Abstract

Abstract The pinion from the drive of the cement mill was failed; the teeth cracked and spall occurred on the sides of several teeth. The failure was only located on one side of the pinion. This type of failure is common with surface-hardened gears. We have found that the failure of the pinion is a direct consequence of the incorrect geometry of the surface hardened layer. The lifespan of the pinion could have been extended if the whole surface of the faces and roots of the teeth had been hardened and if the hardening had been deeper.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced machining processes and optimization · Advanced Machining and Optimization Techniques · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Heat treatment of cold formed steel forgings for the automotive industry
2. Heat treatment of cold formed steel forgings
3. The metallurgy of induction surface hardening
4. Rudnev · 2003
5. Decker · 1975
6. Totten · 1997
7. Achieving uniform temperature through induction heating
8. Temperature field and failure analysis of die-casting die
9. Fatigue cracking of an aircraft wheel10.1016/S1350-6307(02)00008-0 ↗
10. Cannale · 2008
11. Allianz handbook of loss prevention. Berlin: Allianz Versicherungs AG; 1987. p. 344–8.
12. Jocic · 2008
13. Induction hardening of gears: a review
14. Analysis of casting die failures10.1016/S1350-6307(00)00032-7 ↗