The Strength of Silicate Glasses: What Do We Know, What Do We Need to Know?
Source abstract
Abstract
In the last few years, there has been increased interest in methods to improve the practical strength of inorganic glasses. During this same time period, new theoretical and experimental techniques have appeared. In this paper, we discuss this interest and indicate how and where these new techniques may help us to achieve our objective to increase the practical strength of glass. Our ability to measure the intrinsic inert strength of glass fibers as well as the development of stresses around indentations and scratches now allows us to attack these two important issues experimentally. Likewise, major advances have been made in techniques for the modeling glass structure and mechanical properties. The advances in these three areas give us indications of how changes in glass composition and processing can influence the final strength as well as its robustness.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Glass properties and applications · Advanced Surface Polishing Techniques · Laser Material Processing Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Stresses in a Plate Due to the Presence of Cracks and Sharp Corners
2. The Phenomena of Rupture and Flow in Solids
3. An Investigation of the Factors Likely to Affect the Strength and Properties of Glass Fibers
4. 10.1098/rspa.1967.008510.1098/rspa.1967.0085 ↗
5. Effect of Environment and Temperature on the Strength of E‐Glass Fibers
6. 10.1063/1.9390510.1063/1.93905 ↗
7. C. R.KurkjianandP. K.Gupta “Intrinsic Strength and the Structure of Glass ”Proceedings of the XIX International Congress on Glass Vol. 1 Edinburgh Scotland p.11 2001.
8. 10.1017/CBO978051162312710.1017/CBO9780511623127 ↗
9. Varshneya A. K. · 2006
10. 10.1016/B978-008044104-7/50008-310.1016/B978-008044104-7/50008-3 ↗
11. 10.1109/50.5071510.1109/50.50715 ↗
12. Kurkjian C. R. · 1985
13. 10.1016/j.jnoncrysol.2005.05.02910.1016/j.jnoncrysol.2005.05.029 ↗
14. 10.1063/1.44455610.1063/1.444556 ↗
15. 10.1016/0022-3093(85)90357-610.1016/0022-3093(85)90357-6 ↗
16. 10.1016/S0022-3093(98)00741-810.1016/S0022-3093(98)00741-8 ↗
17. D.Liao “Atomistic Simulation of Strength and Deformation of Ceramic Materials ” Ph.D. Thesis MIT p.136 2001.
18. 10.1021/cm800413v10.1021/cm800413v ↗
19. Measurement of the Strength of Thin Glass Rods Using a Transverse Bend Method
20. 10.1109/50.55756510.1109/50.557565 ↗
21. 10.1016/S0022-3093(02)01943-910.1016/S0022-3093(02)01943-9 ↗
22. 10.1016/j.jnoncrysol.2004.07.02310.1016/j.jnoncrysol.2004.07.023 ↗
23. 10.1016/j.jnoncrysol.2004.08.17910.1016/j.jnoncrysol.2004.08.179 ↗
24. The Effects of Melt History on the Failure Characteristics of Pristine Glass Fibers
25. TPB Test Provides New Insight to Fiber Strength and Quality
26. 10.1111/j.1151-2916.1986.tb07366.x10.1111/j.1151-2916.1986.tb07366.x ↗
27. The Diamond Pyramid Hardness of Glass in Relation to the Strength and Structure of Glass
28. 10.1021/nl803581r10.1021/nl803581r ↗
29. 10.1016/j.scriptamat.2008.12.05710.1016/j.scriptamat.2008.12.057 ↗
30. J.Li Private Communication (2009).
31. 10.1038/163323a010.1038/163323a0 ↗
32. W.Hillig “Concerning the Creation and Stability of Pyramidal Hardness Impression on Glass;”Advances in Glass Technology Part 2 eds. F. R.MatsonandG. E.Rindone.Plenum Press New York pp.51–521963.
33. 10.1111/j.1151-2916.1968.tb13318.x10.1111/j.1151-2916.1968.tb13318.x ↗
34. 10.1016/0022-3093(70)90188-210.1016/0022-3093(70)90188-2 ↗
35. 10.1007/BF0075212110.1007/BF00752121 ↗
36. 10.1557/jmr.2005.041810.1557/jmr.2005.0418 ↗
37. 10.3139/146.10147810.3139/146.101478 ↗
38. 10.1088/0022-3727/9/15/01110.1088/0022-3727/9/15/011 ↗
39. 10.1111/j.1151-2916.1995.tb08241.x10.1111/j.1151-2916.1995.tb08241.x ↗
40. 10.1111/j.1151-2916.1990.tb04268.x10.1111/j.1151-2916.1990.tb04268.x ↗
41. 10.1111/j.1551-2916.2005.00464.x10.1111/j.1551-2916.2005.00464.x ↗
42. 10.1098/rspa.1989.011610.1098/rspa.1989.0116 ↗
43. 10.1111/j.1151-2916.1982.tb10496.x10.1111/j.1151-2916.1982.tb10496.x ↗
44. M.Wada H.Furukawa andK.Fujita “Crack Resistance of Glass on Vicker's Indentation ”Proceedings of the X International Congress on Glass Kyoto 39–46 1974.
45. 10.1111/j.1151-2916.1998.tb02649.x10.1111/j.1151-2916.1998.tb02649.x ↗
46. T.Wilantewicz “Crack Initiation Behavior of Optical Glasses from Vickers Indentation ” Ph.D. Thesis Alfred University 2005.
47. 10.1016/S0022-3093(01)00421-510.1016/S0022-3093(01)00421-5 ↗
48. 10.1111/j.1151-2916.1990.tb05119.x10.1111/j.1151-2916.1990.tb05119.x ↗
49. 10.1063/1.32993210.1063/1.329932 ↗
50. 10.1063/1.32993010.1063/1.329930 ↗
51. 10.1080/0141861820823691710.1080/01418618208236917 ↗
52. Y.Kato H.Yamazaki S.Yamamoto S.Yoshida andJ.Matsuoka “Relationship Between Crack Resistance and Stress Generated Beneath Vickers Indentation ”Abstracts of the 3rd International Workshop of Flow and Fracture of Advanced Glasses p. 15 2005.
53. 10.1103/PhysRevLett.103.17550110.1103/PhysRevLett.103.175501 ↗
54. 10.1016/j.actamat.2003.09.01410.1016/j.actamat.2003.09.014 ↗
55. 10.1088/1475-4878/23/3/30210.1088/1475-4878/23/3/302 ↗
56. 10.1016/0022-3093(79)90154-610.1016/0022-3093(79)90154-6 ↗
57. 10.1111/j.1365-2818.1995.tb03669.x10.1111/j.1365-2818.1995.tb03669.x ↗
58. Hertzian Contact of Coated Glasses
59. 10.1016/0022-5096(81)90018-110.1016/0022-5096(81)90018-1 ↗
60. 10.1038/295511a010.1038/295511a0 ↗
61. 10.1111/j.1151-2916.1983.tb15715.x10.1111/j.1151-2916.1983.tb15715.x ↗
62. Fracture of Silicate Glasses
63. 10.1103/PhysRevLett.90.07550410.1103/PhysRevLett.90.075504 ↗
64. 10.1088/0022-3727/42/21/21400610.1088/0022-3727/42/21/214006 ↗