Porous Functional Coatings by Microarc Oxidation

M. A. Markov, D. A. Gerashchenkov, A. V. Krasikov, I. V. Ulin, A. D. Bykova, M. L. Shishkova, N. V. Yakovleva

Glass and Ceramics· Volume 75· Issue 7-8
Publisher page

Abstract

FGUP TsNII KM “Prometey” have proposed a new approach to creating porous functional ceramic coatings on the surface of steel by means of low-temperature heterophase transport combined with microarc oxidation (MAO). The adhesion of the coating to metal is at least 60 MPa. An intermediate layer of the coating contains nickel–aluminum intermetallide compounds and imparts mechanical strength during service at temperatures above 750°C. It is shown for the example of nickel that catalytic active substances with promoters can be deposited on the surface of porous coatings from solutions of their salts or hydroxides followed by decomposition as a result of heat-treatment; metal can also be deposited into the pores of a MAO coating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Catalytic Processes in Materials Science · Catalysts for Methane Reforming · Catalysis and Hydrodesulfurization Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. I. V. Suminov, P. N. Belkin, A. V. Eppelfeld, et al., Plasma-Electrolytic Modification of the Surface of Metals and Alloys [in Russian], Tekhnosfera, Moscow (2011), Vol. 2.
2. I. V. Suminov, A. V. Eppelfeld, and V. B. Lyudin, “Microarc oxidation (review),” Pribory, No. 9, 13 – 23 (2001).
3. I. V. Suminov, A. V. Eppelfeld, V. B. Lyudin, et al., Microarc Oxidation: (Theory, Technology, Equipment) [in Russian], ÉKOMET, Moscow (2005).
4. E. S. Atrotsenko, I. A. Kazantsev, A. E. Rozen, and N. V. Golovanova, “Field of application and properties of coatings obtained by microarc oxidation,” Fiz. Khim. Obrab. Mater., No. 3, 8 – 11 (1996).
5. A. O. Shtokal, E. V. Rykov, and K. B. Dobrosovestnov, “Increase of wear resistance, rigidity, accuracy and electrical resistivity of the units of space vehicles by means of microarc oxidation,” in: Topical Problems of Russian Cosmonautics: Proc. 38th Academic Lectures on Cosmonautics [in Russian], Moscow (2014), pp. 544 – 545.
6. V. Nichelea, M. Signorettoa, F. Menegazzoa, et al., “Hydrogen production by ethanol steam reforming effect of the synthesis parameters on the activity of Ni/TiO2 catalysts,” Int. J. Hydrogen Energy, 39(9), 4252 – 4258 (2014).10.1016/j.ijhydene.2013.12.178 ↗
7. X. Guo, Y. Sun, Y. Yu, et al., “Carbon formation and steam reforming of methane on silica supported nickel catalysts,” Catal. Commun., 19, 61 – 65 (2012).10.1016/j.catcom.2011.12.031 ↗
8. S.-H. Seoka, S.-H. Hanb, and J. S. Lee, “The role of MnO in Ni/MnO–Al2O3 catalysts for carbon dioxide reforming of methane,” Appl. Catal. A, General, 215(1 – 2), 31 – 38 (2001).10.1016/S0926-860X(01)00528-2 ↗
9. A. P. Alkhimov, S. V. Klinkov, V. F. Kosarev, and V. M. Fomin, Cold Gas-Dynamic Sputter Deposition [in Russian], Fizmatlit, Novosibirsk (2010).
10. M. Ye. Avvakumov and M. V. Rufitskii, “Reliability and quality of coating obtained by cold gas-dynamic deposition,” in: Proc. of the Int. Symposium “Reliability and Quality” [in Russian] (2013), Vol. 2.
11. A. P. Alkhimov, V. F. Kosarev, and A. N. Papirin, “Method of cold gas-dynamic sputter deposition,” Dokl. Akad. Nauk SSSR, 315, 1062 – 1065 (1990).
12. D. A. Gerashchenkov, A. F. Vasil’ev, B. V. Farmakovskii, and A. S. Mashek, “Investigation of the flow temperature in cold gas-dynamic spraying of functional coatings,” Vopr. Materialoved., No. 1(77), 87 – 97 (2014).
13. M. A. Markov, A. V. Krasikov, D. A. Gerashchenkov, et al., “Synthesis of wear-resistant ceramic coatings on steel materials with integrated use of supersonic heterophase transfer and microarc oxidation methods,” Ogneup. Tekh. Keram., No. 10, 30 – 35 (2016).
14. A. N. Novikov, A. N. Batishchev, Yu. A. Kuznetsov, and A. V. Kolomeichenko, Restoration and Hardening of Aluminum Alloy Components by Microarc Oxidation [in Russian], Izd. Orel GAU, Orel (2001).
15. V. P. Perminov and V. A. Neronov, Material Science and Technology of Materials [in Russian], SSGA, Novosibirsk (2008), pp. 91 – 92.
16. A. M. Makarov, D. A. Gerashchenkov, and A. F. Vasiliev, “Optimization of the coating deposition process by the CGDS method applied under production conditions for the example of aluminum powder,” Vopr. Materialoved., No. 2, 116 – 123 (2017).
17. A. V. Krasikov and A. A. Ezhov, Water-Based Electrolyte for Nickel-Plating of Articles Made of Steel. Aluminum, Titanium, Copper and Their Alloys, Pat. 2543584 RF, IPC C25D 3/1 [in Russian], applicant and the patent holder FGUP TsNII KM Prometei, 2013134110/02; appl. July 19, 2013; publ. March 10, 2015.
18. A. V. Krasikov, Electrodeposition of Nickel-Tungsten Alloy from Pyrophosphate Electrolyte, Author’s Abstract of Candidate’s Thesis [in Russian], St. Petersburg (2012).