Microstructure and fatigue crack growth behavior of Inconel 718 superalloy manufactured by laser directed energy deposition
Source abstract
Abstract
Abstract In this study, Inconel 718 (IN718) specimens, manufactured by laser directed energy deposition (LDED), are subjected to three different heat-treatments to have different microstructural characteristics. Fatigue crack growth (FCG) testing is performed on both as-deposited and heat-treated specimens. The coarse Laves phases with uneven γ′′/γ′ precipitates severely decrease FCG resistance of LDED IN718. The soft precipitate-free zone around short-acicular δ-phase partly reduces FCG resistance of LDED IN718. The FCG threshold ( Δ K th ) of a judicious heat-treatment specimen increases by ~ 2.6 times vs. as-deposited specimen and reaches 10.8 MPa∙m1/2, and its Δ K th and FCG curve are comparable to those of wrought IN718.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Temperature Alloys and Creep · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Alloy design for aircraft engines10.1038/nmat4709 ↗
2. Gibson · 2010
3. Lippold · 2011
4. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
5. Review on powder-bed laser additive manufacturing of Inconel 718 parts10.1177/0954405415619883 ↗
6. Additive manufacturing of fatigue resistant materials: Challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
7. Yadollahi A, et al. Fatigue behavior and failure analysis of additive manufactured inconel 718 superalloy. Mater Sci Eng A 2016 [submitted for publication].
8. The role of defects and critical pore size analysis in the fatigue response of additively manufactured IN718 via crystal plasticity10.1016/j.matdes.2018.04.022 ↗
9. Competing crack initiation behaviors of a laser additively manufactured nickel-based superalloy in high and very high cycle fatigue regimes10.1016/j.ijfatigue.2020.105580 ↗
10. Kevinsanny, et al. Defect tolerance and hydrogen susceptibility of the fatigue limit of an additively manufactured Ni-based superalloy 718. Int J Fatigue 2020;139: 105740.10.1016/j.ijfatigue.2020.105740 ↗
11. Hot isostatic pressing of IN718 components manufactured by selective laser melting
12. Residual stress via the contour method in compact tension specimens produced via selective laser melting10.1016/j.scriptamat.2014.05.016 ↗
13. The influence of laves phases on the high-cycle fatigue behavior of laser additive manufactured inconel 71810.1016/j.msea.2017.03.098 ↗
14. Microstructural influence on fatigue crack propagation during high cycle fatigue testing of additively manufactured Alloy 71810.1016/j.matchar.2019.01.018 ↗
15. Mitigation of Anisotropic Fatigue in Nickel Alloy 718 Manufactured via Selective Laser Melting10.1016/j.matdes.2019.108095 ↗
16. Low cycle fatigue behavior of direct metal laser sintered Inconel alloy 71810.1016/j.ijfatigue.2016.08.019 ↗
17. Long fatigue crack propagation behavior of Inconel 625 processed by laser powder bed fusion: Influence of build orientation and post-processing conditions10.1016/j.ijfatigue.2018.07.008 ↗
18. Long fatigue crack growth in Inconel 718 produced by selective laser melting10.1016/j.ijfatigue.2016.03.012 ↗
19. Microstructure and deformation behavior of Ti-6Al-4V alloy by high-power laser solid forming10.1016/j.actamat.2017.04.026 ↗
20. In situ tailoring microstructure in laser solid formed titanium alloy for superior fatigue crack growth resistance10.1016/j.scriptamat.2019.08.028 ↗
21. Effect of hot extrusion and T6 heat treatment on microstructure and mechanical properties of Al-10Zn-3.5Mg-2.5Cu nanocomposite reinforced with graphene nanoplatelets10.1016/j.jmapro.2018.10.026 ↗
22. Effects of pre-deformation on microstructure and tensile properties of Al–Zn–Mg–Cu alloy produced by modified strain induced melt activation10.1016/S1003-6326(16)64349-2 ↗
23. Correlating the microstructure to mechanical properties and wear behavior of an accumulative back extruded Al-Mg2Si in-situ composite10.1016/j.triboint.2017.05.034 ↗
24. Effect of multi-pass friction stir processing on the microstructure, mechanical and wear properties of AA5083/ZrO2 nanocomposites10.1016/j.jallcom.2017.08.084 ↗
25. Effect of temperature on microstructural evolution and subsequent enhancement of mechanical properties in a backward extruded magnesium alloy10.1007/s00170-017-1343-5 ↗
26. Microstructure and mechanical properties of wire and arc additive manufactured AZ31 magnesium alloy using cold metal transfer process10.1016/j.msea.2020.138942 ↗
27. Influence of post-heat-treatment on the microstructure and fracture toughness properties of Inconel 718 fabricated with laser directed energy deposition additive manufacturing10.1016/j.msea.2020.140092 ↗
28. Control of microstructure and mechanical properties of laser solid formed Inconel 718 superalloy by electromagnetic stirring10.1016/j.optlastec.2017.09.022 ↗
29. Evolution of interface and crystal orientation of laser solid formed GH4169 superalloy during recrystallization
30. Effect of heat treatment on the microstructure and mechanical properties of Inconel 718 processed by selective laser melting10.1016/j.msea.2015.05.035 ↗
31. Studies of standard heat treatment effects on microstructure and mechanical properties of laser net shape manufactured Inconel 71810.1007/s11661-009-9949-3 ↗
32. Precipitation of the δ-Ni3Nb phase in two nickel base superalloys10.1007/BF02649259 ↗
33. Electron microscopy study of direct laser deposited IN71810.1016/j.matchar.2015.06.017 ↗
34. Gamma-gamma prime-gamma double prime dual-superlattice superalloys10.1016/j.scriptamat.2017.04.029 ↗
35. Fatigue behaviour of two nickel-base alloys I: experimental results on low cycle fatigue, fatigue crack propagation and substructures10.1016/0025-5416(82)90129-X ↗
36. Effects of compressive residual stress on short fatigue crack growth in a nickel-based superalloy10.1016/j.ijfatigue.2017.11.010 ↗
37. Micromechanisms of fatigue crack growth in a forged Inconel 718 nickel-based superalloy10.1016/S0921-5093(99)00214-2 ↗
38. Fatigue crack growth in polycrystalline IN718 superalloy10.1016/S0921-5093(03)00156-4 ↗
39. Effect of oxidation kinetics on the near threshold fatigue crack growth behavior of a nickel base superalloy10.1007/BF02666360 ↗
40. The influence of Laves phases on the room temperature tensile properties of Inconel 718 fabricated by powder feeding laser additive manufacturing10.1016/j.actamat.2018.10.032 ↗
41. The role of δ phase for fatigue crack propagation behavior in a Ni base superalloy at room temperature10.1016/j.msea.2016.12.029 ↗
42. Effect of boron on fatigue crack growth behavior in superalloy IN 718 at RT and 650 °C10.1016/j.msea.2005.08.206 ↗
43. Influence of grain structure and crystallographic orientation on fatigue crack propagation behavior of 7050 alloy thick plate10.1016/j.ijfatigue.2014.03.009 ↗
44. Crystallographic fatigue crack initiation in nickel-based superalloy René 88DT at elevated temperature10.1016/j.actamat.2009.08.022 ↗
45. A combined grain scale elastic–plastic criterion for identification of fatigue crack initiation sites in a twin containing polycrystalline nickel-base superalloy10.1016/j.actamat.2015.09.050 ↗
46. Modeling crack nucleation at coherent twin boundaries in nickel-based superalloys
47. Fatigue crack initiation, slip localization and twin boundaries in a nickel-based superalloy10.1016/j.cossms.2014.06.001 ↗
48. Microstructural modeling of metadynamic recrystallization in hot working of IN 718 superalloy10.1016/S0921-5093(00)01053-4 ↗
49. Experimental investigation of grain size effect on fatigue crack growth rate in turbine disc superalloy GH4169 under different temperatures10.1016/j.msea.2016.05.063 ↗
50. Elastic-plastic stress field in cracked bodies, Fracture Mechanics: an Introduction
51. Fatigue crack closure under cyclic tension10.1016/0013-7944(70)90028-7 ↗
52. Kanninen · 1985
53. Heat treatment-modulated coupling effect of multi-scale second-phase particles on the ductile fracture of aged aluminum alloys10.1016/j.actamat.2006.08.026 ↗
54. Modeling the age-hardening behavior of SiC/Al metal matrix composites10.1007/s11661-006-9064-7 ↗
55. A micromorphic model for the multiple scale failure of heterogeneous materials10.1016/j.jmps.2007.09.008 ↗
56. On the mechanism of 332 twinning in metastable β titanium alloys10.1016/j.actamat.2016.03.040 ↗
57. Twinning-induced plasticity (TWIP) steels10.1016/j.actamat.2017.06.046 ↗
58. Effect of microstructure on high-cycle fatigue properties of alloy 718 plates10.1088/1757-899X/102/1/012001 ↗
59. Modelling the optimum grain size on the low cycle fatigue life of a Ni based superalloy in the presence of two possible crack initiation sites10.1016/j.scriptamat.2003.09.043 ↗