journal article·2016-07

Cracking due to Cu and Ni segregation in a 17-4 PH stainless steel piston rod

Jialong Tian, Wei Wang, Wei Yan, Zhouhua Jiang, Yiyin Shan, Ke Yang

Publisher page

Abstract

Abstract The 17-4 PH stainless steel is employed to produce piston rods in industry due to the high strength and toughness, good workability and nice corrosion resistance. In the present failure analysis, obvious long cracks were observed along the longitudinal direction on the surface of the commercial 17-4 PH stainless steel piston rod after heat treatment. The cracks were carefully looked into by observing the crack tip and characterizing the microstructure along the cracks. The results showed that the cracks were mostly initiated from the surface of the rod and propagated along the phase boundary between martensite and δ ferrite. The EDXA showed that the segregation of Cu and Ni should be responsible for the cracking after heat treatment. In order to define when the crack was coming into being, oxidation film along the crack was considered as a clue. The scrutiny of the oxidation film on the crack edge illustrated that the crack should be formed right in the heat treatment of aging.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. 1969
2. Aging reactions in a 17-4 PH stainless steel10.1016/S0254-0584(01)00460-6 ↗
3. The effect of microstructural evolution on hardening behavior of type 17-4 PH stainless steel in long term aging at 350°C10.1016/j.matchar.2006.02.004 ↗
4. Metallurgical evaluation of 17-4 PH stainless steel castings
5. Correctly heat treatment 17-4 PH investment castings
6. On the hardness criterion for stress corrosion cracking resistance of 17-4 PH stainless steel10.1007/BF00455633 ↗
7. Failure analysis of holding yokes made of investment cast 17-4 PH stainless steel10.1016/j.engfailanal.2011.03.008 ↗
8. Failure of a 17-4 PH stainless steel sailboat propeller shaft10.1016/S1350-6307(03)00041-4 ↗
9. Embrittlement of laser surface-annealed 17-4 PH stainless steel10.1016/S0921-5093(01)00941-8 ↗
10. 1994