Anisotropic high cycle fatigue behavior of Ti–6Al–4V obtained by powder bed laser fusion

Gianni Nicoletto

Publisher page

Abstract

Abstract An original fatigue test methodology aimed at PBF materials is presented and directed to the evaluation of the anisotropic fatigue behavior of DMLS Ti6Al4V. The presence of such anisotropy is intrinsic to the specific and complex microstructure obtained by the layer-by-layer development of the part produced by DMLS. Comparison of the present test results with data obtained with a variety of test methods and test parameters clarified the role of intrinsic (material-dependent) and extrinsic (test-method-dependent) factors on the measured fatigue behavior. The proposed testing method permits substantial cost saving in terms of material and process time, benefits that are especially welcome for developmental studies of PBF alloys and process parameters.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Gibson · 2014 · 498
2. Gebhardt · 2011 · 164
3. Experimental studies on selective laser melting of metallic parts10.1002/mawe.200800327 ↗
4. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
5. Consolidation phenomena in laser and powder-bed based layered manufacturing10.1016/j.cirp.2007.10.004 ↗
6. Microstructure and tensile properties of selectively laser-melted and of HIPed laser-melted Ti–6Al–4V10.1016/j.msea.2013.04.099 ↗
7. As-fabricated and heat-treated microstructures of the Ti–6Al–4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
8. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti–6Al–4V10.1016/j.msea.2014.07.086 ↗
9. Residual stresses in selective laser sintering and selective laser melting10.1108/13552540610707013 ↗
10. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗
11. Van Hooreweder B et al. On the determination of fatigue properties of Ti6Al4V produced by selective laser melting. In: Proc 53rd AIAA/ASME/ASCE/AHS/ASC structures, structural dynamics and materials conference, Honolulu, Hawaii. http://dx.doi.org/10.2514/6.2012-1733.10.2514/6.2012-1733 ↗
12. Rekedal KD. Investigation of the high-cycle fatigue life of selective laser melted and hot-isostatically-pressed Ti–6Al–4V. M.S. Thesis, AFIT-ENY-MS-15-M-212 Wright-Patterson AFB, Ohio; 2015.10.2514/6.2015-0894 ↗
13. High cycle fatigue (HCF) performance of Ti–6Al–4V alloy processed by selective laser melting10.4028/www.scientific.net/AMR.816-817.134 ↗
14. Nicoletto G et al. Tensile and fatigue behavior of Ti6Al4V produced by selective laser melting. In: Proc 4th international conference of engineering against failure (ICEAF IV), Skiathos, Greece; 2015.
15. Nicholas · 2006
16. Microstructure, defects and fractography of Ti6Al4V alloy produced by SLM and DMLS
17. Fatigue of titanium alloys