Abstract

The effects of cyclic frequency on the fatigue behavior of silicon carbide (Nicalon) fiber‐reinforced glass–ceramic matrix (SiC/magnesium aluminosilicate (MAS)) were investigated. Tension–tension fatigue tests were conducted at two frequencies, 10 and 900 Hz, to establish stress versus cycles to failure ( S–N ) relationships. Cycles to failure at a given stress level decreased with an increase of the applied frequency. Analysis of damage mechanisms suggests that there was an enhancement of fiber/matrix interfacial bonding at the higher frequency due to the formation of SiO 2 from the reaction of oxygen species of the matrix with SiC of the fiber.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Innovative concrete reinforcement materials · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Applications of CMCs to Turbojet Engines
2. Ceramic Composite Turbine Disks for Rocket Engines
3. Performances of Four Ceramic–Matrix Composite Divergent Flap Inserts Following Ground Testing on an F110 Turbofan Engine10.1111/j.1151-2916.2000.tb01457.x ↗
4. The Design of the Fibre–Matrix Interfacial Zone in Ceramic Matrix Composites10.1016/S1359-835X(97)00128-0 ↗
5. 10.1016/0010-4361(92)90181-S10.1016/0010-4361(92)90181-S ↗
6. 10.1016/S1359-835X(98)00177-810.1016/S1359-835X(98)00177-8 ↗
7. 10.1016/S0266-3538(01)00096-310.1016/S0266-3538(01)00096-3 ↗
8. 10.1177/07316844920110030210.1177/073168449201100302 ↗
9. 10.1177/07316844940130050310.1177/073168449401300503 ↗
10. 10.1163/156855192X0023310.1163/156855192X00233 ↗
11. 10.1016/0921-5093(90)90030-710.1016/0921-5093(90)90030-7 ↗
12. 10.1016/0955-2219(95)00098-410.1016/0955-2219(95)00098-4 ↗
13. 10.1016/j.tsf.2004.11.11110.1016/j.tsf.2004.11.111 ↗
14. Interfacial Microstructure and Stability of BN‐Coated Nicalon Fiber/Glass–Ceramic Matrix Composites
15. 10.1007/BF0035734610.1007/BF00357346 ↗
16. 10.1007/BF0072652210.1007/BF00726522 ↗
17. 10.1111/j.1151-2916.1993.tb07772.x10.1111/j.1151-2916.1993.tb07772.x ↗
18. 10.1111/j.1151-2916.1994.tb04587.x10.1111/j.1151-2916.1994.tb04587.x ↗
19. High Frequency Fatigue Behavior of Woven‐Fiber‐Fabric‐Reinforced Polymer‐Derived Ceramic‐Matrix Composites10.1111/j.1151-2916.1998.tb02472.x ↗
20. The High Temperature Tensile Fatigue Behavior of a Polymer‐Derived Ceramic‐Matrix Composites
21. 10.1016/j.compscitech.2005.06.02010.1016/j.compscitech.2005.06.020 ↗
22. 10.1016/S0266-3538(03)00190-810.1016/S0266-3538(03)00190-8 ↗
23. 10.1007/BF0036783510.1007/BF00367835 ↗
24. Effect of Loading Rate on the Monotonic Tensile Behavior of a Continuous‐Fiber‐Reinforced Glass–Ceramic Matrix Composite10.1111/j.1151-2916.1996.tb08122.x ↗
25. Development and Healing of Matrix Microcracks in Fibre Reinforced Glass Matrix Composites
26. 10.1111/j.1151-2916.1993.tb06640.x10.1111/j.1151-2916.1993.tb06640.x ↗
27. 10.1016/j.msea.2005.08.04010.1016/j.msea.2005.08.040 ↗
28. SiC Nicalon Fibre Glass Matrix Composites
29. M. C.HalbigandA. J.Eckel “Oxidation of Continuous Carbon Fibers within a Silicon Carbide Matrix under Stressed and Unstressed Conditions ” NASA TM‐2000‐210224 Washington DC 2000.