Source abstract
Abstract
The effects of heating temperature, cooling method, re-curing time and water-to-cement ratio (w/c) on the natural restoration of mechanical properties of concrete exposed to high temperature were experimentally studied. The fire-damaged concrete specimens were re-cured in ambient conditions after they had been rapidly cooled in water and naturally cooled in air. Below 500°C, the natural restoration of the compressive strength of water-cooled concrete was more evident than that of air-cooled concrete. The natural restoration of the compressive strength of air-cooled concrete with low w/c ratio was more obvious than that of concrete with high w/c ratio. After being subjected to 500°C and re-cured for 3 months, the splitting tensile strength decreased to below 26% of the initial value. The splitting tensile strength of water-cooled concrete recovered more evidently than that of the air-cooled concrete. The restoration of elastic modulus was mainly affected by the heating temperature and cooling method. The elastic modulus of water-cooled concrete which had been subjected to 200, 300 and 400°C was obviously restored after being naturally re-cured for 3 months. The effects of w/c on the tensile strength and elastic modulus were not significant.
Source: crossref · Quality: baseline
Affiliations
Associate Professor, State Key Laboratory for Geomechanics and Deep Underground Engineering, China University of Mining and Technology, Xuzhou, China
JiangSu Collaborative Innovation Center for Building Energy Saving and Construction Technology, Xuzhou, Jiangsu, P. R. China (corresponding author: )
MSc candidate, School of Mechanics and Civil Engineering, China University of Mining and Technology, Xuzhou, P. R. China
Professor, School of Mechanics and Civil Engineering, China University of Mining and Technology, Xuzhou, P. R. China