Abstract

Abstract Multiaxial cyclic tests were performed on wrought AZ31B magnesium extrusion. Axial, torsional and multiaxial cyclic behaviours of the material are presented. Effects of phase angle on stress–strain response, cyclic hardening and fatigue life are discussed. It was found that the material exhibits additional cyclic hardening due to non-proportional loading. However, the phase angle has no pronounced effect on fatigue life. Fatigue cracking behaviour was examined and two characteristics of crack geometry, i.e., size and orientation, are presented. Multiaxial fatigue lives using the Fatemi–Socie and the Smith–Watson–Topper models were predicted. In addition, the Jahed–Varvani energy model was used for fatigue life prediction and was shown to have a potential to be evaluated at plane of maximum axial strain energy density. Reverse analysis for predicting fatigue life by pre-defined critical plane as the observed plane is discussed in details.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (89)

Show source-provided references
1. Magnesium: current and potential automotive applications10.1007/BF02701073 ↗
2. Magnesium and its alloys applications in automotive industry10.1007/s00170-007-1279-2 ↗
3. Automotive applications of magnesium and its alloys
4. Research for a new age of magnesium in the automotive industry10.1016/S0924-0136(01)00780-4 ↗
5. Cyclic axial and cyclic torsional behaviour of extruded AZ31B magnesium alloy10.1016/j.ijfatigue.2011.04.012 ↗
6. The effects of texture and extension twinning on the low-cycle fatigue behavior of a rolled magnesium alloy, AZ31B10.1016/j.msea.2010.07.047 ↗
7. Role of initial 10–12 twin in the fatigue behavior of rolled Mg–3Al–1Zn alloy10.1016/j.scriptamat.2010.01.021 ↗
8. Fatigue design with cast magnesium alloys under constant and variable amplitude loading10.1016/j.ijfatigue.2005.06.043 ↗
9. Microstructure and damage evolution during tensile loading in a wrought magnesium alloy10.1016/j.scriptamat.2011.01.029 ↗
10. Effect of twinning, slip, and inclusions on the fatigue anisotropy of extrusion-textured AZ61 magnesium alloy10.1016/j.msea.2011.05.047 ↗
11. Lee, low-cycle fatigue characteristics of rolled Mg–3Al–1Zn alloy10.1016/j.ijfatigue.2010.05.002 ↗
12. Renner F, Zenner H. Standard practice for strain-controlled axial–torsional fatigue testing with thin-walled tubular specimens fatigue strength of die-cast magnesium components, In: Annual book of {ASTM} standards, ASTM, West Conshohocken, PA %L Renner_Zenner_2002, 2002. p. 1157–68 %L Shih_etal_2002.10.1046/j.1460-2695.2002.00607.x ↗
13. Cyclic material behaviour of magnesium die castings and extrusions10.1016/S0142-1123(02)00042-7 ↗
14. Effect of anisotropy on the low-cycle fatigue behavior of rolled AZ31 magnesium alloy10.1016/j.msea.2009.08.044 ↗
15. Evaluation of low cycle fatigue life in AZ31 magnesium alloy10.1016/j.ijfatigue.2006.12.003 ↗
16. Low-cycle fatigue behavior of an as-extruded AM50 magnesium alloy10.1007/s11661-007-9181-y ↗
17. Low cycle fatigue properties of an extruded AZ31 magnesium alloy10.1016/j.ijfatigue.2008.03.009 ↗
18. Roles of deformation twinning and dislocation slip in the fatigue failure mechanism of AZ31 Mg alloys10.1016/j.scriptamat.2010.03.021 ↗
19. Plastic anisotropy and the role of non-basal slip in magnesium alloy AZ31B10.1016/j.ijplas.2004.05.018 ↗
20. Geometrical criterion for the activation of prismatic slip in AZ61 Mg alloy sheets deformed at room temperature10.1016/j.actamat.2005.01.008 ↗
21. Hardening evolution of AZ31B Mg sheet10.1016/j.ijplas.2006.03.005 ↗
22. Twinning and the ductility of magnesium alloys Part II. “Contraction” twins10.1016/j.msea.2007.02.109 ↗
23. Twinning and the ductility of magnesium alloys Part I: “Tension” twins10.1016/j.msea.2006.12.037 ↗
24. The activity of non-basal slip systems and dynamic recovery at room temperature in fine-grained AZ31B magnesium alloys10.1016/S1359-6454(03)00005-3 ↗
25. An experimental study of cyclic deformation of extruded AZ61A magnesium alloy
26. Multiaxial fatigue of extruded AZ61A magnesium alloy10.1016/j.ijfatigue.2010.09.020 ↗
27. A fatigue criterion for general multiaxial loading10.1046/j.1460-2695.2000.00247.x ↗
28. Multiaxial fatigue damage models10.1115/1.3225980 ↗
29. A stress–strain function for the fatigue of metals
30. Jiang · 1992
31. A critical plane approach to multiaxial fatigue damage including out-of-phase loading10.1111/j.1460-2695.1988.tb01169.x ↗
32. Cyclic behaviour of wrought magnesium alloy under multiaxial load10.1016/j.ijfatigue.2011.01.009 ↗
33. Multiaxial fatigue of extruded AZ31B magnesium alloy10.1016/j.msea.2012.03.039 ↗
34. Multiaxial fatigue: an overview and some approximation models for life estimation10.1016/j.ijfatigue.2011.01.003 ↗
35. Critical plane approaches for multiaxial fatigue damage assessment
36. A model for calculating geometry factors for a mixed-mode I–II single edge notched tension specimen10.1016/j.engfracmech.2011.09.005 ↗
37. Analysis of mixed mode crack initiation angles under various loading conditions10.1016/S0013-7944(00)00068-0 ↗
38. A new criterion for mixed mode fracture initiation based on the crack tip plastic core region10.1016/S0749-6419(03)00011-1 ↗
39. Experimental and numerical determination of mixed mode crack extension angle10.1520/JTE101668 ↗
40. A proposed maximum ratio criterion applied to mixed mode fatigue crack propagation10.1016/j.matdes.2010.11.053 ↗
41. Calculating crack initiation directions for in-phase biaxial fatigue loading10.1016/j.ijfatigue.2013.03.011 ↗
42. Microstructure-based fatigue modeling of cast A356-T6 alloy10.1016/S0013-7944(02)00021-8 ↗
43. Micromechanisms of multistage fatigue crack growth in a high-strength aluminum alloy10.1016/j.actamat.2006.11.009 ↗
45. Evaluation and comparison of several multiaxial fatigue criteria10.1016/S0142-1123(03)00110-5 ↗
46. The use of multiaxial fatigue models to predict fretting fatigue life of components subjected to different contact stress fields10.1111/j.1460-2695.2004.00820.x ↗
47. An experimental evaluation of three critical plane multiaxial fatigue criteria10.1016/j.ijfatigue.2006.10.028 ↗
48. Optimal design of machine components using notch correction and plasticity models10.1016/j.compstruc.2006.08.092 ↗
49. Analytical durability modeling and evaluation—complementary techniques for physical testing of automotive components10.1016/j.engfailanal.2003.05.018 ↗
50. Closure-free biaxial fatigue crack growth rate and life prediction under various biaxiality ratios in SAE 1045 steel10.1046/j.1460-2695.1999.t01-1-00189.x ↗
51. Analytical and experimental studies on fatigue crack path under complex multi-axial loading10.1111/j.1460-2695.2006.01001.x ↗
52. Biaxial low cycle fatigue fracture of 316 stainless steel at elevated temperature
53. Brown MW, Miller KJ. A theory for fatigue failure under multiaxial stress–strain conditions, In: Proceedings of the institute of mechanical engineers, 1973. p. 745–55.10.1243/PIME_PROC_1973_187_069_02 ↗
54. A theory for the effect of mean stress on fatigue of metals under combined torsion and axial load or bending10.1115/1.4008327 ↗
55. Wang CH, Brown MW. Life prediction techniques for variable amplitude multiaxial fatigue—Part 1: theories. J Eng Mater Technol Trans ASME, 1996a; 118: 367–370.10.1115/1.2806821 ↗
56. A method based on virtual strain-energy parameters for multiaxial fatigue life prediction
57. Short fatigue crack growth under nonproportional multiaxial elastic–plastic strains10.1016/j.ijfatigue.2005.08.012 ↗
58. Fatigue of 7075-T651 aluminum alloy10.1016/j.ijfatigue.2007.07.005 ↗
59. Strain controlled cyclic deformation behavior of an extruded magnesium alloy10.1016/j.msea.2008.05.016 ↗
60. Yang F, Lv F, Yang XM, Li SX, Zhang ZF, Wang QD. Enhanced very high cycle fatigue performance of extruded Mg–12Gd–3Y–0.5Zr magnesium alloy. Mater Sci Eng A–Struct 2011; 528: 2231–2238.10.1016/j.msea.2010.12.092 ↗
61. Mechanical anisotropy due to twinning in an extruded AZ31 Mg alloy10.1016/j.msea.2007.07.076 ↗
62. Multiaxial fatigue damage models10.1115/1.3225980 ↗
63. Upper and lower fatigue life limits model using energy-based fatigue properties10.1016/j.ijfatigue.2005.07.039 ↗
64. An energy-based fatigue life assessment model for various metallic materials under proportional and non-proportional loading conditions10.1016/j.ijfatigue.2006.07.017 ↗
65. Brown DW, Jain A, Agnew SR, Clausen B. Twinning and detwinning during cyclic deformation of Mg alloy AZ31B. Thermec 2006, Pts 1-5. 2007; 539–543: 3407–3413.10.4028/www.scientific.net/MSF.539-543.3407 ↗
66. In situ neutron diffraction investigation of deformation twinning and pseudoelastic-like behaviour of extruded AZ31 magnesium alloy10.1016/j.ijplas.2008.08.002 ↗
67. The role of twinning and untwinning in yielding behavior in hot-extruded Mg–Al–Zn alloy10.1016/j.actamat.2006.09.010 ↗
68. Abbaschian · 2008
69. Mechanical anisotropy of extruded Mg–6% Al–1% Zn alloy10.1016/j.msea.2004.02.020 ↗
70. Enhanced deformation mechanisms by anisotropic plasticity in polycrystalline Mg alloys at room temperature10.1007/s11661-005-0032-4 ↗
71. A crystal plasticity theory for latent hardening by glide twinning through dislocation transmutation and twin accommodation effects10.1016/j.jmps.2009.12.004 ↗
72. Computer simulation of screw dislocation interactions with twin boundaries in H.C.P. metals10.1016/0956-7151(95)00128-I ↗
73. Slip, twinning, and fracture in hexagonal close-packed metals10.1007/BF02648537 ↗
74. In-phase and out-of-phase multiaxial fatigue10.1115/1.2903365 ↗
75. A critical plane-strain energy density criterion for multiaxial low-cycle fatigue life under non-proportional loading10.1046/j.1460-2695.1999.t01-1-00199.x ↗
76. Nonproportional low cycle fatigue criterion for type 304 stainless steel10.1115/1.2804541 ↗
77. Notch effect on multiaxial low cycle fatigue10.1016/j.ijfatigue.2011.01.011 ↗
78. Low and high cycle fatigue—a continuum supported by AFM observations10.1016/S1359-6454(98)00169-4 ↗
79. Fatigue of constructional steel S460 under complex cyclic stress and strain sequences10.1016/j.proeng.2011.04.047 ↗
80. Deformations and damage to metallic materials under multiaxial non-proportional loading10.1016/j.commatsci.2009.01.022 ↗
81. Short crack approach for multiaxial fatigue assessment10.1002/mawe.200800351 ↗
82. Short-crack-growth-based fatigue assessment of notched components under multiaxial variable amplitude loading10.1016/j.engfracmech.2011.01.016 ↗
83. Short fatigue crack growth under nonproportional multiaxial elastic–plastic strains10.1016/j.ijfatigue.2005.08.012 ↗
84. Deformation behaviour, short crack growth and fatigue live sunder multiaxial nonproportional loading10.1016/j.ijfatigue.2005.05.014 ↗
85. Expected principal stress directions under multiaxial random loading. Part I: theoretical aspects of the weight function method10.1016/S0142-1123(98)00046-2 ↗
86. Expected principal stress directions under multiaxial random loading. Part II: numerical simulation and experimental assessment through the weight function method10.1016/S0142-1123(98)00047-4 ↗
87. A fracture plane approach in multiaxial high-cycle fatigue of metals10.1046/j.1460-2695.2000.00265.x ↗
88. Multiaxial fatigue assessment using a simplified critical plane-based criterion10.1016/j.ijfatigue.2011.01.004 ↗
89. Multiaxial fatigue life estimation in welded joints using the critical plane approach10.1016/j.ijfatigue.2008.03.024 ↗