journal article·2020-03Open access

Fatigue of additive manufactured Ti-6Al-4V, Part I: The effects of powder feedstock, manufacturing, and post-process conditions on the resulting microstructure and defects

J.W. Pegues, S. Shao, N. Shamsaei, N. Sanaei, A. Fatemi, D.H. Warner, P. Li, N. Phan

Abstract

Abstract Additive manufacturing provides an appealing means to process titanium alloy parts with new levels of conformability, complexity, and weight reduction. However, due to the heating/cooling rates and heat transfer associated with directed energy source material processing, the as-built AM parts contain unique material and microstructural features. In order to confidently manufacture fatigue critical additive manufactured (AM) Ti-6Al-4V parts, a better understanding of the interrelationships between powder feedstock, AM processes, structure of the processed parts, their resulting mechanical properties, and their performance under realistic loadings is necessary. Part I of this two-part collection focuses on the powder-process-structure relationships and how powder feedstock, manufacturing, and post-processing conditions can affect the microstructure and defect features that ultimately contribute to the fatigue performance of Ti-6Al-4V parts. The material and physical phenomena inherent to the AM process of Ti-6Al-4V are discussed in detail and related to the phase composition/structure, grain morphology, surface characteristics, defect size/distribution, and post-process treatments available for AM parts. This investigation is the foundation for the structure-performance relationships that will be discussed in detail in Part II.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (100+)

Show source-provided references
1. An overview of Direct Laser Deposition for additive manufacturing. Part II: Mechanical behavior, process parameter optimization and control
2. An overview of Direct Laser Deposition for additive manufacturing. Part I: Transport phenomena, modeling and diagnostics
3. Metal additive manufacturing: a review10.1007/s11665-014-0958-z ↗
4. Laser additive manufacturing of metallic components: materials, processes and mechanisms10.1179/1743280411Y.0000000014 ↗
5. E. Herderick, Additive manufacturing of metals: A review, Materials Science and Technology (MS); 2011. p.1413.
6. ASTM International · 2015
7. Brandt · 2016
8. Gockel J, Beuth J. Understanding Ti-6Al-4V microstructure control in additive manufacturing via process maps. Solid Freeform Fabrication Proceedings, Austin, TX; Aug (2013): p. 12–14.
9. Effects of pre-straining and coating on plastic deformation of aluminum micropillars10.1016/j.actamat.2012.07.048 ↗
10. Lütjering G, Williams JC. Titanium. Springer; 2003.10.1007/978-3-540-71398-2 ↗
11. Microstructures of laser-deposited Ti–6Al–4V10.1016/j.matdes.2003.09.009 ↗
12. The origin of microstructural diversity, texture, and mechanical properties in electron beam melted Ti-6Al-4V10.1007/s11661-010-0397-x ↗
13. Integrated control of solidification microstructure and melt pool dimensions in electron beam wire feed additive manufacturing of Ti-6Al-4V
14. Mean stress/strain effect on fatigue behavior of an epoxy resin10.1016/j.ijfatigue.2006.12.009 ↗
15. Fatigue crack initiation in alpha-beta titanium alloys10.1016/S0142-1123(97)00047-9 ↗
16. Effect of build geometry on the β-grain structure and texture in additive manufacture of Ti6Al4V by selective electron beam melting10.1016/j.matchar.2013.07.012 ↗
17. Fatigue behavior and cyclic deformation of additive manufactured NiTi10.1016/j.jmatprotec.2017.10.006 ↗
18. The mechanical and microstructural characteristics of laser-deposited IN71810.1016/j.jmatprotec.2005.05.005 ↗
19. Gong H, Rafi K, Karthik NV, Starr T, Stucker B. Defect morphology in Ti-6Al-4V parts fabricated by selective laser melting and electron beam melting. Solid Freeform Fabrication Proceedings, Austin, TX; Aug 2018.
20. Correlation between porosity and processing parameters in TiAl6V4 produced by selective laser melting10.1016/j.matdes.2016.05.070 ↗
21. Fatigue of Nitinol: the state-of-the-art and ongoing challenges10.1016/j.jmbbm.2015.06.010 ↗
22. Effects of building orientation and heat treatment on fatigue behavior of selective laser melted 17–4 PH stainless steel10.1016/j.ijfatigue.2016.03.014 ↗
23. Fatigue performance evaluation of selective laser melted Ti–6Al–4V10.1016/j.msea.2014.01.041 ↗
24. Microstructure and mechanical properties of Ti-6Al-4V produced by electron beam melting of pre-alloyed powders10.1108/13552540910960262 ↗
25. Ductility of a Ti-6Al-4V alloy produced by selective laser melting of prealloyed powders10.1108/13552541011083371 ↗
26. Influence of defects on mechanical properties of Ti–6Al–4 V components produced by selective laser melting and electron beam melting10.1016/j.matdes.2015.07.147 ↗
27. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: Fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
28. Microstructures and mechanical properties of electron beam-rapid manufactured Ti–6Al–4V biomedical prototypes compared to wrought Ti–6Al–4V10.1016/j.matchar.2008.07.006 ↗
29. Microstructure and mechanical behavior of Ti–6Al–4V produced by rapid-layer manufacturing, for biomedical applications10.1016/j.jmbbm.2008.05.004 ↗
30. Fabrication of large Ti–6Al–4V structures by direct laser deposition10.1016/j.jallcom.2014.12.234 ↗
31. Selective laser melting of biocompatible metals for rapid manufacturing of medical parts10.1108/13552540710776142 ↗
32. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
33. Microstructure evolution, tensile properties, and fatigue damage mechanisms in Ti-6Al-4V alloys fabricated by two additive manufacturing techniques10.1016/j.proeng.2015.08.007 ↗
34. Fatigue behavior and failure mechanisms of direct laser deposited Ti–6Al–4V10.1016/j.msea.2015.12.026 ↗
35. Fatigue performance of laser additive manufactured Ti–6Al–4V in very high cycle fatigue regime up to 109 cycles10.3389/fmats.2015.00072 ↗
36. Critical assessment of the fatigue performance of additively manufactured Ti–6Al–4V and perspective for future research10.1016/j.ijfatigue.2015.12.003 ↗
37. Analysis of defect generation in Ti–6Al–4V parts made using powder bed fusion additive manufacturing processes
38. In situ X-ray imaging of defect and molten pool dynamics in laser additive manufacturing10.1038/s41467-018-03734-7 ↗
39. Microstructure of additive layer manufactured Ti–6Al–4V after exceptional post heat treatments10.1016/j.matlet.2012.04.116 ↗
40. Selective laser melting produced Ti-6Al-4V: post-process heat treatments to achieve superior tensile properties10.3390/ma11010146 ↗
41. As-fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting10.1007/s11661-011-0731-y ↗
42. Heat treatment of Ti6Al4V produced by Selective Laser Melting: Microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
43. Significance of hot isostatic pressing (HIP) on multiaxial deformation and fatigue behaviors of additive manufactured Ti-6Al-4V including build orientation and surface roughness effects10.1016/j.ijfatigue.2018.07.035 ↗
44. Effect of Inter-Layer Time Interval on the Mechanical Behavior of Direct Laser Deposited Ti-6Al-4V
45. Towards predicting differences in fatigue performance of laser powder bed fused Ti-6Al-4V coupons from the same build10.1016/j.ijfatigue.2019.05.004 ↗
46. Fatigue behaviour of additive manufactured materials: An overview of some recent experimental studies on Ti-6Al-4V considering various processing and loading direction effects10.1111/ffe.13000 ↗
47. Additive manufacturing of Ti6Al4V alloy: A review10.1016/j.matdes.2018.107552 ↗
48. The effect of laser energy input on the microstructure, physical and mechanical properties of Ti-6Al-4V alloys by selective laser melting10.1080/17452759.2016.1142215 ↗
49. Wire based additive layer manufacturing: Comparison of microstructure and mechanical properties of Ti–6Al–4V components fabricated by laser-beam deposition and shaped metal deposition10.1016/j.jmatprotec.2011.01.018 ↗
50. Phase transformations during cooling in α+β titanium alloys10.1016/S0921-5093(97)00802-2 ↗
51. Sieniawski J, Ziaja W, Motyka KKAM. Microstructure and mechanical properties of high strength two-phase titanium alloys. Titanium Alloys - Advances in Properties Control; 2013.10.5772/56197 ↗
52. Atomic-scale analysis of martensitic transformation in titanium alloyed with vanadium Part I: verification of the embedded-atom method model10.1016/0921-5093(95)09894-1 ↗
53. Microstructures and mechanical properties of Ti6Al4V parts fabricated by selective laser melting and electron beam melting10.1007/s11665-013-0658-0 ↗
54. Barrett CR, Nix WD, Tetelman AS. The principles of engineering materials. Prentice Hall; 1973.
55. Callister · 1991
56. Microstructural evolution and microhardness of a selective-laser-melted Ti–6Al–4V alloy after post heat treatments10.1016/j.jallcom.2016.02.183 ↗
57. The laser additive manufacture of Ti-6Al-4V10.1007/s11837-001-0068-x ↗
58. Microstructure and texture evolution during solidification processing of Ti–6Al–4V10.1016/S0924-0136(02)00865-8 ↗
59. Steady state columnar and equiaxed growth of dendrites and eutectic10.1016/0025-5416(84)90201-5 ↗
60. Surface roughness effects on the fatigue strength of additively manufactured Ti-6Al-4V10.1016/j.ijfatigue.2018.07.013 ↗
61. Fatigue life estimation of additive manufactured parts in the as-built surface condition,10.1002/mdp2.36 ↗
62. Moylan S, Slotwinski J, Cooke A, Jurrens K, Donmez MA. Proposal for a standardized test artifact for additive manufacturing machines and processes. In: Proceedings of the 2012 annual international solid freeform fabrication symposium. Austin, TX; 2012.10.6028/NIST.IR.7858 ↗
63. Surface roughness analysis, modelling and prediction in selective laser melting10.1016/j.jmatprotec.2012.11.011 ↗
64. El-Sayed M, Ghazy M, Yehia Y, Essa K. Optimization of SLM Process Parameters for Ti6Al4V Medical Implants.
65. Top surface and side roughness of Inconel 625 parts processed using selective laser melting10.1108/13552540910943397 ↗
66. Gong H, Rafi K, Starr T, Stucker B. The effects of processing parameters on defect regularity in Ti-6Al-4V parts fabricated by selective laser melting and electron beam melting. In: 24th Annual International Solid Freeform Fabrication Symposium—An Additive Manufacturing Conference, Austin, TX; Aug. 2013.
67. Shrestha R, Simsiriwong J, Shamsaei N, Thompson SM, Bian L. Effect of build orientation on the fatigue behavior of stainless steel 316L manufactured via a laser-powder bed fusion process. In: 27th Annual Solid Frefform Fabrication Symposium Proceedings; 2016.
68. Surface texture measurement for additive manufacturing10.1088/2051-672X/3/2/024002 ↗
69. Charles A, Elkaseer A, Müller T, Thijs L, Torge M, Hagenmeyer V, et al. A study of the factors influencing generated surface roughness of down-facing surfaces in selective laser melting. In; Proceedings of the World Congress on Micro and Nano Manufacturing (WCMNM), Portorož, Slovenia; 2018.10.3850/978-981-11-2728-1_57 ↗
70. Surface texture metrology for metal additive manufacturing: a review10.1016/j.precisioneng.2016.06.001 ↗
71. Areal topography measurement of metal additive surfaces using focus variation microscopy
72. Effect of process parameters settings and thickness on surface roughness of EBM produced Ti-6Al-4V10.1108/13552541211250391 ↗
73. Characterization of typical surface effects in additive manufacturing with confocal microscopy10.1088/2051-672X/3/1/014001 ↗
74. Characterization of metal additive manufacturing surfaces using synchrotron X-ray CT and micromechanical modeling10.1007/s00466-017-1531-z ↗
75. X-ray computed tomography for additive manufacturing: a review10.1088/0957-0233/27/7/072001 ↗
76. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
77. A study of the microstructural evolution during selective laser melting of Ti–6Al–4V10.1016/j.actamat.2010.02.004 ↗
78. Laser powder bed fusion additive manufacturing of metals; physics, computational, and materials challenges10.1063/1.4937809 ↗
79. Metal vapor micro-jet controls material redistribution in laser powder bed fusion additive manufacturing10.1038/s41598-017-04237-z ↗
80. Effect of heat treatments on pore morphology and microstructure of laser additive manufactured parts
81. Solubility of argon in laser additive manufactured α-titanium under hot isostatic pressing condition10.1016/j.commatsci.2017.01.040 ↗
82. Is the energy density a reliable parameter for materials synthesis by selective laser melting?10.1080/21663831.2017.1299808 ↗
83. Strain-based fatigue data for Ti–6Al–4V ELI under fully-reversed and mean strain loads10.1016/j.dib.2016.02.014 ↗
84. Progress towards metal additive manufacturing standardization to support qualification and certification10.1007/s11837-017-2265-2 ↗
85. Defect characteristics and analysis of their variability in metal L-PBF additive manufacturing
86. Porosity testing methods for the quality assessment of selective laser melted parts10.1016/j.cirp.2016.04.054 ↗
87. Effects of post-processing on cyclic fatigue response of a titanium alloy additively manufactured by electron beam melting10.1016/j.msea.2016.10.059 ↗
88. Defect distribution and microstructure heterogeneity effects on fracture resistance and fatigue behavior of EBM Ti–6Al–4V10.1016/j.ijfatigue.2016.06.001 ↗
89. Porosity measurements and analysis for metal additive manufacturing process control10.6028/jres.119.019 ↗
90. Linking process, structure, property, and performance for metal-based additive manufacturing: computational approaches with experimental support10.1007/s00466-015-1240-4 ↗
91. Small defects and inhomogeneities in fatigue strength: experiments, models and statistical implications10.1023/A:1009976418553 ↗
92. Murakami · 2019
93. Fatigue life of additively manufactured Ti–6Al–4V in the very high cycle fatigue regime10.1016/j.ijfatigue.2016.05.018 ↗
94. Tang M. Inclusions, porosity, and fatigue of AlSi10Mg parts produced by selective laser melting. Carnegie Mellon University; 2017.10.1016/j.ijfatigue.2016.06.002 ↗
95. Inclusion rating by statistics of extreme values and its application to fatigue strength prediction and quality control of materials
96. Application of the generalized Pareto distribution to the estimation of the size of the maximum inclusion in clean steels10.1016/S1359-6454(99)00034-8 ↗
97. Qualification of AM parts: Extreme value statistics applied to tomographic measurements10.1016/j.matdes.2017.05.091 ↗
98. The need for powder characterisation in the additive manufacturing industry and the establishment of a national facility
99. Sutton AT, Kriewall CS, Leu MC, Newkirk JW. Powders for additive manufacturing processes: Characterization techniques and effects on part properties. In: Proceedings of the 26th Annual International Solid Freeform Fabrication Symposium–An Additive Manufacturing Conference; 2016.
100. Powder characterisation techniques and effects of powder characteristics on part properties in powder-bed fusion processes10.1080/17452759.2016.1250605 ↗