Bond strength to aged CAD/CAM composites and polymer-infiltrated ceramic network using a universal adhesive with or without previous application of a universal primer
Source abstract
Abstract
To analyse the bond strength to aged CAD/CAM composites and a polymer-infiltrated ceramic network (PICN) after different surface pretreatments and the use of a universal adhesive or universal primer and universal adhesive. Specimens were prepared from CAD/CAM composites (Brilliant Crios, Grandio Blocs, Lava Ultimate, Tetric CAD, Cerasmart270, Katana Avencia, Shofu Block HC) or PICN (Vita Enamic) and artificially aged (5000 cycles, 5–55 °C). The surfaces were left untreated or pretreated by mechanical roughening, aluminium oxide sandblasting, silica coating, or hydrofluoric acid etching (PICN only). The surfaces were further conditioned with a universal adhesive only or a universal primer/universal adhesive (each subgroup n = 12). After application of a composite and further thermal cycling, shear bond strength and failure modes were assessed and statistically analysed by ANOVAs, Weibull statistics, and Chi 2 -test (p < 0.05). In CAD/CAM composites, highest bond strength values were obtained for sandblasting (mean of all subgroups: 15.7 ± 4.5 MPa) > silica coating (13.5 ± 4.1 MPa) > mechanical roughening (11.3 ± 4.5 MPa) > no pretreatment (4.1 ± 2.3 MPa). The use of a universal primer led to a significant, albeit small increase of bond strength (11.9 ± 6.0 > 10.4 ± 5.6 MPa). In PICN bond strength was: hydrofluoric acid etching (15.2 ± 4.0 MPa) > silica coating (12.2 ± 4.3 MPa) > sandblasting (11.6 ± 5.3 MPa) > mechanical roughening (10.9 ± 7.2 MPa) > no pretreatment (2.8 ± 2.7 MPa). The application of a universal primer led to a significant increase of bond strength (13.5 ± 6.3 > 7.6 ± 5.0 MPa). Adhesion to aged CAD/CAM composites mainly requires adequate micromechanical retention, while PICN additionally requires the use of a universal primer. • Repair of CAD/CAM composites and PICN is possible. • Repairing CAD/CAM composites requires sandblasting. • Repairing PICN requires surface pretreatment and the use of a universal primer.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Additive Manufacturing and 3D Printing Technologies · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (37)
Show source-provided references
1. From artisanal to CAD-CAM blocks: state of the art of indirect composites10.1177/0022034516634286 ↗
2. Ultrathin CAD-CAM glass-ceramic and composite resin occlusal veneers for the treatment of severe dental erosion: an up to 3-year randomized clinical trial10.1016/j.prosdent.2022.02.009 ↗
3. 5.5-year-survival of CAD/CAM resin-based composite restorations in severe tooth wear patients10.1016/j.dental.2024.03.001 ↗
4. Vervack V., Keulemans F., Hommez G., de Bruyn H., Vandeweghe S. A completely digital workflow for nanoceramic endocrowns: a 5-year prospective study. Int J Prosthodont (IJP) 35:259–268. doi:10.11607/ijp.7545.10.11607/ijp.7545 ↗
5. Monolithic polymer-infiltrated ceramic network CAD/CAM single crowns: three-year mid-term results of a prospective clinical study10.11607/ijp.6548 ↗
6. A 3-year clinical evaluation of endodontically treated posterior teeth restored with two different materials using the CEREC AC chair-side system10.1016/j.prosdent.2017.04.022 ↗
7. Intraoral wear of PICN CAD-CAM composite restorations used in severe tooth wear treatment: 5-year results of a prospective clinical study using 3D profilometry10.1016/j.dental.2024.05.015 ↗
8. Criteria for the replacement of restorations: academy of operative dentistry European section10.2341/15-058-O ↗
9. Same, same, but different? A systematic review of protocols for restoration repair10.1016/j.jdent.2019.05.021 ↗
10. Scoping Review: effect of surface treatments on bond strength of resin composite repair10.1016/j.jdent.2023.104737 ↗
11. Which surface treatment promotes higher bond strength for the repair of resin nanoceramics and polymer-infiltrated ceramics? A systematic review and meta-analysis10.1016/j.prosdent.2020.06.009 ↗
12. Phosphate group adsorption capacity of inorganic elements affects bond strength between CAD/CAM composite block and luting agent10.4012/dmj.2020-029 ↗
13. Repair bond strength of a new self-adhesive composite resin to three different resin-matrix ceramic CAD-CAM materials10.4012/dmj.2023-165 ↗
14. Effect of bonding protocols on the performance of luting agents applied to CAD–CAM composites10.3390/ma15176004 ↗
15. Influence of different universal adhesives on the repair performance of hybrid CAD-CAM materials10.5395/rde.2019.44.e23 ↗
16. Effectiveness and stability of silane coupling agent incorporated in ‘universal’ adhesives10.1016/j.dental.2016.07.002 ↗
17. Influence of universal adhesives and silane coupling primer on bonding performance to CAD‐CAM resin‐based composites: a laboratory investigation10.1111/jerd.13165 ↗
18. How the repair bonding strength of hybrid ceramic CAD/CAM blocks is influenced by the use of surface treatments and universal adhesives10.4012/dmj.2023-237 ↗
19. Influence of accelerated ageing on the physical properties of CAD/CAM restorative materials10.1007/s00784-019-03101-w ↗
20. Does artificial aging affect mechanical properties of CAD/CAM composite materials10.1016/j.jpor.2017.06.001 ↗
21. Adhesion to tooth structure: a critical review of “macro” test methods10.1016/j.dental.2009.11.150 ↗
22. Shear bond strength of a direct resin composite to CAD-CAM composite blocks: relative contribution of micromechanical and chemical block surface treatment10.3390/ma15145018 ↗
23. Influence of different surface treatments and universal adhesives on the repair of CAD-CAM composite resins: an in vitro study10.1016/j.prosdent.2020.02.029 ↗
24. Correlation between microstructure of CAD/CAM composites and the silanization effect on adhesive bonding10.1016/j.jmbbm.2019.103441 ↗
25. Influence of mechanical and chemical pre-treatments on the repair of a hybrid ceramic10.1016/j.dental.2022.05.003 ↗
26. Tensile bond strength of so-called universal primers and universal multimode adhesives to zirconia and lithium disilicate ceramics
27. High bond durability of universal adhesives on glass ceramics facilitated by silane pretreatment10.2341/17-227-L ↗
28. Bonding performance of dispersed filler resin composite CAD/CAM blocks with different surface treatment protocols10.4012/dmj.2020-049 ↗
29. Effect of various surface treatments on the bond strength of resin luting agent and the surface roughness and surface energy of CAD/CAM materials10.4012/dmj.2019-359 ↗
30. Bonding efficacy of universal resin adhesives to zirconia substrates: systematic review and meta-analysis
31. Silane influence on bonding to CAD-CAM composites: an interfacial fracture toughness study10.1016/j.dental.2019.05.019 ↗
32. Combination of a silane coupling agent and resin primer reinforces bonding effectiveness to a CAD/CAM indirect resin composite block10.4012/dmj.2021-083 ↗
33. Effect of surface treatment strategies on bond strength of additively and subtractively manufactured hybrid materials for permanent crowns10.1007/s00784-024-05767-3 ↗
34. Different surface treatments on recently introduced CAD-CAM resin-modified ceramics: implications on bond strength10.1016/j.prosdent.2024.05.032 ↗
35. In vitro and practical guide for the analysis of bond strength to ceramics10.1016/j.ceramint.2023.02.071 ↗
36. Thermal cycling for restorative materials: does a standardized protocol exist in laboratory testing? A literature review10.1016/j.jmbbm.2013.09.013 ↗
37. Evaluation of bond strength of resin cements using different general-purpose statistical software packages for two-parameter Weibull statistics10.1016/j.dental.2012.04.013 ↗