The Effect of Tempering and Wall Thickness on the Fracture of Pint Glasses

Richard W. Earp, Sarah V. Hainsworth, David A. Eustice, Catherine Robinson, Malcolm D. Glendenning

Abstract

This study presents a comprehensive analysis of the effect of tempering and wall thickness on the fracture of tempered drinking glasses typically used in bars and pubs in the United Kingdom. The fracture patterns are related to the manufacturing process, the glass geometry, and the level of residual stress. The bulk of experimentation was split into two categories: Firstly, an assessment of the residual stress was conducted, followed by an assessment of the fracture response of the glass in practical applications. Drinking glasses have a variable wall thickness as a consequence of their design and manufacture. This has a direct effect on the level of residual stress in the article, which in turn produces glasses that break to give fragments of variable sizes, with large sharp‐edged fragments nearer the glass rim. It is also shown that tempered glasses broken by impact have a characteristic fracture pattern. The results show that to control the fracture of glasses to produce small fragments similar to those in tempered flat glass, the wall thickness and resulting level of residual stress need to be optimized.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Structural Analysis of Composite Materials · Conservation Techniques and Studies · 3D Surveying and Cultural Heritage

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Engineering University of Leicester University Road Leicester LE1 7RH UK

Glass Technology Services Ltd. 9 Churchill Way Sheffield South Yorkshire S35 2PY UK

Funding

Engineering and Physical Sciences Research Council · Glass Technology Services

References (31)

Show source-provided references
1. 10.1179/02670830110150998010.1179/026708301101509980 ↗
2. 10.1016/S0016-0032(20)90856-610.1016/S0016-0032(20)90856-6 ↗
3. G.Quinn Fractography of ceramics and glasses. A NIST recommended practice guide; Special Publication 960‐16 National Institute of Standards and Technology Washington DC 2007.10.6028/NBS.SP.960-16 ↗
4. “Toughened Glass. Press release Brewers and Licensed Retailers Association 42 Portman Square London ” BLRA 1997.
5. Glass Technology Services private communication.
6. 10.1097/00005373-199312000-0002110.1097/00005373-199312000-00021 ↗
7. ASTM Standard C147 2010 ‘Standard Test Methods for Internal Pressure Strength of Glass Containers ’ASTM International West Conshohocken PA doi:10.1520/C0147‐86R10 www.astm.org.10.1520/C0147 ↗
8. ASTM Standard C148 2012 ‘Standard Test Methods for Polariscopic Examination of Glass Containers ’ASTM International West Conshohocken PA doi:10.1520/C0148‐12 www.astm.org.10.1520/C0148 ↗
9. ASTM Standard C149 2010 ‘Standard Test Method for Thermal Shock Resistance of Glass Containers ’ASTM International West Conshohocken PA doi:10.1520/C0149‐86R10 www.astm.org.10.1520/C0149 ↗
10. ASTM Standard C1036 2011e1 ‘Standard Specification for Flat Glass ’ASTM International West Conshohocken PA doi:10.1520/C1036‐11E01 www.astm.org.10.1520/C1036 ↗
11. ASTM Standard C1048 2012e1 ‘Standard Specification for Heat‐Strengthened and Fully Tempered Flat Glass ’ASTM International West Conshohocken PA 2003 doi:10.1520/C1048‐12E01 www.astm.org.10.1520/C1048 ↗
12. “BS EN 12150‐1:2000 – Glass in building. Thermally toughened soda lime silicate safety glass. Definition and description ”British Standards Institution 2000.
13. “BS EN 14179‐1:2005 Glass in building. Heat‐soaked thermally‐toughened soda lime silicate safety glass ”British Standards Institution 2005.
14. “BS 6206:1981 Specification for impact performance requirements for flat safety glass and safety plastics for use in buildings ”British Standards Institution 1981.
15. “BS 6262‐4:2005 Glazing for buildings. Code of practice for safety related to human impact ”British Standards Institution 2005.
16. “BS 857:1967 Specification for safety glass for land transport ”British Standards Institution 1967.
17. 2007
18. 10.1007/978-3-642-50071-8_1210.1007/978-3-642-50071-8_12 ↗
19. Bottle Breakage – Causes and Types of Fractures
20. 10.1111/j.1151-2916.1935.tb19376.x10.1111/j.1151-2916.1935.tb19376.x ↗
21. 10.1111/j.1151-2916.1952.tb13108.x10.1111/j.1151-2916.1952.tb13108.x ↗
22. 10.1007/978-1-4899-1325-8_710.1007/978-1-4899-1325-8_7 ↗
23. Fréchette V. D. · 1990 · 100
24. “Using design to reduce injuries from alcohol related violence in pubs and clubs ” Home Office Design Out Crime 2010.
25. Tooley F. V. · 1984
26. R.Gardon “The Tempering of Glass by Forced Convection ” Proc. Int. Congr. Glastt 7th Institut. National du Verre Charleroi Belgique [paper no. 79] 1965.
27. 10.1111/j.1475-1305.2008.00422.x10.1111/j.1475-1305.2008.00422.x ↗
28. S. T.Gulati “Frangibility of Tempered Soda‐Lime Glass Sheet ” Glass Processing Days Tampere Finland 72–76 1997.
29. 10.1007/s11668-011-9432-510.1007/s11668-011-9432-5 ↗
30. 10.1520/JAI1256510.1520/JAI12565 ↗
31. Hull D. · 1999 · 87