Effect of ceramic‐based coatings deposited on low‐alloyed steel T/P22 10H2M exposed at high temperature
Source abstract
Abstract
Abstract The study was carried out in order to evaluate oxidation resistance of the ceramic coatings based on SiO 2 ‐B 2 O 3 ‐TiO 2 ‐Na 2 O composition deposited on the low‐alloyed steel T/P22 (10H2M) surface exposed for 1000 h at 540°C in oxidation atmosphere. Kinetic data were recorded periodically every 250 h; macro‐ and microanalyses as well as chemical composition were carried out using macrolenses, SEM, EDS, EDS X‐ray mappings. The results indicated a high degree of protection by ceramic coatings; much lower mass gain was observed for the coated materials than for the uncoated T/P22 (10H2M) steel. No detachment, delamination, chipping of a coating were found from the steel surface; some of the coatings showed perpendicular tiny cracks to the bulk metal surface.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
ŁUKASIEWICZ Research Network Krakow Institute of Technology St. Krakow Poland
ŁUKASIEWICZ Research Network Institute of Ceramics and Building Materials St. Warszawa Poland
References (23)
Show source-provided references
1. 10.1088/2053-1591/ab526510.1088/2053-1591/ab5265 ↗
2. 10.1007/s11666-013-9887-x10.1007/s11666-013-9887-x ↗
3. Beyond traditional coatings: a review on thermal‐sprayed functional and smart coatings
4. 10.6028/jres.038.01410.6028/jres.038.014 ↗
5. Review of ceramic coating on mild steel methods, applications and opportunities
6. Advanced ceramic coatings on stainless steel, a review of research, methods, materials, applications and opportunities
7. 10.1016/j.ceramint.2013.11.06710.1016/j.ceramint.2013.11.067 ↗
8. 10.1016/S0257-8972(97)00223-510.1016/S0257-8972(97)00223-5 ↗
9. 10.1007/s12540-020-00705-w10.1007/s12540-020-00705-w ↗
10. 10.3184/096034011X1318876575809810.3184/096034011X13188765758098 ↗
11. 10.3184/096034011X1319812696738210.3184/096034011X13198126967382 ↗
12. 10.1002/1527-2648(200104)3:4<193::AID-ADEM193>3.0.CO;2-U10.1002/1527-2648(200104)3:4<193::AID-ADEM193>3.0.CO;2-U ↗
13. 10.1007/s11085-017-9728-210.1007/s11085-017-9728-2 ↗
14. 10.1361/10599639877035071010.1361/105996398770350710 ↗
15. 10.1016/j.jmatprotec.2008.06.01710.1016/j.jmatprotec.2008.06.017 ↗
16. 10.1590/S1516-1439200500040000210.1590/S1516-14392005000400002 ↗
17. 10.1023/B:OXID.0000016274.78642.ae10.1023/B:OXID.0000016274.78642.ae ↗
18. 10.3103/S1068798X1909023510.3103/S1068798X19090235 ↗
19. Numerical study of pore formation in thermal spray coating process by investigating dynamics of air entrapment
20. 10.1007/s11090-007-9097-810.1007/s11090-007-9097-8 ↗
21. 10.1007/s10973-015-4871-y10.1007/s10973-015-4871-y ↗
22. 10.1007/BF0270853910.1007/BF02708539 ↗
23. 10.1016/j.corsci.2014.01.03310.1016/j.corsci.2014.01.033 ↗