journal article·2017-11Open access

Evaluation of fatigue crack propagation behaviour in Ti-6Al-4V manufactured by selective laser melting

K.F. Walker, Q. Liu, M. Brandt

Abstract

Abstract Total fatigue life performance of high strength titanium alloy Ti-6Al-4V manufactured by Additive Manufacturing (AM) based methods such as Selective Laser Melting (SLM) is of significant interest and has gained much attention recently. Researchers often compare the total fatigue life of materials manufactured from SLM with conventional manufacture, and often the SLM lives are reduced because cracks initiate from “defects” such as porosity or Lack of Fusion (LOF). But for repair and alternative manufacture of complex and critical aerospace structures for example, the crack growth/propagation phase of the fatigue process is also very important and it has not been studied as extensively. The aim of the work presented here was to evaluate and better understand crack propagation under constant amplitude loading in Ti-6Al-4V samples manufactured using SLM with a variety of layer thicknesses and build directions (vertical or horizontal). The “as-manufactured” condition was studied, with no post heat treatment. Cracks typically initiated at LOF features which had a negative impact on the total fatigue life. The focus here was on the crack growth phase. Modelling was performed with a conventional Linear Elastic Fracture Mechanics approach using literature data obtained from testing on Compact Tension (C(T)) specimens which were also in the as-manufactured condition with a variety of build directions. The modelling provided a very useful correlation of the data and provided a way of assessing the LOF features in terms of an equivalent initial crack. The crack growth properties of the SLM cases were also compared against literature data for conventionally manufactured material. The work will lead to a better understanding of fatigue crack growth characteristics for components manufactured by AM methods such as SLM. That understanding is an essential requirement for full certification and acceptance into service for critical applications such as aerospace structures.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Huang · 2014
2. The manufacturing of hard tools from metallic powders by selective laser melting10.1016/S0924-0136(01)00522-2 ↗
3. Rapid manufacturing of metal components by laser forming
4. Microstructure and mechanical behavior of Ti-6Al-4V produced by rapid-layer manufacturing, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
5. A study of the microstructural evolution during selective laser melting of Ti-6Al-4V10.1016/j.actamat.2010.02.004 ↗
6. Selective laser melting of biocompatible metals for rapid manufacturing of medical parts10.1108/13552540710776142 ↗
7. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
8. Dhansay NM, Tait R, Becker T, Fatigue and fracture toughness of Ti-6Al-4V titanium alloy manufactured by selective laser melting. Advan Mater Res, vol. 1019. 2014: trans tech publications Ltd. :248–3.10.4028/www.scientific.net/AMR.1019.248 ↗
9. Effect of build direction on the fracture toughness and fatigue crack growth in selective laser melted Ti-6Al-4V10.1111/ffe.12303 ↗
10. Günther, J., et al., Fatigue life of additively manufactured Ti-6Al-4V in the very high cycle fatigue regime. Int J Fatigue, 2017. 94(Part 2): pp. 236–5.10.1016/j.ijfatigue.2016.05.018 ↗
11. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
12. Critical assessment of the fatigue performance of additively manufactured Ti-6Al-4V and perspective for future research10.1016/j.ijfatigue.2015.12.003 ↗
13. The Effect of manufacturing defects on the fatigue behaviour of ti-6al- 4v specimens fabricated using selective laser melting10.4028/www.scientific.net/AMR.891-892.1519 ↗
14. Anon, Metallic materials properties development and standardization, 2016, Batelle Memorial Institute.
15. Typical fatigue-initiating discontinuities in metallic aircraft structures10.1016/j.ijfatigue.2011.10.017 ↗
16. Using the lead crack concept and fractal geometry for fatigue lifing of metallic structural components
17. Walker KF, Lourenco JM, Sun S, Brandt M, Wang CH. Quantitative fractography and modelling of fatigue crack propagation in high strength AerMet100 steel repaired with a laser cladding process. Int J Fatigue 2017;94:288–301. http://dx.doi.org/10.1016/j.ijfatigue.2016.06.031.10.1016/j.ijfatigue.2016.06.031 ↗
18. Harter JA, AFGROW user's guide and technical manual, AFRL-VA-WP-TR-2004, 2004.