Effect of laminating parameters on the adhesion property of flexible copper clad laminate with adhesive layer

Bo-In Noh, Jeong-Won Yoon, Seung-Boo Jung

Publisher page

Abstract

Abstract In this study, the effect of two laminating parameters, laminating pressure and holding time, on the adhesion strength of flexible copper clad laminate (FCCL) with an epoxy-type adhesive layer was evaluated. The changes in the adhesion property, fracture surface, morphology, and chemical bonding state were characterized by 90° peel test, scanning electron microscopy (SEM), atomic force microscopy (AFM), and X-ray photoelectron spectroscopy (XPS). The results showed that the adhesion strength of the FCCL was decreased as the laminating pressure was increased beyond the suitable level. Laminating pressure exerted the greatest influence over the FCCL adhesion strength. On the other hand, the holding time did not significantly affect the peel strength of the FCCL. The fracture of FCCL occurred at the interface between the rolled Cu and the adhesive layer. In addition, the FCCL with high adhesion strength was stable with the variation of adhesion strength after temperature and humidity test.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical Behavior of Composites · Surface Modification and Superhydrophobicity · Electronic Packaging and Soldering Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Kamiya · Surf Coat Technol · 2007 · 202 · 108410.1016/j.surfcoat.2007.07.061 ↗
2. Kazi · Thin Solid Films · 2006 · 515 · 260210.1016/j.tsf.2005.10.077 ↗
3. Kinloch · J Mater Sci · 1998 · 24 · 218310.1007/BF02385439 ↗
4. Park · Mater Sci Eng A · 1999 · 266 · 26110.1016/S0921-5093(98)01117-4 ↗
5. Greenwood · J Adhes Sci Technol · 1995 · 9 · 31110.1163/156856195X00527 ↗
6. Ramos MMD. Vacuum 2002;64:255.10.1016/S0042-207X(01)00332-3 ↗
7. He · Thermochim Acta · 2001 · 367–368 · 10110.1016/S0040-6031(00)00654-7 ↗
8. Liston · J Adhes Sci Technol · 1993 · 7 · 109110.1163/156856193X00600 ↗
9. Burkstrand · J Vac Sci Technol · 1979 · 16 · 107210.1116/1.570163 ↗
10. Jordan · J Vac Sci Technol A · 1986 · 4 · 104610.1116/1.573451 ↗
11. Lee · Appl Surf Sci · 2003 · 205 · 12810.1016/S0169-4332(02)01016-4 ↗
12. Liu · Surf Coat Technol · 2005 · 196 · 19210.1016/j.surfcoat.2004.08.127 ↗
13. Hsieh · Surf Coat Technol · 1999 · 112 · 23510.1016/S0257-8972(98)00779-8 ↗
14. Ge · Thin Solid Films · 2003 · 440 · 19810.1016/S0040-6090(03)00851-4 ↗
15. Prolongo · Int J Adhes Adhes · 2006 · 26 · 12510.1016/j.ijadhadh.2005.02.004 ↗