journal article·2025-07

Vitreous silica formation within shear bands in a dynamically compacted granular crystalline α‐quartz

Andrew A. Wereszczak, Chad M. Parish, Emily F. Ghezawi, Michael J. Lance, Sabrina E. Calzada, Dean C. Forrest

Publisher page

Abstract

Abstract A shear band is a heterogeneous, narrow seam within a solid material whose formation is caused by intense localized shearing when a sufficiently large amount of deformation occurs. If that deformation occurs at a sufficiently rapid rate, with operative friction, then co‐located ephemeral heating will occur in the shear band. In this study, shear bands were produced from dynamic shear‐induced compaction of a granular form of crystalline α‐quartz (SiO 2 ). The produced shear bands were approximately 25‐µm thick and were examined with scanning electron microscopy/electron backscatter diffraction, transmission electron microscopy, Raman spectroscopy, and nanoindentation. They were found to contain a mixture of vitreous silica and small‐sized crystallites. This finding is significant because the presence of the vitreous silica within the shear band is a postmortem indicator that the localized temperature had reached or exceeded the melting temperature (∼1723°C) of crystalline SiO 2 during the rapid shear and compaction and then sufficiently rapid cooling quenched in that vitreous state.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Mineralogy and Gemology Studies · Geological and Geochemical Analysis · Building materials and conservation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Materials Sciences and Technology Division Oak Ridge National Laboratory Oak Ridge Tennessee USA

Tickle College of Engineering University of Tennessee Knoxville Tennessee USA

Funding

U.S. Department of Energy

References (26)

Show source-provided references
1. 10.1016/j.ijimpeng.2004.03.00510.1016/j.ijimpeng.2004.03.005 ↗
2. ASTM International.Standard specification for standard sand: ASTM C778 (Vol. 04.01).West Conshohocken PA:ASTM International;2021.
3. ASTM International.Standard test method for compressive strength for hydraulic cement mortars (using 50 mm [2 in.] cube specimens): ASTM C109/C109M (Vol. 04.01).West Conshohocken PA:ASTM International;2020.
4. www.ussilica.com/locations/ottawa‐il
5. 10.1016/j.ijimpeng.2014.01.00310.1016/j.ijimpeng.2014.01.003 ↗
6. 10.1016/j.ijsolstr.2022.11202410.1016/j.ijsolstr.2022.112024 ↗
7. 10.1016/j.jmps.2024.10564410.1016/j.jmps.2024.105644 ↗
8. 10.1016/1359-6454(95)00304-510.1016/1359-6454(95)00304-5 ↗
9. International Centre for Diffraction Data.α‐SiO2(α‐quartz). PDF# 02‐005‐4718. International Centre for Diffraction Data.www.icdd.com
10. Sosman RB · 1965
11. 10.1063/1.55567010.1063/1.555670 ↗
12. Klein C · 1993
13. Cullity BD · 2001
14. 10.1016/S0074-6142(03)80021-910.1016/S0074-6142(03)80021-9 ↗
15. 10.1038/nmat153610.1038/nmat1536 ↗
16. 10.1016/j.mser.2022.10067310.1016/j.mser.2022.100673 ↗
17. 10.1111/maps.1328910.1111/maps.13289 ↗
18. 10.1038/334052a010.1038/334052a0 ↗
19. 10.1126/science.259.5095.66610.1126/science.259.5095.666 ↗
20. 10.1038/292140a010.1038/292140a0 ↗
21. 10.1016/0038-1098(81)91202-310.1016/0038-1098(81)91202-3 ↗
22. Evaluation of hardness and fracture toughness in natural quartz crystals by indentation experiments
23. Wilantewicz T · 2005
24. 10.1007/978-0-387-28920-5_1310.1007/978-0-387-28920-5_13 ↗
25. 10.1016/j.jnoncrysol.2008.05.04210.1016/j.jnoncrysol.2008.05.042 ↗
26. Varshneya AK · 2013