Failure analyses and wear mechanisms of rock drill rods, a case study
Source abstract
Abstract
Abstract Rock drill rod failure is a big concern for the mining industry. The tough conditions required to break down rock material into small pieces subject rock drill components to high mechanical stresses and corrosion that lead to the failure of the drill rods. This paper describes a detailed examination of rock drill rods failed during field operations. The drill rods were manufactured from a high strength, hardened and tempered steel 22NiCrMo12-5F, carburized for better surface performance. The examination was carried out by means of light optical microscopy and scanning electron microscope. Microhardness profiles were performed for the studied rods. The focus of the present case study was to characterize the failure mechanisms and surface damages of the failed drill rods. The examined drill rods failed due to the initiation and propagation of fatigue microcracks at the outer surface of the thread. Surface cracks propagated to a certain crack length until the fracture toughness of the drill rod was exceeded and the final failure occurred. Multiple short cracks were observed on the fracture surface of the failed rods. The observed cracks propagated perpendicularly to the impacting direction towards the inner surface of the rods. Two different crack initiation mechanisms were observed in the present study, crack initiation from pits and crack initiation from severe plastic surface deformation. Sliding and abrasive wear damage, severe plastic deformation and pitting corrosion were observed on the threaded portion of the rods. Sliding wear was the most common wear damage mechanism observed in the thread joint. Pitting corrosion and severe plastic deformation, made the worn surface susceptible to crack initiation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Surface Treatment and Residual Stress · Advanced machining processes and optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Atlas Copco Face Drilling Third Edition. Örebro: Atlas copco Rock Drills (AB2004).
2. Introduction to surface hardening of steel ASM handbook
3. Davis · 2002
4. Totten · 2002
5. Lampman · 1996 · vol. 19 · 680
6. Bending fatigue crack characterization and fracture toughness of gas carburized SAE 4320 steel
7. Phosphorus and carbon segregation: effects on fatigue and fracture of gas-carburized modified 4320 steel10.1007/BF02652297 ↗
8. Shot-peening treatments
9. Zhu · J. Mater. Sci. · 2013 · 48 · 41310.1007/s10853-012-6756-9 ↗
10. 1987 · 12
11. The effect of phosphorus content on grain boundary cementite formation in AISI 52100 steel10.1007/BF02642342 ↗
12. The effect of phosphorous content and proeutectoid carbide distribution on the fracture behavior of 52100 steel10.1007/BF02833224 ↗
13. Microstructure and high bending fatigue strength in carburized steel10.1007/BF02833192 ↗
14. Effects of strain hardening and fine structure on strength and toughness of tempered martensite in carbon steels
15. Heat treated martensitic steels: microstructural systems for advanced manufacture10.2355/isijinternational.35.349 ↗
16. Influence of pitting on the fatigue life of a turbine blade steel10.1046/j.1460-2695.1999.00226.x ↗
17. Corrosion pitting and environmentally assisted small crack growth
18. Prediction of fatigue crack initiation life based on pit growth10.5006/1.3577891 ↗
19. Penetration rate prediction for percussive drilling with rotary in very hard rock
20. Investigation of white etching layers on rails by optical microscopy, electron microscopy, X-ray and synchrotron X-ray diffraction10.1016/S0921-5093(00)01842-6 ↗
21. Nanostructure formation on the surface of railway tracks10.1016/S0921-5093(00)01947-X ↗