloys10.1080/14686996.2017.1361305 ↗
6. 3D printing of high-strength aluminium alloys10.1038/nature23894 ↗
7. Selective laser melting of AlSi10Mg: Influence of post-processing on the microstructural and tensile properties development10.1016/j.matdes.2016.05.066 ↗
8. Fatigue life of additively manufactured Ti–6Al–4V in the very high cycle fatigue regime10.1016/j.ijfatigue.2016.05.018 ↗
9. VHCF response of as-built SLM AlSi10Mg specimens with large loaded volume10.1111/ffe.12830 ↗
10. Influence of the annealing and defects on the VHCF behavior of an SLM AlSi10Mg alloy10.1111/ffe.13123 ↗
11. A review about the effects of structural and operational factors on the gigacycle fatigue of steels10.1111/ffe.12779 ↗
12. Fatigue behavior of carburized steel with internal oxides and nonmartensitic microstructure near the surface10.1007/BF02648572 ↗
13. Stepwise S-N curve and fish-eye failure in gigacycle fatigue10.1046/j.1460-2695.1999.00206.x ↗
14. Cyclic plasticity at pores and inclusions in cast Al–Si alloys10.1016/S0013-7944(02)00097-8 ↗
15. Propensities of crack interior initiation and early growth for very-high-cycle fatigue of high strength steels10.1016/j.ijfatigue.2013.02.023 ↗
16. Application of mechanical surface finishing processes for roughness reduction and fatigue improvement of additively manufactured Ti-6Al-4V parts10.1016/j.ijfatigue.2017.05.008 ↗
17. The formation mechanism of characteristic region at crack initiation for very-high-cycle fatigue of high-strength steels10.1016/j.ijfatigue.2015.11.029 ↗
18. A physically based universal functional to characterize the mechanism of fatigue crack growth in materials10.1016/j.scriptamat.2015.05.035 ↗
19. On the mechanism of fatigue failure in the superlong life regime (N>107 cycles). Part I: influence of hydrogen trapped by inclusions10.1046/j.1460-2695.2000.00328.x ↗
20. A comparison of fatigue strength sensitivity to defects for materials manufactured by AM or traditional processes10.1016/j.ijfatigue.2016.06.020 ↗
21. Prediction of threshold value for FGA formation10.1016/j.msea.2011.05.070 ↗
22. High-cycle and very-high-cycle fatigue behaviour of a titanium alloy with equiaxed microstructure under different mean stresses10.1111/ffe.13050 ↗
23. Experimental and theoretical investigation of environmental media on very-high-cycle fatigue behavior for a structural steel10.1016/j.actamat.2010.10.064 ↗
24. Very-high-cycle fatigue behavior of Ti-6Al-4V manufactured by selective laser melting: Effect of build orientation
25. Very-high-cycle fatigue behavior of AlSi10Mg manufactured by selective laser melting: Effect of build orientation and mean stress10.1016/j.ijfatigue.2020.105696 ↗
26. Influence of working environment and built orientation on the tensile properties of selective laser melted AlSi10Mg alloy10.1016/j.msea.2019.01.103 ↗
27. On the effect of shot-peening on fatigue resistance of AlSi10Mg specimens fabricated by additive manufacturing using selective laser melting (AMSLM)10.1016/j.addma.2018.03.030 ↗
28. Reducing porosity in AlSi10Mg parts processed by selective laser melting10.1016/j.addma.2014.08.001 ↗
29. Effects of hot isostatic pressing and internal porosity on the performance of selective laser melted AlSi10Mg alloys10.1016/j.msea.2019.138713 ↗
30. Influence of defect size on the fatigue resistance of AlSi10Mg alloy elaborated by selective laser melting (SLM)
31. High-temperature mechanical properties of AlSi10Mg specimens fabricated by additive manufacturing using selective laser melting technologies (AMSLM)10.1016/j.addma.2018.09.033 ↗
32. Strain rate sensitivity and fracture mechanism of AlSi10Mg parts produced by Selective Laser Melting10.1016/j.msea.2016.11.070 ↗
33. Selective laser melting of AlSi10Mg alloy: Process optimisation and mechanical properties development10.1016/j.matdes.2014.09.044 ↗
34. Numerical modelling of surface roughness effect on the fatigue behavior of Ti-6Al-4V obtained by additive manufacturing10.1016/j.ijfatigue.2019.02.014 ↗
35. Comparative study of fatigue properties of Ti-6Al-4V specimens built by electron beam melting (EBM) and selective laser melting (SLM)10.1016/j.matchar.2018.03.028 ↗
36. Effects of thickness and orientation on the small scale fracture behaviour of additively manufactured Ti-6Al-4V10.1016/j.matchar.2018.04.003 ↗
37. Fatigue properties and material characteristics of additively manufactured AlSi10Mg-Effect of the contour parameter on the microstructure, density, residual stress, roughness and mechanical properties10.1016/j.ijfatigue.2018.08.023 ↗
38. Effect of heat treatment and laser surface remelting on AlSi10Mg alloy fabricated by selective laser melting10.1007/s00170-018-03272-y ↗
39. In situ X-ray imaging of defect and molten pool dynamics in laser additive manufacturing10.1038/s41467-018-03734-7 ↗
40. Role of melt pool boundary condition in determining the mechanical properties of selective laser melting AlSi10Mg alloy10.1016/j.msea.2018.10.083 ↗
41. A unified statistical model for S-N fatigue curves: probabilistic definition10.1111/j.1460-2695.2012.01711.x ↗
42. Fine-structured aluminum products with controllable texture by selective laser melting of pre-alloyed AlSi10Mg powder10.1016/j.actamat.2012.11.052 ↗
43. Notched fatigue testing of Inconel 718 prepared by selective laser melting10.1111/ffe.12880 ↗
44. LCF behaviour and a comprehensive life prediction model for AlSi10Mg obtained by SLM10.1016/j.ijfatigue.2018.07.030 ↗
45. A novel hybrid selective laser melting/hot isostatic pressing of near-net shaped Ti-6Al-4V alloy using an in-situ tooling: Interfacial microstructure evolution and enhanced mechanical properties10.1016/j.msea.2018.01.079 ↗
46. In-situ investigation on fatigue behaviors of Ti-6Al-4V manufactured by selective laser melting10.1016/j.ijfatigue.2019.105424 ↗
47. In-situ investigation of the anisotropic mechanical properties of laser direct metal deposition Ti6Al4V alloy10.1016/j.msea.2017.11.106 ↗
48. Evaluation of fatigue crack propagation behaviour in Ti-6Al-4V manufactured by selective laser melting10.1016/j.ijfatigue.2017.07.014 ↗
49. Killer notches: The effect of as-built surface roughness on fatigue failure in AlSi10Mg produced by laser powder bed fusion10.1016/j.addma.2020.101424 ↗
50. Improving the fatigue behaviour of a selectively laser melted aluminum alloy: Influence of heat treatment and surface quality10.1016/j.matdes.2016.05.041 ↗
51. Formation and reduction of hydrogen porosity during selective laser melting of AlSi10Mg10.1016/j.jmatprotec.2015.02.013 ↗
52. In situ detection of thermally induced porosity in additively manufactured and sintered objects10.1007/s10853-019-03452-5 ↗
53. Design of dog-bone-shaped ultrasonic vibrational fatigue specimen and its application in study on VHCF behavior of 6063 aluminium alloy
54. The effect of manufacturing defects on the fatigue life of selective laser melted Ti-6Al-4V structures10.1016/j.matdes.2020.108708 ↗
55. Murakami · 1993
56. Material defects as the basis of fatigue design10.1016/j.ijfatigue.2011.12.001 ↗
57. Statistical estimation of duplex S-N curves10.4028/www.scientific.net/KEM.664.285 ↗
58. S-N curves in the very-high-cycle fatigue regime: statistical modeling based on the hydrogen embrittlement consideration10.1111/ffe.12431 ↗
59. A stress-strain function for the fatigue of metals