journal article·2014-01

The influence of torsional and tensile pre-straining on the validity of ductile fracture criteria

Dragisa Vilotic, Sergei Alexandrov, Leposava Sidjanin, Marko Vilotic

Publisher page

Abstract

Continuous loading and smooth strain paths are usually used to obtain data for empirical ductile fracture criteria or to verify such criteria. It is of interest to understand whether or not these ductile fracture criteria are valid for discontinuous paths. To this end, an experimental program is carried out and its results are combined with two conventional empirical ductile fracture criteria. It is shown that the criteria are not applicable for discontinuous loading paths. Based on the experimental results obtained and experimental results available in the literature it is hypothesized that a measure of rotation of the principal stress (or principal strain rate) axes relative to the material affects the initiation of ductile fracture.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal Forming Simulation Techniques · Metallurgy and Material Forming · High-Velocity Impact and Material Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department for Production Engineering, Faculty of Technical Sciences, University of Novi Sad, Novi Sad, Serbia

A.Yu. Ishlinsky Institute for Problems in Mechanics, Russian Academy of Sciences, Moscow, Russia

References (30)

Show source-provided references
1. 10.1243/09544062JMES105510.1243/09544062JMES1055 ↗
2. 10.1016/0924-0136(95)01875-110.1016/0924-0136(95)01875-1 ↗
3. 10.1115/1.318786610.1115/1.3187866 ↗
4. Chae D, Bandstra JP and Koss DA (2000) The effect of pre-strain and strain-path changes on ductile fracture: experiment and computational modeling. Material Science and Engineering A 285: 165–171.10.1016/S0921-5093(00)00642-0 ↗
5. Dodd B and Boddington P (1980) The causes of edge cracking in cold rolling. Journal of Mechanical Working Technology 3: 239–252.10.1016/0378-3804(80)90045-5 ↗
6. Enami K (2005a) The effects of compressive and tensile prestrain on ductile fracture initiation in steels. Engineering Fracture Mechanics 72: 1089–1105.10.1016/j.engfracmech.2004.07.012 ↗
7. Enami K (2005b) Ductile crack initiation behavior in steels with compressive prestrain. Journal of Marine Science and Technology 10: 41–52.10.1007/s00773-004-0187-5 ↗
8. Franz EC (1954) Effect of repeated tensile prestrain on the ductility of some metals. Transactions of AIME, Journal of Metals 198: 56–57.10.1007/BF03397980 ↗
9. Ganser H‐P, Atkins AG, Kolednik O, et al. (2001) Upsetting of cylinders: A comparision of two different damage indicators. Transactions of ASME, Journal of Engineering Materials and Technology 123: 94–99.10.1115/1.1286186 ↗
10. Gao X, Zhang T, Hayden M, et al. (2009) Effects of the stress state on plasticity and ductile failure of an aluminum 5083 alloy. International Journal of Plasticity 25: 2366–2382.10.1016/j.ijplas.2009.03.006 ↗
11. Hancock JW and Mackenzie AC (1976) On the mechanisms of ductile failure in high strenght steels subjected to multi-axial stress-states. Journal of the Mechanics and Physics of Solids 24: 147–169.10.1016/0022-5096(76)90024-7 ↗
12. Kivivuori S (1987) Assessing cold forgeability by the upsetting test. Scandinavian Journal of Metallurgy 16: 98–102.
13. Kuhn HA, Lee PW and Erturk T (1973) A fracture criterion for cold forming. Transactions of ASME, Journal of Engineering Materials and Technology 95: 213–218.10.1115/1.3443155 ↗
14. Nypan LJ (1971) Effect of unidirectional and reversed torsion on the strength and ductility of 2024 aluminium. Journal of Strain Analysis 6: 25–26.10.1243/03093247V061025 ↗
15. O'Donnell M, Banabic D, Leacock AG, et al. (2008) The effect of pre-sain and solution heat treatment on the formability of a 2024 aluminium alloy. International Journal of Material Forming Suppl 1: 253–256.10.1007/s12289-008-0353-0 ↗
16. Oh SI, Chen CC and Kobayashi S (1979) Ductile fracture in axisymmetric Extrusion. Transactions of ASME, Journal of Engineering for Industry 101: 36–44.10.1115/1.3439471 ↗
17. Oh SI and Kobayashi S (1976) Workability of aluminum alloy 7075-T6 in upsetting and rolling. Transactions of ASME, Journal of Engineering for Industry 98: 800–806.10.1115/1.3439032 ↗
18. Oyane M, Sato T, Okimoto K, et al. (1980) Criteria for ductile fracture and their applications. Journal of Mechanical Working Technology 4: 65–81.10.1016/0378-3804(80)90006-6 ↗
19. Pepe JJ (1976) Central burst formation during hydrostatic extrusion. Journal of Metallurgical Engineering 16: 46–58.
20. Rockey KC (1967) The influence of large torsional strains upon the subsequent extensional behaviour of a low carbon steel. International Journal of Mechanical Sciences 9: 767–774.10.1016/0020-7403(67)90033-1 ↗
21. Shah JJ and Kuhn HA (1986) An empirical formula for workability limits in cold upsetting and bolt heading. Journal of Applied Metalworking 4: 255–261.10.1007/BF02833933 ↗
22. Sklad MP, Atzema EH, Schouten FJ, et al. (2008) Experimental study of forming limits in multistage deformation processes. In: Proceedings of IDDRG 2008, International Conference , Olofstrom, Sweden, pp. 1–12.
23. Sowerby R and Chandrasekaran N (1984) The cold upsetting and free surface ductility of some commercial steels. Journal of Applied Metalworking 3: 257–263.10.1007/BF02833653 ↗
24. Sowerby R, O'Reilly I, Chandrasekaran N, et al. (1984) Materials testing for cold forging. Transactions of ASME, Journal of Engineering Materials and Technology 106: 101–106.10.1115/1.3225668 ↗
25. Theocaris PS and Samaras G (1968) The effect of torsional prestrain on the embrittlement of mild steel. Journal of Materials 3: 780–801.
26. Xue L (2007) Damage accumulation and fracture initiation in uncracked ductile solids subject to triaxial loading. International Journal of Solids and Structures 44: 5163–5181.10.1016/j.ijsolstr.2006.12.026 ↗
27. Vilotic D, Plancak M, Grbic S, et al. (2003) An approach to determining the workability diagram based on upsetting tests. Fatigue and Fracture of Engineering Materials and Structures 26: 305–310.10.1046/j.1460-2695.2003.00469.x ↗
28. Vilotic D, Planchak M, Chupkovich D, et al. (2006) Free surface fracture in three upsetting tests. Experimental Mechanics 46: 115–120.10.1007/s11340-006-5860-7 ↗
29. Vujović V and Shabaik A (1986) A new workability criterion for ductile materials. Transactions of ASME, Journal of Engineering Materials and Technology 108: 245–249.10.1115/1.3225876 ↗
30. Zhou J, Gao X, Hayden M, et al. (2012) An investigation of the strain rate and temperature effects on the plastic flow stress and ductile failure strain of aluminum alloys 5083-H116, 6082-T6 and a 5183 weld metal. Engineering Fracture Mechanics 85: 103–116.10.1177/0954406212450962 ↗