The adhesion of linoleic acid heated at different temperatures ranging from 220 to 280°C on three different substrates has been investigated. During heating, several chemical modifications of linoleic acid occur and strong adhesion to the substrate develops. In order to obtain quantitative data, a specific adhesion test has been developed. The adhesion of linoleic acid at high temperature can be strongly reduced by using fluoroalkylsilane-treated plates.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Adsorption, diffusion, and thermodynamic properties of materials · Silicone and Siloxane Chemistry · Polymer Nanocomposites and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. Mostefaı̈ · Int J Adhesion Adhesives · 1998 · 18 · 27310.1016/S0143-7496(98)00006-2 ↗
2. van Oss · Langmuir · 1988 · 4 · 88410.1021/la00082a018 ↗
3. De Palma · Langmuir · 1989 · 5 · 86810.1021/la00087a049 ↗
4. Dang · Surf Interface Anal · 1990 · 15 · 11310.1002/sia.740150209 ↗
5. Kazufumi O. Mamoru S. Shinzi O. Shiego I. Eur Pat Appl EP 571, 896, 1992.
6. Arkles B, Steinmetz JR, Zazyczny J, Mehta P. In: Mittal KL, editor. Silanes and other coupling agents. Utrednt, The Netherlands: VSP, 1992. p. 91.
7. Kazufumi O. Norihisa M. Mamoru S. Eur Pat Appl EP 493, 747, 1992.
8. Albinson RB. Eur Pat Appl EP 367, 438, 1990.