Abstract
Abstract Effects of build orientation (0°, 45°, 90°) and post heat treatments (hot isostatic pressing 820 °C, 950 °C or annealing 1020 °C) on the fatigue crack growth rates (FCGRs) of Ti-6Al-4V fabricated by laser powder bed fusion were examined. Coarser α′/α lath thicknesses resulted in slower FCGRs and higher fatigue thresholds while texture and build orientation had little influence. Fatigue thresholds were defined by the ability to transfer slip from one α′/α lath to another, with a minor role of roughness induced crack closure. The transition away from microstructure sensitive FCG occurred where the packet/colony size equaled the cyclic plastic zone size.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (85)
Show source-provided references
1. Rapid manufacturing and rapid tooling with layer manufacturing (LM) technologies, state of the art and future perspectives10.1016/S0007-8506(07)60206-6 ↗
2. Additive manufacturing of metals10.1016/j.actamat.2016.07.019 ↗
3. Microstructure and mechanical behavior of Ti–6Al–4V produced by rapid-layer manufacturing, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
4. Compressive and fatigue behavior of beta-type titanium porous structures fabricated by electron beam melting10.1016/j.actamat.2016.12.052 ↗
5. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
6. An overview of Direct Laser Deposition for additive manufacturing; Part II: Mechanical behavior, process parameter optimization and control
7. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
8. Selective laser melting of weak-textured commercially pure titanium with high strength and ductility: a study from laser power perspective10.1016/j.matdes.2016.12.019 ↗
9. The origin of microstructural diversity, texture, and mechanical properties in electron beam melted Ti-6Al-4V10.1007/s11661-010-0397-x ↗
10. Microstructural evolution in laser-deposited multilayer Ti-6Al-4V builds: Part I. Microstructural characterization10.1007/s11661-004-0094-8 ↗
11. On the texture formation of selective laser melted Ti-6Al-4V10.1007/s11661-014-2218-0 ↗
12. Lütjering · 2007
13. Influence of texture on fatigue properties of Ti-6Al-4V10.1007/BF02657799 ↗
14. New development in selective laser melting of Ti–6Al–4V: a wider processing window for the achievement of fully lamellar α+ β microstructures
15. A review of the as-built SLM Ti-6Al-4V mechanical properties towards achieving fatigue resistant designs10.3390/met8010075 ↗
16. Influence of post fabrication heat treatments on the fatigue behavior of Ti-6Al-4V produced by selective laser melting10.1016/j.prostr.2017.11.070 ↗
17. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
18. Heat treatment of Ti6Al4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
19. Heat treatment of Ti-6Al-7Nb components produced by selective laser melting10.1108/13552540810907974 ↗
20. Influence of tempering temperature and time on the α′-Ti-6Al-4V martensite10.1016/0925-8388(95)02057-8 ↗
21. Ductility improvement due to martensite α′ decomposition in porous Ti–6Al–4V parts produced by selective laser melting for orthopedic implants10.1016/j.jmbbm.2015.09.020 ↗
22. Influence of processing on microstructure and mechanical properties of (α+β) titanium alloys10.1016/S0921-5093(97)00778-8 ↗
23. Formation of α-Widmanstätten structure: effects of grain size and cooling rate on the Widmanstätten morphologies and on the mechanical properties in Ti6Al4V alloy10.1016/S0925-8388(01)01571-7 ↗
24. Additive manufacturing of fatigue resistant materials: challenges and opportunities10.1016/j.ijfatigue.2017.01.001 ↗
25. Ti-6Al-4V additively manufactured by selective laser melting with superior mechanical properties10.1007/s11837-015-1297-8 ↗
26. Characterization of titanium aluminide alloy components fabricated by additive manufacturing using electron beam melting10.1016/j.actamat.2009.11.032 ↗
27. Effect of hot isostatic pressing procedure on performance of Ti6Al4V: surface qualities, microstructure and mechanical properties10.1016/j.jallcom.2016.05.280 ↗
28. Microstructure and mechanical properties of pure titanium models fabricated by selective laser melting10.1243/0954406041319545 ↗
29. Fatigue behaviour of notched additive manufactured Ti6Al4V with as-built surfaces10.1016/j.ijfatigue.2017.04.009 ↗
30. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
31. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V10.1016/j.msea.2013.04.099 ↗
32. Fatigue performances of selective laser melted Ti-6Al-4V alloy: Influence of surface finishing, hot isostatic pressing and heat treatments10.1016/j.ijfatigue.2018.11.019 ↗
33. Effects of processing parameters on microstructure and mechanical property of selective laser melted Ti6Al4V10.1016/j.matdes.2011.09.051 ↗
34. Influence of defects on mechanical properties of Ti–6Al–4V components produced by selective laser melting and electron beam melting10.1016/j.matdes.2015.07.147 ↗
35. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗
36. Van Hooreweder B, Boonen R, Moens D, Kruth J-P, Sas P. On the determination of fatigue properties of Ti6Al4V produced by selective laser melting. In: 53rd AIAA/ASME/ASCE/AHS/ASC structures, structural dynamics and materials conference, American Institute of Aeronautics and Astronautics; 2012.10.2514/6.2012-1733 ↗
37. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗
38. On the fatigue properties of metals manufactured by selective laser melting – the role of ductility10.1557/jmr.2014.157 ↗
39. Analysis of defect generation in Ti–6Al–4V parts made using powder bed fusion additive manufacturing processes
40. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
41. Microstructures and mechanical properties of Ti6Al4V parts fabricated by selective laser melting and electron beam melting10.1007/s11665-013-0658-0 ↗
42. An overview of Direct Laser Deposition for additive manufacturing. Part I: Transport phenomena, modeling and diagnostics
43. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
44. Effects of the microstructure and porosity on properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)
45. Effects of heat treatments on microstructure and properties of Ti-6Al-4V ELI alloy fabricated by electron beam melting (EBM)10.1016/j.msea.2017.01.019 ↗
46. Micro-and meso-structures and their influence on mechanical properties of selectively laser melted Ti-6Al-4V10.1016/j.actamat.2018.05.044 ↗
47. A comprehensive study on variability of relative density in selective laser melting of Ti-6Al-4V10.1080/17452759.2019.1614198 ↗
48. Microstructure, defects and mechanical behavior of beta-type titanium porous structures manufactured by electron beam melting and selective laser melting10.1016/j.actamat.2016.04.029 ↗
49. Enhanced fatigue characteristics of a topology-optimized porous titanium structure produced by selective laser melting
50. Compressive and fatigue behavior of functionally graded Ti-6Al-4V meshes fabricated by electron beam melting10.1016/j.actamat.2018.02.060 ↗
51. The influence of oxygen on the chemical composition and mechanical properties of Ti-6Al-4V during laser powder bed fusion (L-PBF)
52. Effect of build direction on the fracture toughness and fatigue crack growth in selective laser melted Ti-6Al-4 V10.1111/ffe.12303 ↗
53. Crack propagation and fracture toughness of Ti6Al4V alloy produced by selective laser melting
54. Microstructural optimization through heat treatment for enhancing the fracture toughness and fatigue crack growth resistance of selective laser melted Ti6Al4V alloy10.1016/j.actamat.2019.03.003 ↗
55. Influence of re-melting on surface roughness and porosity of AlSi10Mg parts fabricated by selective laser melting10.1016/j.jallcom.2019.04.017 ↗
56. Effect of scanning strategy on mechanical properties of selective laser melted Inconel 71810.1016/j.msea.2019.03.007 ↗
57. Evaluation of the impact of scanning strategies on residual stresses in selective laser melting10.1007/s00170-019-03396-9 ↗
58. The effect of hatch angle rotation on parts manufactured using selective laser melting10.1108/RPJ-06-2017-0111 ↗
59. Numerical analysis of the effect of the scan strategy on the residual stress in the multi-laser selective laser melting
60. Microstructure modelling for metallic additive manufacturing: a review10.1080/17452759.2019.1677345 ↗
61. Comparison of density measurement techniques for additive manufactured metallic parts10.1108/13552541111156504 ↗
62. ASTM Standard E8/E8M-16ae1 Standard Test Methods for Tension Testing of Metallic Materials, in: ASTM International, West Conshohocken, PA; ASTM International; 2016. doi: 10.1520/E0008_E0008M-16AE01, www.astm.org.10.1520/E0008_E0008M-16AE01 ↗
63. ASTM Standard E647-15e1, Standard Test Method for Measurement of Fatigue Crack Growth Rates, in: ASTM International, West Conshohocken, Pennsylvania, USA; 2015, doi: 10.1520/E0647-1515E1501, www.astm.org.
64. Conversion of intercept density to grain size
65. ISO/DIS 21920-2:2020(E). Geometrical Product Specifications (GPS)--surface Texture: Profile Method--rules and Procedures for the Assessment of Surface Texture in: ISO, Switzerland; 2020, doi: 10.31030/3137774, www.iso.org.10.31030/3137774 ↗
66. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti6Al4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
67. Diffraction-based misorientation mapping: a continuum mechanics description10.1016/j.jmps.2019.103709 ↗
68. Microstructural influences on fatigue crack growth in Ti-6Al-4V10.1016/0025-5416(74)90104-9 ↗
69. Fatigue crack propagation resistance of beta-annealed Ti-6AI-4V alloys of differing interstitial oxygen contents10.1007/BF02661812 ↗
70. Quantitative analysis of microstructural effects on fatigue crack growth in widmanstätten Ti-6A1-4V and Ti-8Al-1Mo-1V10.1016/0013-7944(79)90138-3 ↗
71. Observations on microstructurally sensitive fatigue crack growth in a widmanstätten Ti-6Al-4V alloy10.1007/BF02646877 ↗
72. Fatigue crack growth transitions in Ti-6Al-4V alloy10.1016/0036-9748(89)90343-8 ↗
73. Fractographic and microstructural analysis of fatigue crack growth in a Ti-6Al-4V fan disc forging10.1016/0142-1123(89)90179-5 ↗
74. A study on the change of fatigue fracture mode in two titanium alloys10.1046/j.1460-2695.1998.00095.x ↗
75. Modeling the tensile properties in β-processed α/β Ti alloys10.1007/s11661-006-0028-8 ↗
76. Formation and control of martensite in Ti-6Al-4V alloy produced by selective laser melting10.1016/j.matdes.2016.06.117 ↗
77. Predicting tensile properties of Ti-6Al-4V produced via directed energy deposition10.1016/j.actamat.2017.05.025 ↗
78. Dislocation pile-up model of fatigue thresholds for 2024- and 7075-alike aluminium alloys10.1016/0167-8442(95)00040-2 ↗
79. Theoretical modelling of fatigue threshold for aluminium alloys10.1016/0013-7944(95)00206-5 ↗
80. Near-threshold fatigue: a review10.1016/S0142-1123(99)00053-5 ↗
81. Fatigue growth threshold of small cracks10.1007/BF00033345 ↗
82. A geometric model for fatigue crack closure induced by fracture surface roughness10.1007/BF02644803 ↗
83. Some considerations on fatigue crack closure at near-threshold stress intensities due to fracture surface morphology10.1007/BF02642409 ↗
84. Fatigue crack deflection and fracture surface contact: Micromechanical models10.1007/BF02816051 ↗
85. Rice J, Tracey DM. Computational fracture mechanics. In: Numerical and computer methods in structural mechanics. Elsevier; 1973. p. 585–623.10.1016/B978-0-12-253250-4.50031-2 ↗