Boiling water and silane pre-treatment of aluminium alloys for durable adhesive bonding
Source abstract
Abstract
Three series of aluminium alloys received a surface pre-treatment including immersion in boiling water followed by soaking in a 1% aqueous solution of 3-glycidoxytrimethoxysilane. When aluminium was pre-treated in this manner, adhesive joints formed with a range of epoxy resins produced notable improvements in bond durability in comparison with simple abrasion pre-treatments. In some cases, the pre-treatment improved joint durability to the level observed for the phosphoric acid anodise process. The development of a platelet structure in the outer film region combined with the hydrolytic stability of adhesive bonds made to the epoxy silane appear to be critical in developing the bond durability observed. Generally, immersion of the aluminium alloys at temperatures above 80°C for periods between 4 and 60 min provide the optimum conditions required to prepare a surface film, which will produce durable bonds with epoxy adhesive.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Anodic Oxide Films and Nanostructures · Electronic Packaging and Soldering Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Alwitt RS. In: Diggle JW, Ashok KV, editors. Oxides and oxide films, vol. 4. New York: Marcel Dekker, 1976.
2. Alwitt · J Electrochem Soc · 1971 · 118 · 173010.1149/1.2407826 ↗
3. Stralin · J Appl Polym Sci · 1993 · 49 · 51110.1002/app.1993.070490315 ↗
4. Vedder · Trans Faraday Soc · 1969 · 65 · 56110.1039/tf9696500561 ↗
5. McCarvill · J Appl Polym Sci · 1974 · 18 · 33510.1002/app.1974.070180202 ↗
6. Wegman RF. Report No. PA-TR-3495. New Jersey: Feltmann Res Labs, 1967.
7. McCarvill · J Appl Polym Sci · 1974 · 18 · 34310.1002/app.1974.070180203 ↗
8. Smith · J Adhes · 1982 · 14 · 14510.1080/00218468208074898 ↗
9. Minford · 1993
10. Minford JD. In: Mittal KL, editor. Adhesive joints-formation, characteristics, and testing. New York: Plenum Press, 1984. p. 503.
11. Bainbridge · Int J Adhes Adhes · 1982 · 2 · 17510.1016/0143-7496(82)90086-0 ↗
12. Perkins · J Adhes · 1980 · 11 · 22110.1080/00218468008078918 ↗
13. Uchiyama · Keikinzoku · 1985 · 35 · 29
14. Stralin · J Adhes · 1993 · 41 · 5110.1080/00218469308026554 ↗
15. Isoyama · Aluminium · 1987 · 63 · 1151
16. Bernard · J Electrochem Soc · 1959 · 106 · 64310.1149/1.2427463 ↗
17. Lambrianidis, LT, Arnott DR, Wilson, AR, Van den Berg J, Vargas O. Proceedings of the International Aerospace Congress Melbourne, 1995. p. 355–60.
18. Venables · J Mater Sci · 1985 · 19 · 243110.1007/BF00550796 ↗
19. Arnott DR, Rider AN, Olsson–Jacques CL. Proceedings of the 21st Congress ICAAS. Melbourne, 1998.
20. Woldman NE. In: Frick JP, editor, Woldman's Engineering Alloys, 7th ed. Ohio: ASM International, 1990.
21. ASTM, Annual Book of ASTM Standards Section 15, vol 15.06, Adhesives. Philadelphia: ASTM, 1992.
22. Asami · Corros Sci · 1977 · 17 · 55910.1016/S0010-938X(77)80002-4 ↗
23. Rider AN, Arnott DR. In: Wang C.H. editor, Proceedings of the Structural Integrity and Fracture. Melbourne: Australian Fracture Group inc., ISBN:0 646 36038 8; 1998. p. 121–132.
24. Unpublished results.
25. Rider · Surf Interface Anal · 1996 · 24 · 58310.1002/(SICI)1096-9918(19960916)24:9<583::AID-SIA159>3.0.CO;2-Z ↗
26. Arnott · Appl Surf Sci · 1993 · 70–1 · 10910.1016/0169-4332(93)90408-4 ↗