A major challenge for additively manufactured structural parts is the low fatigue strength connected to rough as-built surfaces. In this study, Ti6Al4V manufactured with laser powder bed fusion (L-PBF) and electron beam powder bed fusion (E-PBF) have been subjected to five surface processing methods, shot peening, laser shock peening, centrifugal finishing, laser polishing and linishing, in order to increase the fatigue strength. Shot peened and centrifugal finished L-PBF material achieved comparable fatigue strength to machined material. Moreover, the surface roughness alone was found to be an insufficient indicator on the fatigue strength since subsurface defects were hidden below smooth surfaces.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Characterization and analysis of surface notches on Ti-alloy plates fabricated by additive manufacturing techniques10.1088/2051-672X/3/4/044006 ↗
2. Surface roughness and directional fatigue behavior of as-built EBM and DMLS Ti6Al4V10.1016/j.ijfatigue.2018.06.011 ↗
3. The present and future of additive manufacturing in the aerospace sector: a review of important aspects10.1177/0954410014568797 ↗
4. Fatigue behaviour of notched additive manufactured Ti6Al4V with as-built surfaces
5. Fatigue performance of additive manufactured TiAl6V4 using electron and laser beam melting10.1016/j.ijfatigue.2016.05.001 ↗
6. Fatigue life of additively manufactured Ti–6Al–4V in the very high cycle fatigue regime10.1016/j.ijfatigue.2016.05.018 ↗
7. Surface roughness and radiusing of Ti6Al4V selective laser melting-manufactured parts conditioned by barrel finishing
8. Electropolishing and electropolishing-related allowances for powder bed selectively laser-melted Ti-6Al-4V alloy components10.1016/j.jmatprotec.2016.11.014 ↗
9. Enhancing surface finish of additively manufactured titanium and cobalt chrome elements using laser based finishing10.1016/j.phpro.2016.08.021 ↗
10. Laser polishing of additive manufactured Ti alloys10.1016/j.optlaseng.2017.02.005 ↗
11. Surface treatment of powder-bed fusion additive manufactured metals for improved fatigue life10.1007/s11665-018-3732-9 ↗
12. LSP Technologoes I. No Title; 2019. (accessed July 24, 2019).
13. Noyan · 1987
14. Svensson M, Ackelid U, Ab A. Titanium alloys manufactured with electron beam melting mechanical and chemical properties. Med Device Mater V Proc from Mater Process Med Devices Conf 2009; 2009. p. 189–94. doi: 10.1007/978-4-431-54237-7.10.1007/978-4-431-54237-7 ↗
15. Fatigue behaviour of additive manufactured Ti6Al4V, with as-built surfaces, exposed to variable amplitude loading10.1016/j.ijfatigue.2017.06.023 ↗
16. Improvement of fatigue resistance and ductility of TiAl6V4 processed by selective laser melting10.1016/j.jmatprotec.2015.01.025 ↗
17. On the mechanical behaviour of titanium alloy TiAl6V4 manufactured by selective laser melting: fatigue resistance and crack growth performance10.1016/j.ijfatigue.2012.11.011 ↗
18. Modeling and characterization of residual stresses in material processing10.1016/B978-0-08-096532-1.00218-1 ↗
19. Fatigue life and microstructure of additive manufactured Ti6Al4V after different finishing processes10.1016/j.msea.2019.03.119 ↗
20. Lightweight materials: understanding the basics
21. Application of mechanical surface finishing processes for roughness reduction and fatigue improvement of additively manufactured Ti-6Al-4V parts10.1016/j.ijfatigue.2017.05.008 ↗
22. High cycle fatigue (HCF) performance of Ti-6Al-4V alloy processed by selective laser melting10.4028/www.scientific.net/AMR.816-817.134 ↗
23. Fatigue properties of EBM as-built and chemically etched thin parts10.1016/j.prostr.2017.11.073 ↗
24. Military Handbook. Titanium and titanium alloys. Department of Defense; 1974.
25. Staircase testing of a titanium alloy in the gigacycle regime10.1016/j.ijfatigue.2005.10.007 ↗
26. Mechanical properties of biomedical titanium alloys10.1016/S0921-5093(97)00806-X ↗
27. Khairallah Saad, Anderson, Andrew, Rubenchik, Alexander, King W. Laser powder-bed fusion additive manufacturing: physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones. Acta Mater 2016;108:36–45. doi: 10.1016/j.actamat.2016.02.014.10.1016/j.actamat.2016.02.014 ↗
28. Ramachandran M, editor. Basic orthopaedic sciences, 2nd ed.; 2018. doi: 10.1201/9781315117294.10.1201/9781315117294 ↗
29. Pressure-induced electronic phase transitions and superconductivity in titanium10.1142/S0217979209051978 ↗